Thermo-luminescence kinetic parameters of γ-irradiated Sr4Al14O25:Eu2+, Dy3+ phosphors

被引:4
|
作者
Bedyal, A. K. [1 ]
Kumar, Vinay [1 ,2 ]
Singh, V. K. [1 ]
Lochab, S. P. [3 ]
Singh, Fouran [3 ]
Ntwaeaborwa, O. M. [2 ]
Swart, H. C. [2 ]
机构
[1] Shri Mata Vaishno Devi Univ, Sch Phys, Katra 182320, Jammu & Kashmir, India
[2] Univ Free State, Dept Phys, ZA-9300 Bloemfontein, South Africa
[3] Interuniv Accelerator Ctr, New Delhi 110067, India
来源
RADIATION EFFECTS AND DEFECTS IN SOLIDS | 2013年 / 168卷 / 11-12期
关键词
thermo-luminescence; aluminates; kinetic parameter; combustion synthesis; GLOW-CURVE DECONVOLUTION; SOLID-STATE REACTION; THERMOLUMINESCENCE; SRAL2O4EU2+; DY3+; SRAL2O4-EU2+;
D O I
10.1080/10420150.2013.784910
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
In this paper, we present a detailed investigation of the thermo-luminescence (TL) kinetics of the long afterglow phosphor, Sr4Al14O25:Eu2+,Dy3+, synthesized by the combustion method. Kinetic parameters such as the activation energy (E), the frequency factor (s) and the order of kinetics (b) were calculated using Chen's formulism. The crystalline structure of the phosphor was examined using X-ray powder diffraction and transmission electron microscopy. The average particle size was found to be in the range of 45-52nm. The optimum dopant concentrations were Eu (1mol%) and that of Dy (2mol%). The TL response of the phosphor was monitored after the samples were irradiated with a -dose using a Co-60 source in the 20-800Gy range. A broad TL peak, (stretching from 328 to 410K) with a maximum at 368K was observed. With increasing irradiation dose, the main peak shifts toward higher temperatures. Symmetry factor calculations show that the main TL glow peak obeys second-order kinetics, which could be attributed to the creation of deep level traps. This means that -ray irradiation greatly affects the distribution of traps in the Sr4Al14O25:Eu2+,Dy3+ phosphor. The phosphor showed a linear response with -dose.
引用
收藏
页码:1022 / 1029
页数:8
相关论文
共 50 条
  • [41] Highly water resistant surface coating by fluoride on long persistent Sr4Al14O25:Eu2+/Dy3+ phosphor
    Luitel, Hom Nath
    Watari, Takanori
    Torikai, Toshio
    Yada, Mitsunori
    Chand, Rumi
    Xu, Chao-Nan
    Nanoka, Kazuhiro
    APPLIED SURFACE SCIENCE, 2010, 256 (08) : 2347 - 2352
  • [42] Luminescence characteristics of Sr4Al14O25:Eu,Dy under proton irradiation
    Toh, K.
    Nagata, S.
    Tsuchiya, B.
    Shikama, T.
    NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 2006, 249 : 209 - 212
  • [43] 复合蓄能光催化材料BiOCl/Sr4Al14O25:Eu2+,Dy3+的研究
    安惠中
    王聪
    张俊英
    郝维昌
    王天民
    稀有金属材料与工程, 2008, (10) : 1714 - 1718
  • [44] 激发波长和Eu2+的掺杂量对Sr4Al14O25∶Eu2+,Dy3+发光性能的影响
    王仁清
    发光学报, 2010, 31 (05) : 686 - 690
  • [45] 温度和B2O3量对Sr4Al14O25:Eu2+,Dy3+性能的影响
    王博
    金应荣
    西华大学学报(自然科学版), 2009, 28 (05) : 91 - 93
  • [46] Optimizing after-glow luminescent parameters of Sr4Al14O25:Eu2+, Dy3+, by sol-gel method and combustion process
    Huang, Wei-Jhe
    Su, Yen-Hsun
    Kung, Po-Yen
    Lin, Kuan-Bo
    OPTICAL AND QUANTUM ELECTRONICS, 2017, 49 (07)
  • [47] Prompt isothermal decay properties of the Sr4Al14O25 co-doped with Eu2+ and Dy3+ persistent luminescent phosphor
    Asal, Eren Karsu
    Polymeris, George S.
    Gultekin, Serdar
    Kitis, George
    NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 2018, 425 : 55 - 61
  • [48] 纳米长余辉发光材料Sr4Al14O25∶Eu2+,Dy3+的制备及性能测试
    彭子飞
    周亚丽
    徐岷
    余军保
    中国稀土学报, 2005, (S2) : 8 - 11
  • [49] Enhanced Photocatalytic Decomposition for Toluene Gas with the Heterojunction Photocatalyst of Zn-TiO2/Sr4Al14O25:Eu2+, Dy3+
    Jeong, Hye-Rin
    Kim, Jung-Sik
    TOPICS IN CATALYSIS, 2024,
  • [50] Comparative investigation on synthesis and luminescence of Sr4Al14O25:Eu2+ applied in InGaN LEDs
    Wu, Zhanchao
    Gong, Menglian
    Shi, Jianxin
    Su, Qiang
    JOURNAL OF ALLOYS AND COMPOUNDS, 2008, 458 (1-2) : 134 - 137