摘要
In power management semiconductor industry, the most comprehensively used metals in microelectronic packages include Copper, Aluminum, Nickel, Gold and Silver. When different metals contact to each other, Intermetallic Compound (IMC) will for-in at the interface. Under different conditions, IMC may vary to show very complicated characteristic and composition, some Moderate IMC will increase interfacial strength and form reliable bond, but as the brittle intermetallic compound layer thickness increases, the joint contact resistance will increase and the bonding strength will decrease. Excessive IMC growth acts as a major cause for bonding failure such as discontinuous connection, even crack or bond lift. Especially when a package undergoes reliability test of moisture and high temperature, IMC growth will accelerate much faster than in the ambient environment. This paper mainly studies the IMC growth and interfacial adhesion of At wire bond on Cu based leadframe with Bare Cu surface, Ni plated surface and Ag plated surface. The interfacial adhesion force is measured by bond shear and wire pull test at initial condition, after Temperature Cycling (TC, -65 degrees C to 150 degrees C), Autoclave (AC, Ta=121 degrees C, relative humidity =100%, Pressure=15 psi), High Temperature Storage (HTS, 150 degrees C), simulating several typical package storage and usage conditions. The failure mechanism is studied from the fracture surface characteristics and cross section analysis after different aging time. In Autoclave environment with moisture and temperature effect, At and Cu form an electrochemical couple. Because At has low electrode potential and is more active, Al acts as anode to lose electrons and corroded in the galvanic corrosion. Further more, in HAST (130C/85%RH, 80% of rated BV) test, the effect of electrical bias to galvanic corrosion is analyzed.
引用
收藏
页码:688 / 691
页数:4
相关论文
共 50 条
  • [32] Dependency of the thermal and electrical conductivity on the temperature and composition of Cu in the Al based Al-Cu alloys
    Aksoz, S.
    Ocak, Y.
    Marasli, N.
    Cadirli, E.
    Kaya, H.
    Boyuk, U.
    EXPERIMENTAL THERMAL AND FLUID SCIENCE, 2010, 34 (08) : 1507 - 1516
  • [33] Effect of some phenols on corrosion of Al, Cu, and Al-Cu alloys in NaOH solutions
    El Shayeb, HA
    El Wahab, FMA
    El Abedin, SZ
    BRITISH CORROSION JOURNAL, 1999, 34 (02): : 145 - 150
  • [34] Simultaneously increasing the strength and ductility of the modified casting Al-Cu alloy
    Zhao W.
    Wang H.
    Wang J.
    Li Y.
    Jiang Q.
    J Mater Res, 2008, 4 (1076-1081): : 1076 - 1081
  • [35] Linear friction welding of Al-Cu Part 2-Interfacial characteristics
    Dalgaard, E.
    Wanjara, P.
    Trigo, G.
    Jahazi, M.
    Comeau, G.
    Jonas, J. J.
    CANADIAN METALLURGICAL QUARTERLY, 2011, 50 (04) : 360 - 370
  • [36] Effect of γ-irradiation on the mechanical properties of Al-Cu alloy
    Abo-Elsoud, M.
    Ismail, H.
    Sobhy, Maged S.
    SURFACE REVIEW AND LETTERS, 2006, 13 (06) : 773 - 777
  • [37] Hierarchical structure in Al-Cu alloys to promote strength/ductility synergy
    Wu, S. H.
    Xue, H.
    Yang, C.
    Kuang, J.
    Zhang, P.
    Zhang, J. Y.
    Li, Y. J.
    Roven, Hans J.
    Liu, G.
    Sun, J.
    SCRIPTA MATERIALIA, 2021, 202
  • [38] Development of ultrafine grained high strength Al-Cu alloy by cryorolling
    Shanmugasundaram, T
    Murty, BS
    Sarma, VS
    SCRIPTA MATERIALIA, 2006, 54 (12) : 2013 - 2017
  • [39] Simultaneously increasing the strength and ductility of the modified casting Al-Cu alloy
    Zhao, Wengui
    Wang, Huiyuan
    Wang, Jinguo
    Li, Yong
    Jiang, Qichuan
    JOURNAL OF MATERIALS RESEARCH, 2008, 23 (04) : 1076 - 1081
  • [40] EFFECT OF STIRRING ON THE SOLIDIFICATION STRUCTURE OF AN AL-CU ALLOY
    THANH, LN
    DURAND, F
    MEMOIRES ET ETUDES SCIENTIFIQUES DE LA REVUE DE METALLURGIE, 1990, 87 (12): : 749 - 759