Effects of microstructure and carbide spheroidization on fatigue behaviour in high V-Cr-Ni cast irons

被引:36
|
作者
Tokaji, K [1 ]
Horie, T
Enomoto, Y
机构
[1] Gifu Univ, Dept Mech & Syst Engn, Gifu 5011193, Japan
[2] Okamoto Co Ltd, Gifu 5008743, Japan
[3] Hitachi Omron Terminal Solut Corp, Shinagawa Ku, Tokyo, Japan
关键词
fatigue behaviour; V-Cr-Ni cast iron; microstructure; vanadium carbide; spheroidization; crack initiation; small crack growth;
D O I
10.1016/j.ijfatigue.2005.05.009
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
This paper describes the effects of microstructure and spheroidization of vanadium carbides (VCs) on fatigue behaviour in high V-Cr-Ni cast irons. Rotary bending fatigue tests have been performed in laboratory air at ambient temperature using smooth specimens of materials with different C and V contents, i.e. microstructures and VC morphologies. The microstructure of the cast irons consisted of three distinct regions: austenitic matrix microstructure, lamellar microstructure consisting of the austenitic microstructure and (V, Cr)-carbides, and isolated VCs dispersed within them. In the materials with non-spheroidal VC, fatigue strength roughly increased with increasing C and V content, but it was found that there existed a good correlation between fatigue limit and the constituent phases of the microstructure, where fatigue limit increased as the area fraction of the larnellar microstructure increased, indicating that the lamellar microstructure was a most important microstructural variable controlling fatigue strength. The fatigue strengths of the materials with spheroidal VC decreased significantly compared with the corresponding materials with non-spheroidal VC, which was more remarkable in the material with large spheroidal VC in size. This indicated that fatigue strength was not improved by VC spheroidization. Regardless of VC morphology, crack initiation was always related to VC. Particularly, in the material with large spheroidal VC cracks were generated due to VC fracture and subsequently often grew with VC fracture and along the boundary between VC and microstructure, leading to considerably low crack initiation and growth resistance. Furthermore, it was found that the fatigue limit of the materials with spheroidal VC did not conform to the above relationship between fatigue limit and the area fraction of the lamellar microstructure. (c) 2005 Elsevier Ltd. All rights reserved.
引用
收藏
页码:281 / 288
页数:8
相关论文
共 50 条
  • [31] The effects of microstructure and temperature on the deformation heterogeneities and fatigue behaviour of a Ni-based superalloy
    Rai, R. K.
    Paulose, N.
    Sahu, J. K.
    PHILOSOPHICAL MAGAZINE, 2024, 104 (11-12) : 537 - 556
  • [32] High temperature deformation behaviour and microstructure of cast in-situ TiAl matrix composite reinforced with carbide particles
    Lapin, J.
    Pelachova, T.
    Bajana, O.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 797 : 754 - 765
  • [33] High Cr-Ni Cast Iron Base Deposits with Tantalum Carbide Particles Produced by Plasma Spraying
    Hoshiyam, Yasuhiro
    Otani, Toshiaki
    Miyake, Hidekazu
    METALLOGRAPHY XV, 2014, 782 : 563 - +
  • [34] Effect of rare earth elements on thermal fatigue of high Ni-Cr alloy cast iron
    Yang, QX
    Wang, AR
    Ren, XJ
    Wu, HQ
    JOURNAL OF RARE EARTHS, 1996, 14 (04) : 286 - 290
  • [35] Effect of Rare Earth Elements on Thermal Fatigue of High Ni-Cr Alloy Cast Iron
    杨庆祥
    王爱荣
    任学军
    吴浩泉
    JournalofRareEarths, 1996, (04) : 286 - 290
  • [36] Relationship between microstructure, hardness and corrosion resistance in 20 wt.%Cr, 27 wt.%Cr and 36 wt.%Cr high chromium cast irons
    Wiengmoon, A.
    Pearce, J. T. H.
    Chairuangsri, T.
    MATERIALS CHEMISTRY AND PHYSICS, 2011, 125 (03) : 739 - 748
  • [37] Effect of multicomponent modifier on microstructure and mechanical properties of high Ni-Cr-Mo cast iron
    Dun, X. L.
    Liu, K. P.
    Liu, H. S.
    Lai, J. P.
    Fu, X. H.
    Zhou, J.
    MATERIALS SCIENCE AND TECHNOLOGY, 2011, 27 (12) : 1840 - 1845
  • [38] Effect of Ni on microstructure and wear behaviour of 13Cr-W-Mo-2C white cast iron
    Teker, Tanju
    Yilmaz, S. Osman
    REVISTA DE METALURGIA, 2023, 59 (02)
  • [39] Effects of chromium carbide volume fraction on high-stress abrasion performance of NbC-bearing high chromium white cast irons
    Pourasiabi, Hamid
    Gates, J. D.
    WEAR, 2022, 498
  • [40] LOW CYCLE FATIGUE BEHAVIOUR OF A 1Cr-Mo-V STEEL WITH BAINITE AND FERRITE MICROSTRUCTURE.
    Bhambri, S.K.
    Prasad, C.R.
    Vasudevan, R.
    1600, (09):