Compositional variation and microstructural evolution in laser additive manufactured Ti/Ti-6Al-2Zr-1Mo-1V graded structural material

被引:40
|
作者
Liang, Yao-Jian [1 ]
Tian, Xiang-Jun [1 ]
Zhu, Yan-Yan [1 ]
Li, Jing [1 ]
Wang, Hua-Ming [1 ]
机构
[1] Beihang Univ, Sch Mat Sci & Engn, Minist Educ Laser Direct Mfg Large Metall Compone, Engn Res Ctr, Beijing 100191, Peoples R China
关键词
Laser additive manufacturing; Graded structural material; Titanium alloys; Microstructure; Hardness; PHASE EVOLUTION; TITANIUM-VANADIUM; GRADIENT MATERIAL; ALLOY; DEPOSITION; DIFFUSION;
D O I
10.1016/j.msea.2014.01.092
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The compositional variation and the microstructural evolution in laser additive manufactured Ti/Ti-6Al-2Zr-1Mo-1V graded structural material were investigated. An anomalous compositional variation and its good correlation with hardness were found. Although, during the forming process, the ratio of Ti-6Al-2Zr-1Mo-1V in feeded powders abruptly changes from 0% to 100%, all the elements exhibit a gradual variation, which is preferred to a graded material because such gradient change can decrease the discontinuity of its microstructures and properties and can remarkably reduce the costs due to the simplified manufacturing process and the rational distribution of materials. (c) 2014 Elsevier B.V. All rights reserved.
引用
收藏
页码:242 / 246
页数:5
相关论文
共 50 条
  • [41] The Dislocation Sub-structure Evolution during Hot Compressive Deformation of Ti-6Al-2Zr-1Mo-1V Alloy at 800℃
    刘勇
    Journal of Wuhan University of Technology(Materials Science), 2009, (02) : 202 - 205
  • [42] Ti-6Al-2Zr-1Mo-1V合金临界损伤因子的计算机模拟
    左晓华
    李庆丽
    铸造技术, 2014, 35 (08) : 1905 - 1907
  • [43] Loading Path Design for Grain Refinement in Hot Forming Process of Ti-6Al-2Zr-1Mo-1V Alloy
    Liu, Yingying
    Quan, Guozheng
    Yu, Yanze
    Wu, Daijian
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024,
  • [44] Cavity nucleation during hot forging of Ti-6Al-2Zr-1Mo-1V alloy with colony alpha microstructure
    Dong Xian-juan
    Lu Shi-qiang
    Zheng Hai-zhong
    Li Xin
    Ouyang De-lai
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2010, 20 (12) : 2259 - 2264
  • [45] Ti-6Al-2Zr-1Mo-1V合金的热压变形特性及塑性流动方程
    洪权
    张振祺
    赵永庆
    曲恒磊
    魏寿庸
    广东有色金属学报, 2001, (02) : 129 - 133
  • [46] 应力比对Ti-6Al-2Zr-1Mo-1V合金疲劳裂纹扩展行为的影响
    季英萍
    吴素君
    航空材料学报, 2018, 38 (03) : 72 - 76
  • [47] Effect of different temperatures and strain rates on critical damage factor of Ti-6Al-2Zr-1Mo-1V alloy
    Quan, G.-Z. (quangz_2006@yahoo.com.cn), 1600, Editorial Office of Transactions of Materials, 18 Xueqing Road, Beijing, 100083, China (34):
  • [48] Alpha texture induced fracture mechanism of laser directed energy deposited Ti-6Al-2Zr-1Mo-1V alloy with changing directions
    Li, Renka
    He, Bei
    MATERIALS LETTERS, 2022, 321
  • [49] Hot tensile deformation behavior and globularization mechanism of bimodal microstructured Ti-6Al-2Zr-1Mo-1V alloy
    Zhao, Hui-jun
    Wang, Bao-yu
    Ju, Dong-ying
    Chen, Guo-jin
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2018, 28 (12) : 2449 - 2459
  • [50] Superplasticity deformation of Ti-6Al-2Zr-1Mo-1V induced by the cyclic change of strain-rate and MaxmSPD
    Wang, G. C.
    Fu, M. W.
    Dong, H. B.
    Lu, J.
    Sun, Q. J.
    Cao, C. X.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2010, 491 (1-2) : 213 - 217