Low-temperature processing of porous SiC ceramics

被引:41
|
作者
Lim, Kwang-Young [1 ]
Kim, Young-Wook [1 ]
Song, In-Hyuck [2 ]
机构
[1] Univ Seoul, Dept Mat Sci & Engn, Funct Ceram Lab, Seoul 130743, South Korea
[2] Korea Inst Mat Sci, Engn Ceram Grp, Chang Won 641010, South Korea
关键词
SILICON-CARBIDE CERAMICS; POLYMER-DERIVED CERAMICS; OXYCARBIDE GLASSES; MECHANICAL-PROPERTIES; THERMAL-OXIDATION; MEMBRANE SUPPORT; POROSITY; FOAMS; FABRICATION; STRENGTH;
D O I
10.1007/s10853-012-6963-4
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Porous silicon carbide ceramics were fabricated from SiC, polysiloxane, and polymer microbead (as a pore former) at a temperature as low as 800 A degrees C by a simple pressing and heat-treatment process. The effects of polysiloxane and template contents on the porosity and strength of the ceramics were investigated. During heat treatment, the polysiloxane transformed to an amorphous SiOC phase, which acted as the bonding material between SiC particles, and the polymer microbeads decomposed into gases and left pores. The porosity of porous SiC ceramics could be controlled within a range of 26-56 % with the present set of processing variables. The porous SiC ceramics showed a maximal porosity of 56 % when 10 mu m SiC particles and 16 % polysiloxane were used with 20 % polymer microbeads. Flexural strength generally increased with increasing polysiloxane content and decreased with increasing polymer microbead content. Typical flexural strength of the porous SiC ceramics was 53 MPa at 42 % porosity.
引用
收藏
页码:1973 / 1979
页数:7
相关论文
共 50 条
  • [21] High-Frequency Characterization of Porous Low-Temperature Cofired Ceramics Substrates
    Bittner, Achim
    Seidel, Helmut
    Schmid, Ulrich
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2010, 93 (11) : 3778 - 3781
  • [22] Low-temperature sintering of SiC ceramics using a mixture of preceramic precursor and metal nanoparticles
    Wang, Anqi
    Nettleship, Ian
    Lee, Jung-Kun
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2024, 44 (15)
  • [23] Low-temperature reactive spark plasma sintering of dense SiC-Ti3SiC2 ceramics
    Podbolotov, Kirill
    Moskovskikh, Dmitry
    Abedi, Mohammad
    Suvorova, Veronika
    Nepapushev, Andrey
    Ostrikov, Kostya Ken
    Khort, Alexander
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2023, 43 (04) : 1343 - 1351
  • [24] Low-Temperature Synthesis of α-SiC Nanocrystals
    K. Kh. Nussupov
    N. B. Beisenkhanov
    D. I. Bakranova
    S. Keinbai
    A. A. Turakhun
    A. A. Sultan
    Physics of the Solid State, 2019, 61 : 2473 - 2479
  • [25] SINTERING OF SIC BY LOW-TEMPERATURE PLASMA
    KIJIMA, K
    KITAMURA, M
    AKIMOTO, S
    UETUKI, T
    TANAKA, K
    NIPPON SERAMIKKUSU KYOKAI GAKUJUTSU RONBUNSHI-JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1990, 98 (02): : 182 - 186
  • [26] Low-Temperature Synthesis of α-SiC Nanocrystals
    Nussupov, K. Kh.
    Beisenkhanov, N. B.
    Bakranova, D. I.
    Keinbai, S.
    Turakhun, A. A.
    Sultan, A. A.
    PHYSICS OF THE SOLID STATE, 2019, 61 (12) : 2473 - 2479
  • [27] Low-Temperature Sintering of SiC Reticulated Porous Ceramics Using Al2O3-SiO2 as Sintering Aids
    Zhao, Jing
    Ru, Hongqiang
    Wang, Wei
    Yue, Xinyan
    HIGH-PERFORMANCE CERAMICS VIII, 2014, 602-603 : 216 - 220
  • [28] Low-temperature glue for SiC composites
    不详
    AMERICAN CERAMIC SOCIETY BULLETIN, 1999, 78 (07): : 18 - 18
  • [29] LOW-TEMPERATURE SINTERING OF PZT CERAMICS
    LI, LT
    ZHANG, XW
    CHAI, JH
    FERROELECTRICS, 1990, 101 : 101 - 108
  • [30] LOW-TEMPERATURE SWELLING OF METALS AND CERAMICS
    BORODIN, VA
    RYAZANOV, AI
    SHERSTENNIKOV, DG
    JOURNAL OF NUCLEAR MATERIALS, 1993, 202 (1-2) : 169 - 179