Effects of Aging Temperature and Time on the Corrosion Protection Provided by Trivalent Chromium Process Coatings on AA2024-T3

被引:49
|
作者
Li, Liangliang [2 ]
Swain, Greg M. [1 ,2 ]
机构
[1] Michigan State Univ, Dept Chem, E Lansing, MI 48824 USA
[2] Michigan State Univ, Dept Chem Engn & Mat Sci, E Lansing, MI 48824 USA
关键词
trivalent chromium process coating; TCP; aging temperature; aging time; corrosion protection; AA2024; CHROMATE CONVERSION COATINGS; SOLUBLE HEXAVALENT CHROMIUM; PROCESS TCP COATINGS; IMPEDANCE SPECTROSCOPY; KINETICS; POROSITY; RELEASE; STORAGE; ALLOYS; FILMS;
D O I
10.1021/am4020023
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effects of aging temperature and time on the physical structure of and corrosion protection provided by trivalent chromium process (TCP) coatings on AA2024-T3 are reported. The TCP coating forms a partially blocking barrier layer on the alloy surface that consists of hydrated channels and or defects. It is through these channels and defects that ions and dissolved O-2 can be transported to small areas of the underlying alloy. Reactions initiate at these sites, which can ultimately lead to undercutting of the coating and localized corrosion. We tested the hypothesis that collapsing the channels and or reducing the number of defects in the coating might be possible through post-deposition heat treatment, and that this would enhance the corrosion protection provided by the coating. This was tested by aging the TCP-coated AA2024 alloys in air overnight at room temperature (RT), 55, 100, or 150 degrees C. The TCP coating became dehydrated and thinner at the high temperatures (55 and 100 degrees C). This improved the corrosion protection as evidenced by a 2X increase in the charge transfer resistance. Aging at 150 degrees C caused excessive coating dehydration and shrinkage. This led to severe cracking and detachment of the coating from the surface. The TCP-coated AA2024 samples were also aged in air at RT from 1 to 7 days. There was no thinning of the coating, but the corrosion protection was enhanced with a longer aging period as evidenced by a 4x increase in the charge transfer resistance. The coating became more hydrophobic after aging at elevated temperature (up to 100 degrees C) and with aging time at RT as evidenced by an increased water contact angle from 7 to 100 degrees C.
引用
收藏
页码:7923 / 7930
页数:8
相关论文
共 50 条
  • [21] Multifunctional epoxy coatings combining a mixture of traps and inhibitor loaded nanocontainers for corrosion protection of AA2024-T3
    Kartsonakis, I. A.
    Athanasopoulou, E.
    Snihirova, D.
    Martins, B.
    Koklioti, M. A.
    Montemor, M. F.
    Kordas, G.
    Charitidis, C. A.
    CORROSION SCIENCE, 2014, 85 : 147 - 159
  • [22] Influence of buffering on the spontaneous deposition of cerium conversion coatings for corrosion protection of AA2024-T3 aluminum alloy
    Stephan V. Kozhukharov
    Olaia F. Acuña
    Maria. S. Machkova
    Vladimir S. Kozhukharov
    Journal of Applied Electrochemistry, 2014, 44 : 1093 - 1105
  • [23] On the importance of irreversibility of corrosion inhibitors for active coating protection of AA2024-T3
    Visser, P.
    Terryn, H.
    Mol, J. M. C.
    CORROSION SCIENCE, 2018, 140 : 272 - 285
  • [24] Influence of buffering on the spontaneous deposition of cerium conversion coatings for corrosion protection of AA2024-T3 aluminum alloy
    Kozhukharov, Stephan V.
    Acuna, Olaia F.
    Machkova, Maria. S.
    Kozhukharov, Vladimir S.
    JOURNAL OF APPLIED ELECTROCHEMISTRY, 2014, 44 (10) : 1093 - 1105
  • [25] Corrosion Inhibition of AA2024-T3 By Sodium Silicate
    Lopez-Garrity, O.
    Frankel, G. S.
    ELECTROCHIMICA ACTA, 2014, 130 : 9 - 21
  • [26] Mechanisms of corrosion inhibition of AA2024-T3 by vanadates
    Iannuzzi, M.
    Frankel, G. S.
    CORROSION SCIENCE, 2007, 49 (05) : 2371 - 2391
  • [27] Corrosion of AA2024-T3 Part III: Propagation
    Glenn, A. M.
    Muster, T. H.
    Luo, C.
    Zhou, X.
    Thompson, G. E.
    Boag, A.
    Hughes, A. E.
    CORROSION SCIENCE, 2011, 53 (01) : 40 - 50
  • [28] Comparison of Corrosion Resistance of the AA2524-T3 and the AA2024-T3
    Queiroz, Fernanda Martins
    Terada, Maysa
    Bugarin, Aline F. Santos
    de Melo, Hercilio Gomes
    Costa, Isolda
    METALS, 2021, 11 (06)
  • [29] A Pseudoboehmite-Silane Hybrid Coating for Enhanced Corrosion Protection of AA2024-T3
    Kumar, Arun
    Kanta, A.
    Birbilis, N.
    Williams, T.
    Muddle, B. C.
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2010, 157 (10) : C346 - C356
  • [30] Corrosion Protection of AA2024-T3 by Cerium Malate and Cerium Malate-Doped Sol-Gel Coatings
    Hu, Tian-Hui
    Shi, Hong-Wei
    Wei, Tao
    Fan, Shi-Hua
    Liu, Fu-Chun
    Han, En-Hou
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2019, 32 (07) : 913 - 924