Mechanical properties of Hi-Nicalon fiber-reinforced celsian composites after high-temperature exposures in air

被引:8
|
作者
Bansal, Narottam P. [1 ]
机构
[1] NASA, Glenn Res Ctr, Struct & Mat Div, Cleveland, OH 44135 USA
关键词
Ceramic composites; Mechanical properties; SiC fibers; Barium aluminosilicate; Fiber-matrix interface; CERAMIC-MATRIX COMPOSITES; SHEAR-STRENGTH; COATINGS;
D O I
10.1016/j.jeurceramsoc.2008.06.023
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
BN/SiC-coated Hi-Nicalon fiber-reinforced celsian matrix composites (CMCs) were annealed for 100 h in air at various temperatures to 1200 degrees C, followed by flexural strength measurements at room temperature. Values of yield stress and strain, ultimate strength, and composite modulus remain almost unchanged for samples annealed up to 1100 degrees C. A thin porous layer formed on the surface of the 1100 degrees C annealed sample and its density decreased from 3.09 to 2.90 g/cm(3). The specimen annealed at. 1200 degrees C gained 0.43% weight, was severely deformed, and was covered with a porous layer of thick shiny glaze which could be easily peeled off. Some gas bubbles were also present on the surface. This surface layer consisted of elongated crystals of monoclinic celsian and some amorphous phase(s). The fibers in this surface ply of the CMC had broken into small pieces. The fiber-matrix interface strength was characterized through fiber push-in technique. Values of debond stress, sigma(d), and frictional sliding stress, tau(f), for the as-fabricated CMC were 0.31 +/- 0.14 GPa and 10.4 +/- 3.1 MPa, respectively. These values compared with 0.53 +/- 0.47 GPa and 8.33 +/- 1.72 MPa for the fibers in the interior of the 1200 degrees C annealed sample, indicating hardly any change in fiber-matrix interface strength. The effects of thermal aging on microstructure were investigated using scanning electron microscopy. Only the surface ply of the 1200 degrees C annealed specimens had degraded from oxidation whereas the bulk interior part of the CMC was unaffected. A mechanism is proposed explaining the various steps involved during the degradation of the CMC on annealing in air at 1200 degrees C. Published by Elsevier Ltd.
引用
收藏
页码:525 / 535
页数:11
相关论文
共 50 条
  • [31] Microstructural and Mechanical Characteristics of Fiber-Reinforced Cementitious Composites under High-Temperature Exposure
    Moghadam, Mehrdad Abdi
    Izadifard, Ramezan Ali
    Khalighi, Amir
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2022, 34 (09)
  • [32] RECENT DEVELOPMENTS IN FIBER-REINFORCED HIGH-TEMPERATURE CERAMIC COMPOSITES
    MAH, TI
    MENDIRATTA, MG
    KATZ, AP
    MAZDIYASNI, KS
    AMERICAN CERAMIC SOCIETY BULLETIN, 1987, 66 (02): : 304 - &
  • [33] Research on Mechanical Properties of Steel-Polypropylene Fiber-Reinforced Concrete after High-Temperature Treatments
    Shen, Xinggang
    Li, Xia
    Liu, Lei
    Chen, Xinzuo
    Du, Jun
    APPLIED SCIENCES-BASEL, 2024, 14 (09):
  • [34] Stress-temperature-lifetime response of Nicalon fiber-reinforced silicon carbide (SiC) composites in air
    Lin, HT
    Becher, PF
    THERMAL AND MECHANICAL TEST METHODS AND BEHAVIOR OF CONTINUOUS-FIBER CERAMIC COMPOSITES, 1997, 1309 : 128 - 141
  • [35] Hi-nicalon™ fiber-reinforced CVI-SiC matrix composites:: I.: Effects of PyC and PyC-SiC multilayers on the fracture behaviors and flexural properties
    Yang, W
    Araki, H
    Noda, T
    Park, JY
    Katoh, Y
    Hinoki, T
    Yu, JN
    Kohyama, A
    MATERIALS TRANSACTIONS, 2002, 43 (10) : 2568 - 2573
  • [36] Stress-temperature-lifetime working envelope of Nicalon fiber-reinforced SiC matrix composites in air
    Lin, HT
    Becher, PF
    COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 1997, 28 (11) : 935 - 942
  • [37] Correlation of high-temperature properties and interphase characteristics in oxide/oxide fiber-reinforced composites
    Saruhan, B
    Bartsch, M
    Schmücker, M
    Schneider, H
    Nubian, K
    Wahl, G
    INTERNATIONAL JOURNAL OF MATERIALS & PRODUCT TECHNOLOGY, 2001, 16 (1-3): : 259 - 268
  • [38] Effects of fiber coating composition on mechanical behavior of silicon carbide fiber-reinforced celsian composites
    Bansal, Narottam P.
    Eldridge, Jeffrey L.
    Ceramic Engineering and Science Proceedings, 1999, 20 (03): : 353 - 363
  • [39] Correlation of high-temperature properties and interphase characteristics in oxide/oxide fiber-reinforced composites
    Saruhan, B.
    Bartsch, M.
    Schmücker, M.
    Schneider, H.
    Nubian, K.
    Wahl, G.
    International Journal of Materials and Product Technology, 2001, 16 (1-3) : 259 - 268
  • [40] HIGH-TEMPERATURE MECHANICAL-BEHAVIOR OF FIBER-REINFORCED GLASS-CERAMIC-MATRIX COMPOSITES
    MAH, T
    MENDIRATTA, MG
    KATZ, AP
    RUH, R
    MAZDIYASNI, KS
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1985, 68 (09) : C248 - C251