Brittle Failure and Effect of Thermal Aging on Pb-free Solder Flip Chip Using Electroless Ni-P UBM

被引:0
|
作者
Kwon, Yong-Min [1 ]
Jeon, Young-Doo [1 ]
Paik, Kyung-Wook [1 ]
Kim, Jung-Do [2 ]
Lee, Jin-woo [2 ]
机构
[1] Korea Adv Inst Sci & Technol, Dept Mat Sci & Engn, Taejon 305701, South Korea
[2] Samsung Techwin Co LTD, Yongin 449712, South Korea
关键词
electroless Ni-P; Pb-free; brittle failure; reliability;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Electroless Ni plating is a cost effective process for manufacturing the under bump metallurgy (UBM) in a solder bump flip chip. However, Pb-free solder joints using electroless Ni UBM are prone to brittle failure during reflow and underfill processes. Hence, application of electroless Ni UBM to a Pb-free solder flip chip is restricted by low assembly yield. In order to analyze the causes of brittle failure, thermal cycling tests were performed with various solder flip chips. In the thermal cycling tests, a eutectic PbSn solder flip chip before underfill shows no brittle failure, even after 5 cycles. On the other hand, most Pb-free solder flip chips before underfill failed less than 5 cycles because of brittle failure such as Si cratering and delamination on the electroless Ni-P/Al interface. Consequently, the flip chip assembly using Pb-free solder and electroless Ni-P UBM shows low yield problem during the flip chip assembly cooling process due to the thermo-mechanical stress build at the UBM/solder joint. To reduce stress on the solder joints, the effects of additional aging after reflowing were investigated. SnAgCu solder flip chips before underfilling were aged for various times and temperatures immediately after the solder reflow process. The results showed that the yield of the assembly process was increased by about 30 percent by additional aging. Furthermore, SnAgCu solder joints aged for longer time showed better reliability in thermal cycling tests before underfilling. Measurement of the flip chip warpage reveals that the additional aging processes cause creep deformation in the solder bumps and result in smaller flip chip warpage in comparison with directly air-cooled flip chips.
引用
收藏
页码:37 / 42
页数:6
相关论文
共 50 条
  • [21] Electromigration in Pb-free flip chip solder joints on flexible substrates
    Nah, J.W.
    Ren, Fei
    Tu, K.N.
    Venk, Sridharan
    Camara, Gabe
    Journal of Applied Physics, 2006, 99 (02): : 1 - 6
  • [22] Electromigration and Thermomigration in Pb-Free Flip-Chip Solder Joints
    Chen, Chih
    Tong, H. M.
    Tu, K. N.
    ANNUAL REVIEW OF MATERIALS RESEARCH, VOL 40, 2010, 40 : 531 - 555
  • [23] Effect of electoless Ni/Au UBM thickness on mechanical and electromigration relibility of Pb-free solder joints
    Kwon, Yong-Min
    Paik, Kyung-Wook
    2007 INTERNATIONAL CONFERENCE ON ELECTRONIC MATERIALS AND PACKAGING, 2007, : 305 - 309
  • [24] Transmission electron microscopy of interfaces in joints between Pb-free solders and electroless Ni-P
    Torazawa, N
    Arai, S
    Takase, Y
    Sasaki, K
    Sakai, H
    MATERIALS TRANSACTIONS, 2003, 44 (07) : 1438 - 1447
  • [25] An evaluation of electromigration performance of SnPb and Pb-free flip chip solder joints
    Su, P
    Ding, M
    Uehling, T
    Wontor, D
    Ho, PS
    55TH ELECTRONIC COMPONENTS & TECHNOLOGY CONFERENCE, VOLS 1 AND 2, 2005 PROCEEDINGS, 2005, : 1431 - 1436
  • [26] A Comparison Study of Electromigration Performance of Pb-free Flip Chip Solder Bumps
    Su, Peng
    Li, Li
    2009 IEEE 59TH ELECTRONIC COMPONENTS AND TECHNOLOGY CONFERENCE, VOLS 1-4, 2009, : 903 - 908
  • [27] Improvement in thermal reliability of a flip chip interconnection system joined by Pb-free solder and Au bumps
    Terashima, S
    Uno, T
    Hashino, E
    Tatsumi, K
    MATERIALS TRANSACTIONS, 2001, 42 (05) : 803 - 808
  • [28] Electromigration in Pb-free solder bumps with Cu column as flip chip joints
    Nah, Jae-Woong
    Suh, J. O.
    Tu, K. N.
    Yoon, Seung Wook
    Chong, Chai Tai
    Kripesh, V.
    Su, B. R.
    Chen, Chih
    56TH ELECTRONIC COMPONENTS & TECHNOLOGY CONFERENCE 2006, VOL 1 AND 2, PROCEEDINGS, 2006, : 657 - +
  • [29] Electric current induced brittle failure of eutectic lead and lead-free solder joints with electroless Ni-P metallization
    Kumar, Aditya
    Chen, Zhong
    Wong, C. C.
    Mhaisalkar, S. G.
    Kripesh, Vaidhyanathan
    ADVANCED ELECTRONIC PACKAGING, 2007, 968 : 141 - +
  • [30] Reliability of the Pb-free solder bump on electroless Ni under bump metallurgies
    Kim, N.S.
    Jung, S.Y.
    Oh, S.Y.
    Proc Electron Compon Technol Conf, 1600, (77-82):