Temperature stable K0.5(Nd1-xBix)0.5MoO4 microwave dielectrics ceramics with ultra-low sintering temperature
被引:35
|作者:
Pang, Li-Xia
[1
,2
]
Zhou, Di
[2
,3
,4
]
Wang, Da-Wei
[2
]
Zhao, Jin-Xiong
[5
]
Liu, Wei-Guo
[1
]
Yue, Zhen-Xing
[6
]
Reaney, Ian M.
[2
]
机构:
[1] Xian Technol Univ, Microoptoelect Syst Labs, Xian, Shaanxi, Peoples R China
[2] Univ Sheffield, Mat Sci & Engn, Sheffield, S Yorkshire, England
[3] Xi An Jiao Tong Univ, Minist Educ, Elect Mat Res Lab, Key Lab, Xian, Shaanxi, Peoples R China
[4] Xi An Jiao Tong Univ, Int Ctr Dielect Res, Xian, Shaanxi, Peoples R China
[5] State Grid Gansu Elect Power Res Inst, Lanzhou, Gansu, Peoples R China
[6] Tsinghua Univ, State Key Lab New Ceram & Fine Proc, Dept Mat Sci & Engn, Beijing, Peoples R China
基金:
英国工程与自然科学研究理事会;
关键词:
electroceramics;
LTCC;
microwaves;
PHASE EVOLUTION;
ND;
SYSTEM;
CE;
BI;
LN;
D O I:
10.1111/jace.15388
中图分类号:
TQ174 [陶瓷工业];
TB3 [工程材料学];
学科分类号:
0805 ;
080502 ;
摘要:
K-0.5(Nd1-xBix)(0.5)MoO4 (0.2x0.7) ceramics were prepared via the solid-state reaction method. All ceramics densified below 720 degrees C with a uniform microstructure. As x increased from 0.2 to 0.7, relative permittivity ((r)) increased from 13.6 to 26.2 commensurate with an increase in temperature coefficient of resonant frequency (TCF) from - 31ppm/degrees C to + 60ppm/degrees C and a decrease in Qf value (Q=quality factor; f=resonant frequency) from 23400 to 8620GHz. Optimum TCF was obtained for x=0.3 (-15ppm/degrees C) and 0.4 (+4ppm/degrees C) sintered at 660 and 620 degrees C with (r) similar to 15.4, Q(f) similar to 19650GHz, and (r) similar to 17.3, Q(f) similar to 13050GHz, respectively. Ceramics in this novel solid solution are a candidate for ultra low temperature co-fired ceramic (ULTCC) technology.