Wear of ceramic-on-carbon fiber-reinforced poly-ether ether ketone hip replacements

被引:62
|
作者
Brockett, Claire L. [1 ]
John, Gemma [2 ]
Williams, Sophie [1 ]
Jin, Zhongmin [1 ]
Isaac, Graham H. [1 ,2 ]
Fisher, John [1 ]
机构
[1] Univ Leeds, Inst Med & Biol Engn, Sch Mech Engn, Leeds LS2 9JT, W Yorkshire, England
[2] DePuy Int Ltd, Leeds, W Yorkshire, England
基金
英国工程与自然科学研究理事会; 美国国家卫生研究院; 英国惠康基金;
关键词
hip replacement; wear; friction; carbon fiber-reinforced PEEK; MOLECULAR-WEIGHT POLYETHYLENE; JOINT SIMULATOR; IN-VITRO; DEBRIS; PEEK; RESISTANCE; SQUEAKING; BEARINGS; FRICTION; IMPLANTS;
D O I
10.1002/jbm.b.32664
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Total hip replacement has been a successful surgical intervention for over 50 years, with the majority of bearings using a polyethylene cup. Long-term failure due to osteolysis and loosening has been widely documented and alternative bearings have been sought. A novel carbon fiber-reinforced poly-ether ether ketone (CFR-PEEK) cup was investigated through experimental friction and wear studies. Friction studies demonstrated the bearings operated in a boundary lubrication condition, with friction factors higher than those for other hip replacement bearings. The wear study was conducted with 36 mm diameter bearings tested against Biolox Delta heads for a period of 10 million cycles. The mean volumetric wear rate was 0.3 mm3/Mc, indicating the ceramic-on-CFR-PEEK bearing to be a very low wearing option for total hip replacement. (c) 2012 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater 100B: 14591465, 2012.
引用
收藏
页码:1459 / 1465
页数:7
相关论文
共 50 条
  • [41] Modified Continuous Carbon Fiber-Reinforced Poly(phthalazinone ether sulfone ketone) Composites by Blending Polyetherimide and Polyethersulfone
    Zheng, Liang
    Liao, Gong-Xiong
    Gu, Tie-Sheng
    Han, Yong-Jin
    Jian, Xi-Gao
    POLYMER COMPOSITES, 2009, 30 (12) : 1842 - 1847
  • [42] Additive manufacturing of continuous carbon fiber reinforced poly-ether-ether-ketone with ultrahigh mechanical properties
    Chang, Baoning
    Li, Xuemu
    Parandoush, Pedram
    Ruan, Shilun
    Shen, Changyu
    Lin, Dong
    POLYMER TESTING, 2020, 88
  • [43] Comparative study of the crystallization behavior and morphologies of carbon and glass fiber reinforced poly(ether ether ketone) composites
    Wang, Pan
    Lin, Qing
    Wang, Yaming
    Liu, Chuntai
    Shen, Changyu
    POLYMERS & POLYMER COMPOSITES, 2021, 29 (08): : 1229 - 1239
  • [44] Miner's rule for fatigue life of short carbon fiber reinforced poly-ether-ether-ketone
    Noguchi, Hiroshi
    Nishizawa, Akio
    Nisitani, Hironobu
    Kim, Yun-Hae
    Zairyo/Journal of the Society of Materials Science, Japan, 1994, 43 (489) : 672 - 678
  • [45] FAILURE MECHANISMS IN CARBON-FIBER REINFORCED POLY(ETHER ETHER KETONE) .2. MATERIAL VARIABLES
    HINE, PJ
    BREW, B
    DUCKETT, RA
    WARD, IM
    COMPOSITES SCIENCE AND TECHNOLOGY, 1991, 40 (01) : 47 - 67
  • [46] Enhanced glass fiber-reinforced phenolphthalein poly(ether ketone) composites by blending poly(phenylene sulfide)
    Yang, YM
    Li, BY
    Dong, LS
    JOURNAL OF APPLIED POLYMER SCIENCE, 1996, 59 (03) : 531 - 535
  • [47] Model for thermal degradation of carbon fiber filled poly(ether ether ketone)
    Dolo, Guillaume
    Ferec, Julien
    Cartie, Denis
    Grohens, Yves
    Ausias, Gilles
    POLYMER DEGRADATION AND STABILITY, 2017, 143 : 20 - 25
  • [48] Preparation and properties of graphene/carbon fiber/poly(ether ether ketone) composites
    Jing, De-Qi (jingdq@sxicc.ac.cn), 1600, Institute of Metal Research Chinese Academy of Sciences (32):
  • [49] Preparation and properties of graphene/carbon fiber/poly(ether ether ketone) composites
    Su Ya-nan
    Zhang Shou-chun
    Zhang Xing-hua
    Zhao Zhen-bo
    Chen Cheng-meng
    Jing De-qi
    NEW CARBON MATERIALS, 2017, 32 (02) : 152 - 159
  • [50] Thermal characterizations of basalt fiber-reinforced poly(aryl-ether-ketone) biomedical composites
    Alice, A. Queen
    Kumar, A. Arul Jeya
    Prakash, M.
    Kumar, I. Ashok
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2022, 147 (03) : 1945 - 1953