Pb-free BGA Solder Joint Reliability Improvement with Sn3.5Ag Solder Alloy on Ni/Au Finish

被引:0
|
作者
Leng, Eu Poh [1 ]
Ding, Min [2 ]
Lindsay, Wayne [2 ]
Chopin, Sheila [2 ]
Ahmad, Ibrahim [3 ]
Jalar, Azman [4 ]
机构
[1] Freescale Semicond Malaysia Sdn Bhd, 2 Jalan SS 8-2 Free Ind Zone,Sungei Way Petaling, Petaling Jaya 47300, Malaysia
[2] Freescale Semicond Inc, Drive West, TX 78735 USA
[3] Natl Univ Malaysia, Fac Engn, Dept Elect & Elect Syst, Bangi 43600, Malaysia
[4] Natl Univ Malaysia, Fac Sci & Technol, Bangi 43600, Malaysia
关键词
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this work, Sn3.5Ag solder alloy was being studied for the purpose of Pb-free solder joint reliability improvement over conventional Sn3.8AgO.7Cu solder balls on Ball Grid Array (BGA) packages with Ni/Au pad finishing. The study was carried out in different levels. At individual solder joint level, Sn3.5Ag showed no intermetallic brittle failure in cold ball pull test even upto 6x multiple reflow and 168hrs high temperature storage for TBGA & TePBGA, and 504hrs high temperature storage for PBGA Spanish Oak. In contrast, 70 similar to 100% of the failure mode of SAC387 was brittle failure. At package level, Sn3.5Ag survived 8 similar to 10x more drop cycles than SAC387 in tray drop and packing drop tests. These results indicate that the mechanical strength of Sn3.5Ag on Ni/Au pad is considerably stronger than that of SAC387. The difference in mechanical strength between the two alloys was correlated to their microstructures. At the same time, board level solder joint reliability tests such as thermal cycling and mechanical bend test were carried out. Sn3.5Ag showed better or similar performance as SAC387.
引用
收藏
页码:131 / +
页数:2
相关论文
共 50 条
  • [41] Current-induced weakening of Sn3.5Ag0.7Cu Pb-free solder joints
    Zhang, L.
    Wang, Z. G.
    Shang, J. K.
    SCRIPTA MATERIALIA, 2007, 56 (05) : 381 - 384
  • [42] Bend fatigue reliability test and analysis for Pb-free solder joint
    Che, FX
    Pang, HLJ
    PROCEEDINGS OF THE 7TH ELECTRONICS PACKAGING TECHNOLOGY CONFERENCE, VOLS. 1 AND 2, 2005, : 868 - 872
  • [43] Optimization of Pb-Free Solder Joint Reliability from a Metallurgical Perspective
    Zeng, Kejun
    Pierce, Mike
    Miyazaki, Hiroshi
    Holdford, Becky
    JOURNAL OF ELECTRONIC MATERIALS, 2012, 41 (02) : 253 - 261
  • [44] Effects of load and thermal conditions on Pb-free solder joint reliability
    J. Liang
    S. Downes
    N. Dariavach
    D. Shangguan
    S. M. Heinrich
    Journal of Electronic Materials, 2004, 33 : 1507 - 1515
  • [45] Low-cycle fatigue prediction model for pb-free solder 96.5Sn-3.5Ag
    C. Kanchanomai
    Y. Mutoh
    Journal of Electronic Materials, 2004, 33 : 329 - 333
  • [46] Low-cycle fatigue prediction model for Pb-free solder 96.5Sn-3.5Ag
    Kanchanomai, C
    Mutoh, Y
    JOURNAL OF ELECTRONIC MATERIALS, 2004, 33 (04) : 329 - 333
  • [47] IMC morphology, interfacial reaction and joint reliability of Pb-free Sn-Ag-Cu solder on electrolytic NiBGA substrate
    Yoon, JW
    Kim, SW
    Jung, SB
    JOURNAL OF ALLOYS AND COMPOUNDS, 2005, 392 (1-2) : 247 - 252
  • [48] Effect of Ag and Cu content in Sn based Pb-free solder on Electromigration
    Lu, Minhua
    Goldsmith, Charles
    Wassick, Thomas
    Perfecto, Eric
    Arvin, Charles
    2014 IEEE 64TH ELECTRONIC COMPONENTS AND TECHNOLOGY CONFERENCE (ECTC), 2014, : 1940 - 1943
  • [49] The growth of intermetallic compound in Cu/Sn3.5Ag/Au solder joints under current stressing
    Chiu, Tsung-Chieh
    Lin, Kwang-Lung
    INTERMETALLICS, 2012, 23 : 208 - 216
  • [50] A perspective on effect by Ag addition to corrosion evolution of Pb-free Sn solder
    Qiao, Chuang
    Sun, Xu
    Wang, Youzhi
    Hao, Long
    An, Xizhong
    MATERIALS LETTERS, 2021, 297