Flexural strengths, failure load, and hardness of glass-ceramics for dental applications

被引:8
|
作者
Alghazzawi, Tariq F. [1 ,2 ,3 ]
机构
[1] Taibah Univ, Dept Substitut Dent Sci, Madina, Saudi Arabia
[2] Univ Alabama Birmingham, Dept Mat Sci & Engn, Birmingham, AL USA
[3] POB 51209, Riyadh 11543, Saudi Arabia
来源
JOURNAL OF PROSTHETIC DENTISTRY | 2022年 / 128卷 / 03期
关键词
MECHANICAL-PROPERTIES; FRACTURE-RESISTANCE; CROWNS;
D O I
10.1016/j.prosdent.2022.05.023
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Statement of problem. Glass-ceramics are often selected for use in dental restorations based upon advertised flexural strengths obtained from standardized tests on prefabricated specimens (bars and disks); these may not accurately reflect their performance in dental applications. Purpose. The purpose of this in vitro study was to determine and compare 4-point flexural strength, biaxial flexural strength, hardness, and crown failure loads for 3 commercially available glass-ceramics. Material and methods. Specimens were pressed and prepared from 3 brands of glass-ceramics: Celtra (CEL), IPS e.max (EMA), and Lisi (LIS). Rectangular bars, circular disks, and fully contoured crowns were created (n=15 specimens per glass-ceramic, 45 specimens per geometry, totaling 135 specimens). Disks were tested for biaxial flexural strength by using a piston-on-3-ball (POB) test, while bars were tested for 4-point flexural strength by using 4-point bending (4PB) and Vickers hardness (VH) tests. Crown failure loads were assessed in "crunch-the-crown " (CTC) tests. The results were analyzed by using general linear modeling, the Pearson correlation coefficient, and Weibull analysis. Results. The general linear modeling revealed significant differences (P <.05) in the failure load for crown specimens (EMA > LIS > CEL), the 4-point flexural strength (EMA > LIS > CEL), and the biaxial flexural strength (EMA > LIS=CEL). The disk specimens had higher flexural strengths than the bar specimens for CEL and EMA materials. LIS had a higher Weibull modulus than EMA and CEL for bar and crown specimens. CEL had a higher Weibull modulus than LIS and EMA for disk specimens. There was no correlation among the VH (R-2=0.86 and P=.24), biaxial flexural strength (R-2=0.84 and P=.26), and crown failure load. However, there was a high correlation between the failure load (crown specimens) and 4-point flexural strength (bar specimens) (R2=0.99 and P=.03). Conclusions. The 4-point flexural strength correlated significantly with crown failure load.
引用
收藏
页码:512.e1 / 512.e9
页数:9
相关论文
共 50 条
  • [31] Clinical applications of glass-ceramics in dentistry
    Wolfram Höland
    Volker Rheinberger
    Elke Apel
    Christian van ’t Hoen
    Marlies Höland
    Alex Dommann
    Marcel Obrecht
    Corinna Mauth
    Ursula Graf-Hausner
    Journal of Materials Science: Materials in Medicine, 2006, 17 : 1037 - 1042
  • [32] Molded Glass-Ceramics for Infrared Applications
    Roze, Mathieu
    Calvez, Laurent
    Hubert, Mathieu
    Toupin, Perrine
    Bureau, Bruno
    Boussard-Pledel, Catherine
    Zhang, Xiang-Hua
    INTERNATIONAL JOURNAL OF APPLIED GLASS SCIENCE, 2011, 2 (02) : 129 - 136
  • [33] Clinical applications of glass-ceramics in dentistry
    Hoeland, Wolfram
    Rheinberger, Volker
    Apel, Elke
    van't Hoen, Christian
    Hoeland, Marlies
    Dommann, Alex
    Obrecht, Marcel
    Mauth, Corinna
    Graf-Husner, Ursula
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN MEDICINE, 2006, 17 (11) : 1037 - 1042
  • [34] Glass-ceramics for special applications - Preface
    Schaeffer, HA
    GLASS SCIENCE AND TECHNOLOGY-GLASTECHNISCHE BERICHTE, 2000, 73 : V - V
  • [35] Transparent glass-ceramics for optical applications
    O. Dymshits
    M. Shepilov
    A. Zhilin
    MRS Bulletin, 2017, 42 : 200 - 205
  • [36] Transparent glass-ceramics for optical applications
    Dymshits, O.
    Shepilov, M.
    Zhilin, A.
    MRS BULLETIN, 2017, 42 (03) : 200 - 205
  • [37] STRUCTURE, PROPERTIES AND APPLICATIONS OF GLASS-CERAMICS
    BEALL, GH
    AMERICAN CERAMIC SOCIETY BULLETIN, 1971, 50 (04): : 416 - &
  • [38] Impact of Experimental Protocols on the Flexural Strength Testing of Lithium Disilicate-Based Dental Glass-Ceramics
    Xu, Xinyi
    Young, Joseph
    Goel, Ashutosh
    TRANSACTIONS OF THE INDIAN CERAMIC SOCIETY, 2021, 80 (04) : 258 - 264
  • [39] Nucleation efficacy and flexural strength of novel leucite glass-ceramics
    Cattell, Michael J.
    Patzig, Christian
    Bissasu, Sami
    Tsoutsos, Andreas
    Karpukhina, Natalia
    DENTAL MATERIALS, 2020, 36 (05) : 592 - 602
  • [40] Study of local Silica sand deposits for producing Leucite Glass-ceramics for dental applications
    Nurddin, Siti Mazatul Azwa Saiyed Mohd
    Selamat, Malek
    MALAYSIAN JOURNAL OF FUNDAMENTAL AND APPLIED SCIENCES, 2014, 10 (04): : 169 - 173