Flexural strengths, failure load, and hardness of glass-ceramics for dental applications

被引:8
|
作者
Alghazzawi, Tariq F. [1 ,2 ,3 ]
机构
[1] Taibah Univ, Dept Substitut Dent Sci, Madina, Saudi Arabia
[2] Univ Alabama Birmingham, Dept Mat Sci & Engn, Birmingham, AL USA
[3] POB 51209, Riyadh 11543, Saudi Arabia
来源
JOURNAL OF PROSTHETIC DENTISTRY | 2022年 / 128卷 / 03期
关键词
MECHANICAL-PROPERTIES; FRACTURE-RESISTANCE; CROWNS;
D O I
10.1016/j.prosdent.2022.05.023
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Statement of problem. Glass-ceramics are often selected for use in dental restorations based upon advertised flexural strengths obtained from standardized tests on prefabricated specimens (bars and disks); these may not accurately reflect their performance in dental applications. Purpose. The purpose of this in vitro study was to determine and compare 4-point flexural strength, biaxial flexural strength, hardness, and crown failure loads for 3 commercially available glass-ceramics. Material and methods. Specimens were pressed and prepared from 3 brands of glass-ceramics: Celtra (CEL), IPS e.max (EMA), and Lisi (LIS). Rectangular bars, circular disks, and fully contoured crowns were created (n=15 specimens per glass-ceramic, 45 specimens per geometry, totaling 135 specimens). Disks were tested for biaxial flexural strength by using a piston-on-3-ball (POB) test, while bars were tested for 4-point flexural strength by using 4-point bending (4PB) and Vickers hardness (VH) tests. Crown failure loads were assessed in "crunch-the-crown " (CTC) tests. The results were analyzed by using general linear modeling, the Pearson correlation coefficient, and Weibull analysis. Results. The general linear modeling revealed significant differences (P <.05) in the failure load for crown specimens (EMA > LIS > CEL), the 4-point flexural strength (EMA > LIS > CEL), and the biaxial flexural strength (EMA > LIS=CEL). The disk specimens had higher flexural strengths than the bar specimens for CEL and EMA materials. LIS had a higher Weibull modulus than EMA and CEL for bar and crown specimens. CEL had a higher Weibull modulus than LIS and EMA for disk specimens. There was no correlation among the VH (R-2=0.86 and P=.24), biaxial flexural strength (R-2=0.84 and P=.26), and crown failure load. However, there was a high correlation between the failure load (crown specimens) and 4-point flexural strength (bar specimens) (R2=0.99 and P=.03). Conclusions. The 4-point flexural strength correlated significantly with crown failure load.
引用
收藏
页码:512.e1 / 512.e9
页数:9
相关论文
共 50 条
  • [1] GLASS-CERAMICS FOR DENTAL APPLICATIONS
    WALSH, J
    HATTON, PV
    JOHNSON, A
    CLIFFORD, A
    HILL, R
    JOURNAL OF DENTAL RESEARCH, 1995, 74 (03) : 895 - 895
  • [2] Sintered glass-ceramics for dental applications
    Höland, W
    Rheinberger, V
    Schweiger, M
    GLASS SCIENCE AND TECHNOLOGY, 2003, 76 : 48 - 53
  • [3] Preparation of nepheline glass-ceramics for dental applications
    Hamawy, Esmat M. A.
    El-Meliegy, Emad A. M.
    MATERIALS CHEMISTRY AND PHYSICS, 2008, 112 (02) : 432 - 435
  • [4] Hardness of basaltic glass-ceramics
    Section of Chemistry, Aalborg University, DK-9000 Aalborg, Denmark
    不详
    Glass Technol. Euro. J. Glass Sci. Technol. Part A, 2009, 4 (189-195):
  • [5] Hardness of basaltic glass-ceramics
    Jensen, M.
    Smedskjaer, M. M.
    Estrup, M.
    Kristjansson, M.
    Lonnroth, N.
    Yue, Y. Z.
    GLASS TECHNOLOGY-EUROPEAN JOURNAL OF GLASS SCIENCE AND TECHNOLOGY PART A, 2009, 50 (04): : 189 - 195
  • [6] Novel Testing for Corrosion of Glass-Ceramics for Dental Applications
    Esquivel-Upshaw, J. F.
    Ren, F.
    Hsu, S. M.
    Dieng, F. Y.
    Neal, D.
    Clark, A. E.
    JOURNAL OF DENTAL RESEARCH, 2018, 97 (03) : 296 - 302
  • [7] Lithium Disilicate based Glass-Ceramics for Dental Applications
    Gaddam, Anuraag
    Goyal, Mudit
    Jain, Sudhanshu
    Bhargava, Parag
    TRANSACTIONS OF THE INDIAN CERAMIC SOCIETY, 2013, 72 (01) : 56 - 60
  • [8] Novel Coating to Minimize Corrosion of Glass-Ceramics for Dental Applications
    Hsu, Shu-Min
    Ren, Fan
    Chen, Zhiting
    Kim, Mijin
    Fares, Chaker
    Clark, Arthur E.
    Neal, Dan
    Esquivel-Upshaw, Josephine F.
    MATERIALS, 2020, 13 (05)
  • [9] Synthesis and characterization of wollastonite glass-ceramics for dental implant applications
    Saadaldin, Selma A.
    Rizkalla, Amin S.
    DENTAL MATERIALS, 2014, 30 (03) : 364 - 371
  • [10] Bioactive and inert dental glass-ceramics
    Montazerian, Maziar
    Zanotto, Edgar Dutra
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART A, 2017, 105 (02) : 619 - 639