Effect of heating rate of final annealing stage on secondary recrystallization in grain-oriented silicon steel

被引:4
|
作者
Fan, Lifeng [1 ,2 ]
Zhao, Xingyuan [1 ]
Zhu, Rong [1 ]
He, Jianzhong [3 ]
Zhang, Yuan Xiang [4 ]
机构
[1] Inner Mongolia Univ Technol, Sch Mat Sci & Engn, Hohhot 010000, Peoples R China
[2] Inner Mongolia Univ Technol, Sch Mat Sci & Engn, Inner Mongolia Key Lab Thin Film & Coatings, Hohhot 010051, Peoples R China
[3] Inner Mongolia Baotou Steel Union Co Ltd, Baotou 014010, Inner Mongolia, Peoples R China
[4] State Key Lab Rolling & Automat, Shenyang 110819, Peoples R China
基金
中国国家自然科学基金;
关键词
Grain-oriented silicon steel; heating rate; inhibitor; secondary recrystallization; texture; TEXTURE DEVELOPMENT; MAGNETIC-PROPERTIES; EVOLUTION; IRON; SI;
D O I
10.1051/metal/2020063
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
A grain-oriented silicon steel sheet was manufactured by slab reheated at "medium temperature" and two-stage cold rolling method. The function of heating rate on secondary recrystallization in grain-oriented silicon steel was investigated. The results show that: compared with 30 degrees C/h heating rate, the initial temperature of the secondary recrystallization can increase by 10 degrees C at the heating rate of 20 degrees C/h. Furthermore, the temperature region of secondary recrystallization also extended either with the increased heating rate. Even though the inhibitors maintain AlN, complex precipitation of AlN and sulphide in both heating rate, the average diameter and Zener factor of inhibitors are distinct. Inhibitors in the route of 20 degrees C/h heating rate express stronger inhibition than that of 30 degrees C/h, and the average diameter and Zener factor are 17.519nm and 3.925x10(-4)nm(-1), respectively. In addition, more Goss texture component and less gamma -fiber texture ({111}//ND) component form at the heating rate of 30 degrees C/h than 20 degrees C/h at 1000 degrees C, but the final Goss texture component of 20 degrees C/h is greater than 30 degrees C/h. The average grain size of the final annealing sheets increased with the heating rate decreasing from 30 degrees C/h to 20 degrees C/h, and iron loss reduced by 0.05W/Kg, the magnetic induction intensity increased by 0.025T.
引用
收藏
页数:11
相关论文
共 50 条
  • [21] STUDY ON THE SECONDARY RECRYSTALLIZATION BEHAVIOR OF GRAIN-ORIENTED SILICON STEEL CONTAINING ALN AS AN INHIBITOR .6. EFFECT OF COINCIDENCE BOUNDARIES ON THE SECONDARY RECRYSTALLIZATION BEHAVIOR OF GRAIN-ORIENTED SILICON STEEL CONTAINING ALN AS AN INHIBITOR
    HARASE, J
    SHIMIZU, R
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 26 (11) : B350 - B350
  • [22] EFFECT OF INITIAL TEXTURE ON SECONDARY RECRYSTALLIZATION OF GRAIN-ORIENTED ELECTRICAL STEEL
    IWANAGA, I
    MASUI, H
    HARASE, J
    IWAYAMA, K
    TAKAHASHI, N
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 1994, 3 (02) : 223 - 227
  • [23] Orientation Selection Behavior During Secondary Recrystallization in Grain-Oriented Silicon Steel
    Xu Zhanyi
    Sha Yuhui
    Zhang Fang
    Zhang Huabing
    Li Guobao
    Chu Shuangjie
    Zuo Liang
    ACTA METALLURGICA SINICA, 2020, 56 (08) : 1067 - 1074
  • [24] EFFECT OF FINAL ANNEALING ATMOSPHERE ON SECONDARY RECRYSTALLIZATION BEHAVIOR IN THIN GAUGE MEDIUM TEMPERATURE GRAIN ORIENTED SILICON STEEL
    Liu Gongtao
    Yang Ping
    Mao Weimin
    ACTA METALLURGICA SINICA, 2016, 52 (01) : 25 - 32
  • [26] Mechanism of Secondary Recrystallization in Grain-Oriented Si Steel
    Ushigami, Yoshiyuki
    Nakamura, Shuichi
    RECRYSTALLIZATION AND GRAIN GROWTH IV, 2012, 715-716 : 122 - 127
  • [27] Complete Goss Secondary Recrystallization by Control of the Grain Size and Texture of Primary Recrystallization in Grain-Oriented Silicon Steel
    Xu, Zhanyi
    Sha, Yuhui
    He, Zhenghua
    Zhang, Fang
    Liu, Wei
    Zhang, Huabing
    Zuo, Liang
    MATERIALS, 2021, 14 (18)
  • [28] CREEP STRENGTH SECONDARY RECRYSTALLIZATION + GRAIN-BOUNDARY MOBILITY IN GRAIN-ORIENTED SILICON STEEL
    LENHART, RE
    JOM-JOURNAL OF METALS, 1964, 16 (01): : 117 - &
  • [29] EFFECT OF FINAL THICKNESS ON SECONDARY RECRYSTALLIZATION OF GRAIN-ORIENTED ELECTRICAL STEEL PRODUCED BY SINGLE-STAGE COLD-ROLLING PROCESS
    NAKASHIMA, S
    TAKASHIMA, K
    HARASE, J
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1991, 55 (08) : 898 - 906
  • [30] Effects of Normalizing Annealing on Grain-oriented Silicon Steel
    Ling, Chen
    Xiang, Li
    Qiu, Sheng-tao
    Gan, Yong
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2014, 21 (07) : 690 - 694