Comparative Performance of Silicone Rubber Insulators with IEC Stipulated Test Methods

被引:0
|
作者
Vasudev, N. [1 ]
Vynatheya, S. [1 ]
Senthilkumar, R. T. [2 ]
机构
[1] Cent Power Res Inst, Bangalore, Karnataka, India
[2] KS Rangasamy coll Technol, Tiruchengode, Tamil Nadu, India
关键词
accelerated ageing; pollution; polymeric insulator; rotating wheel dip test; salt fog test;
D O I
暂无
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
IEC standard 61109 /62217 stipulates three alternatives for design tests for polymeric insulators, namely (a) tracking and erosion test(1000hours), (b) track wheel test (30,000 cycles) and (c) multi-stress ageing test (5000 hours). The minimum requirement for the insulator to comply with the design test is compliance with any one of these tests. However, experience in carrying out these tests in CPRI indicate that the assess the relative merits of the tracking and erosion test and the track wheel test, both the tests were carried out on a 33 kV polymeric insulator. Both the tests were terminated after 1000 hours. The results indicate track wheel test is severe. Analytical tests such as hydrophobicity test, EDX and XRD tests were performed to check the degree of degradation of the insulator material.
引用
收藏
页数:4
相关论文
共 50 条
  • [21] Long Term Ageing Performance of Silicone Rubber Insulators Under Different Conditions
    Vasudev, N.
    Nambudri, P. V. Vasudevan
    Dinesh, M. N.
    Ravi, K. N.
    Krishnan, V.
    ICPADM 2009: PROCEEDINGS OF THE 9TH INTERNATIONAL CONFERENCE ON PROPERTIES AND APPLICATIONS OF DIELECTRIC MATERIALS, VOLS 1-3, 2009, : 276 - +
  • [22] Hydrophobicity lifetime of silicone rubber composite insulators
    Lu, Zhiwei
    Gaoya Dianqi/High Voltage Apparatus, 2000, 36 (01): : 39 - 40
  • [23] Degradation Monitoring of Silicone Rubber Used for Insulators
    Khaing, May Thin
    Yoshimura, Kosei
    Sakoda, Tatsuya
    Oasa, Junki
    Higashiyama, Shoichi
    Inaoka, Yuko
    2022 9TH INTERNATIONAL CONFERENCE ON CONDITION MONITORING AND DIAGNOSIS (CMD), 2022, : 382 - 386
  • [24] Silicone Rubber Insulators for Polluted Environments Part 2: Textured Insulators
    Albano, M.
    Charalampidis, P.
    Waters, R. T.
    Griffiths, H.
    Haddad, A.
    IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 2014, 21 (02) : 749 - 757
  • [25] Biofilms on silicone rubber insulators;: microbial composition and diagnostics of removal by use of ESEM/EDS -: Composition of biofilms infecting silicone rubber insulators
    Wallström, S
    Karlsson, S
    POLYMER DEGRADATION AND STABILITY, 2004, 85 (02) : 841 - 846
  • [26] Performance of Insulators Treated with Semiconductive Silicone Rubber Coating during Fog and Polluted conditions
    Wei, Xiaoxing
    Peng, Xiangyang
    Jia, Zhidong
    Sun, Zhenting
    Guan, Zhicheng
    PROCEEDINGS OF THE 2012 IEEE INTERNATIONAL POWER MODULATOR AND HIGH VOLTAGE CONFERENCE, 2012, : 439 - 442
  • [27] Preparation of hydrophobic silicone rubber composite insulators and the research of anti-aging performance
    Zhang, Zhaohua
    E-POLYMERS, 2024, 24 (01)
  • [28] Performance comparison and lifespan assessment of naturally and artificially chalked silicone rubber for composite insulators
    Zeng, Shiyin
    Zhao, Xin
    Li, Wendong
    Peng, Yanan
    Liu, Yuelin
    Yan, Xinyi
    Zhang, Guanjun
    POLYMER DEGRADATION AND STABILITY, 2025, 232
  • [29] Influence of shed parameters on the aging performance of silicone rubber insulators in salt-fog
    El-Hag, AH
    Jayaram, SH
    Cherney, EA
    IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 2003, 10 (04) : 655 - 664
  • [30] Improving surface performance of silicone rubber for composite insulators by multifunctional Nano-coating
    Liu, Shuming
    Liu, Shuqi
    Wang, Qian
    Zuo, Zhou
    Wei, Lan
    Chen, Zhong
    Liang, Xidong
    CHEMICAL ENGINEERING JOURNAL, 2023, 451