Effect of core design on fracture resistance of zirconia-lithium disilicate anterior bilayered crowns

被引:1
|
作者
Ko, Kyung-Ho
Park, Chan-Jin
Cho, Lee-Ra
Huh, Yoon-Hyuk
机构
[1] Gangneung Wonju Natl Univ, Coll Dent, Dept Prosthodont, Kangnung, South Korea
[2] Gangneung Wonju Natl Univ, Coll Dent, Res Inst Oral Sci, Kangnung, South Korea
来源
JOURNAL OF ADVANCED PROSTHODONTICS | 2020年 / 12卷 / 04期
基金
新加坡国家研究基金会;
关键词
Lithium disilicate; Zirconia; Metal-ceramic crown; Fracture resistance; FIXED DENTAL PROSTHESES; METAL; STRENGTH; TRANSLUCENCY; THICKNESS; STABILITY; STUDENTS; LINER;
D O I
10.4047/jap.2020.12.4.181
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
PURPOSE. The effect of core design on the fracture resistance of zirconia-lithium disilicate (LS2) bilayered crowns for anterior teeth is evaluated by comparing with that of metal-ceramic crowns. MATERIALS AND METHODS. Forty customized titanium abutments for maxillary central incisor were prepared. Each group of 10 units was constructed using the same veneer form of designs A and B, which covered labial surface to approximately one third of the incisal and cervical palatal surface, respectively. 1.52 pressed-on-zirconia (POZ) and porcelain-fused-to-metal (PFM) crowns were divided into "POZ_A," "POZ_B," "PFM_A," and "PFM_B" groups, and 6000 thermal cycles (5/55 degrees C) were performed after 24 h storage in distilled water at 37 degrees C. All specimens were prepared using a single type of self-adhesive resin cement. The fracture resistance was measured using a universal testing machine. Failure mode and elemental analyses of the bonding interface were performed. The data were analyzed using Welch's t-test and the Games-Howell exact test. RESULTS. The PFM_B (1376.8 +/- 93.3 N) group demonstrated significantly higher fracture strength than the PFM_A (915.8 +/- 206.3 N) and POZ_B (963.8 +/- 316.2 N) groups (P<.05). There was no statistically significant difference in fracture resistance between the POZ_A (1184.4 +/- .319.6 N) and POZ_B groups (P>.05). Regardless of the design differences of the zirconia cores, fractures involving cores occurred in all specimens of the POZ groups. CONCLUSION. The bilayered anterior POZ crowns showed different fracture resistance arid fracture pattern according to the core design compared to PFM.
引用
收藏
页码:181 / 188
页数:8
相关论文
共 50 条
  • [1] Comparison of fracture resistance and fracture characterization of bilayered zirconia/fluorapatite and monolithic lithium disilicate all ceramic crowns
    Altamimi, Abdulaziz M.
    Tripodakis, Aris Petros D.
    Eliades, George
    Hirayama, Hiroshi
    INTERNATIONAL JOURNAL OF ESTHETIC DENTISTRY, 2014, 9 (01): : 98 - 110
  • [2] Effects of the Thickness Ratio of Zirconia-Lithium Disilicate Bilayered Ceramics on the Translucency and Flexural Strength
    Kim, Jong-Hoi
    Ko, Kyung-Ho
    Huh, Yoon-Hyuk
    Park, Chan-Jin
    Cho, Lee-Ra
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2020, 29 (04): : 334 - 340
  • [3] Fracture Strength After Fatigue Loading of Lithium Disilicate Pressed Zirconia Crowns
    Kim, So-Yeun
    Choi, Jae-Won
    Ju, Sung-Won
    Ahn, Jin-Soo
    Yoon, Mi-Jung
    Huh, Jung-Bo
    INTERNATIONAL JOURNAL OF PROSTHODONTICS, 2016, 29 (04) : 369 - 371
  • [4] Fracture resistance of implant- supported monolithic crowns cemented to zirconia hybrid-abutments: zirconia-based crowns vs. lithium disilicate crowns
    Elshiyab, Shareen H.
    Nawafleh, Noor
    Ochsner, Andreas
    George, Roy
    JOURNAL OF ADVANCED PROSTHODONTICS, 2018, 10 (01): : 65 - 72
  • [5] Effect of Different Veneering Techniques on the Fracture Resistance of Bioceramic Lithium Disilicate Ceramics Crowns
    Barakat, Ali
    Alomari, Mohammed
    JOURNAL OF BIOMATERIALS AND TISSUE ENGINEERING, 2023, 13 (04) : 594 - 600
  • [6] The fracture resistance of pulpotomized primary molars restored with zirconia crowns, lithium disilicate or resin based ceramic endocrowns
    Ali, Amany Abd Elhady Muhammad
    Abo-ELsoud, Asmaa Ali Emam
    Helmy, Yousra Samir
    BMC ORAL HEALTH, 2024, 24 (01):
  • [7] Influence of veneer pore defects on fracture behavior of bilayered lithium disilicate glass-ceramic crowns
    Jian, Yutao
    Dao, Li
    Wang, Xiaodong
    Zhang, Xinping
    Swain, Michael, V
    Zhao, Ke
    DENTAL MATERIALS, 2019, 35 (04) : E83 - E95
  • [8] Fracture strength of lithium disilicate crowns compared to polymer infiltrated ceramic-network and zirconia reinforced lithium silicate crowns
    Sieper, Kim
    Wille, Sebastian
    Kern, Matthias
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2017, 74 : 342 - 348
  • [9] Effect of Lithium Disilicate Reinforced Liner Treatment on Bond and Fracture Strengths of Bilayered Zirconia All-Ceramic Crown
    Jang, Yong-Seok
    Noh, Hyeong-Rok
    Lee, Min-Ho
    Lim, Myung-Jin
    Bae, Tae-Sung
    MATERIALS, 2018, 11 (01):
  • [10] Fracture Load of Monolithic CAD/CAM Lithium Disilicate Ceramic Crowns and Veneered Zirconia Crowns as a Posterior Implant Restoration
    Kim, Jee Hwan
    Lee, Su-Jeong
    Park, Jun Sub
    Ryu, Jae Jun
    IMPLANT DENTISTRY, 2013, 22 (01) : 66 - 70