Structure of rapidly quenched Al-Sc alloys

被引:4
|
作者
Beresina, A
Chuistov, K
Monastyrskaya, T
Schmidt, U
机构
[1] Ukrainian Acad Sci, Inst Met Phys, Kiev, Ukraine
[2] Univ Halle Wittenberg, Halle Saale, Germany
关键词
D O I
10.1080/10667857.2002.11752960
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A study was conducted to examine the abnormal super saturation of Al-Sc alloys with different compositions and at various cooling rates and to understand the structural changes during aging. As a result, the required cooling rate and regimes for aging were determined, thus allowing increased volume fraction of the strengthening Al3Sc phase and providing the foundations for a new class of refractory aluminum alloys.
引用
收藏
页码:26 / 29
页数:4
相关论文
共 50 条
  • [41] STRUCTURE AND PHASE-COMPOSITION OF RAPIDLY QUENCHED AL-FE ALLOYS
    PARKHUTIC, PA
    KALINICHENKO, AS
    KUPRIYANOVA, IY
    CHEBOTKO, IS
    ANTONEVICH, MA
    SAVITSKAYA, YV
    FIZIKA METALLOV I METALLOVEDENIE, 1990, (08): : 162 - 168
  • [42] THE EFFECT OF SOLUTION TREATMENT ON THE AGING PROCESSES OF AL-SC ALLOYS
    DRITS, ME
    DUTKIEWICZ, J
    TOROPOVA, LS
    SALAWA, J
    CRYSTAL RESEARCH AND TECHNOLOGY, 1984, 19 (10) : 1325 - 1330
  • [43] Some comments on the misfit and coherency loss of Al3Sc particles in Al-Sc alloys
    Royset, J
    Ryum, N
    SCRIPTA MATERIALIA, 2005, 52 (12) : 1275 - 1279
  • [44] Coherency loss of Al3SC precipitates during ageing of dilute Al-Sc alloys
    Tsivoulas, D.
    Robson, J. D.
    ALUMINIUM ALLOYS 2006, PTS 1 AND 2: RESEARCH THROUGH INNOVATION AND TECHNOLOGY, 2006, 519-521 : 473 - 478
  • [45] Decomposition of rapidly quenched supersaturated Al-Sc-X (X: Li, Ta, Ti) alloys
    Schmidt, U
    Beresina, AL
    Chuistov, KV
    Monastyrskaja, TA
    Rud, AD
    ADVANCED LIGHT ALLOYS AND COMPOSITES, 1998, 59 : 283 - 289
  • [46] Structure and properties of rapidly quenched zirconium alloys
    Bovda, A. M.
    Dmilrenko, A. E.
    Malykhin, D. G.
    Onischenko, L. V.
    Pelykh, V. N.
    PROBLEMS OF ATOMIC SCIENCE AND TECHNOLOGY, 2007, (04): : 173 - 178
  • [47] The effect of Sc additions on the microstructure and age hardening behaviour of as cast Al-Sc alloys
    Costa, S.
    Puga, H.
    Barbosa, J.
    Pinto, A. M. P.
    MATERIALS & DESIGN, 2012, 42 : 347 - 352
  • [48] Effects of Li additions on precipitation-strengthened Al-Sc and Al-Sc-Yb alloys
    Krug, M. E.
    Dunand, D. C.
    Seidman, D. N.
    ACTA MATERIALIA, 2011, 59 (04) : 1700 - 1715
  • [49] Preparation of Al-Sc application alloys by molten salt electrolysis method
    School of Materials and Metallurgy, Northeastern University, Shenyang 110004, China
    Xiyou Jinshu, 2008, 5 (645-648):
  • [50] FIRST-PRINCIPLES STUDY OF THE PHASE STRACTURES OF Al-Sc ALLOYS
    Su Zhenxing
    Wang Yuchen
    Wang Shaoqing
    ACTA METALLURGICA SINICA, 2010, 46 (05) : 623 - 628