Arc corrosion behavior of Cu-Ti3AlC2 composites in air atmosphere

被引:16
|
作者
Huang, XiaoChen [1 ]
Feng, Yi [1 ,2 ]
Qian, Gang [2 ]
Zhao, Hao [1 ]
Song, ZhaoKun [1 ]
Zhang, JingCheng [2 ]
Zhang, XueBin [1 ]
机构
[1] Hefei Univ Technol, rch Mat Sci & Engn, Hefei 230009, Anhui, Peoples R China
[2] Hefei Univ Technol, Instrumental Anal Ctr, Hefei 230009, Anhui, Peoples R China
基金
中国国家自然科学基金;
关键词
Cu-Ti3AlC2; arc erosion; FE-SEM; Raman spectroscopy; ELECTRON-IRRADIATION; M(N+1)AX(N) PHASES; CATHODE SPOT; MAX PHASES; VACUUM-ARC; EROSION; PROGRESS;
D O I
10.1007/s11431-017-9166-3
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The arc corrosion evolution of Cu-20 vol.% Ti3AlC2 cathodes is presented here. After eroded by 3, 4, 5, 6, 7, 8, 9, 10 kV DC voltage, respectively, the surface morphologies were characterized by field emission scanning electron microscope with craters and protrusions. Compared to small craters and dense protrusions of the morphology by high voltage, the eroded surface was covered with bigger craters and sparse protrusions at low voltage. No crack was discovered on the surface even at 10 kV. By means of energy dispersive spectroscopy and Raman spectroscopy, the decomposition of Cu-20 vol.% Ti3AlC2 cathode to CuO, Al2O3 and TiO2 were proved. Meanwhile, W anode is oxidized to WO2. The peak current increases with the increasing breakdown voltage, which is recorded by a digital memory oscilloscope.
引用
收藏
页码:551 / 557
页数:7
相关论文
共 50 条
  • [41] Oxidation behavior of Ti2AlC/TiAl composites
    Wei, ZJ
    Wang, HW
    Fang, WB
    Zeng, SY
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2003, 13 : 218 - 222
  • [42] Arc erosion behavior of Ag/Ti3AlC2 electrical contact materials
    Ding, J.
    Tian, W. B.
    Zhang, P.
    Zhang, M.
    Zhang, Y. M.
    Sun, Z. M.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 740 : 669 - 676
  • [44] High-temperature oxidation behavior of Ti3AlC2 in air
    徐学文
    李养贤
    朱教群
    梅炳初
    TransactionsofNonferrousMetalsSocietyofChina, 2006, (S2) : 869 - 873
  • [45] High-temperature oxidation behavior of Ti3AlC2 in air
    Xu Xue-wen
    Li Yang-xian
    Zhu Jia-qun
    Mei Bing-chu
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2006, 16 : S869 - S873
  • [46] The decomposition behavior of Ti3AlC2 in the Cu-graphite system
    Wei, H. M.
    Zou, J. P.
    MATERIALS LETTERS, 2023, 351
  • [47] A Critical Review of the Oxidation of Ti2AlC, Ti3AlC2 and Cr2AlC in Air
    Tallman, Darin J.
    Anasori, Babak
    Barsoum, Michel W.
    MATERIALS RESEARCH LETTERS, 2013, 1 (03): : 115 - 125
  • [48] Oxidation and creep behavior of textured Ti2AlC and Ti3AlC2
    Li, Xiaoqiang
    Xie, Xi
    Gonzalez-Julian, Jesus
    Yang, Rui
    Schwaiger, Ruth
    Malzbender, Juergen
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2022, 42 (02) : 364 - 375
  • [49] Corrosion behavior of Ti3AlC2 in NaOH and H2SO4
    Li, Dan
    Liang, Ying
    Liu, Xiaoxia
    Zhou, Yanchun
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2010, 30 (15) : 3227 - 3234
  • [50] High temperature corrosion of Ti3AlC2 in Ar-1%SO2 atmosphere
    Lee, D. B.
    Choi, J. H.
    ECO-MATERIALS PROCESSING AND DESIGN VIII, 2007, 544-545 : 343 - +