Surface Strengthening of Ti-6A1-4V Alloy by Glow Plasma Carbonization Process

被引:0
|
作者
Xing Yazhe [1 ]
Jiang Chaoping [1 ]
Hao Jianmin [1 ]
机构
[1] Changan Univ, Xian 710064, Peoples R China
关键词
Ti-6A1-4V; carbonization; surface modification; wear; TI-6AL-4V ALLOY; TITANIUM-ALLOYS; MICROSTRUCTURE; BEHAVIOR;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A glow plasma carburizing technique was applied to strengthen the surface of the Ti-6A1-4V alloy. The alloy was carburized at 950 degrees C and 30 similar to 35 Pa for 3 h using plasma of Ar gas. Graphite rod was employed as carbon supply to avoid the hydrogen brittleness which is common in traditional gas carbonization. The carburized layer was examined by an optical microscope (OM), field emission scanning electron microscope (FESEM), and X-ray diffractometer (XRD). The wear resistance under ring-block wear testing and the surface hardness were evaluated and compared to those for the untreated material. Results show that a carburized layer (416 mu m thick), mainly composed of TiC and V8C7, is found. These hard carbides contributed to the imrovement of the hardness and wear resistance.
引用
收藏
页码:1101 / 1104
页数:4
相关论文
共 50 条
  • [21] EFFECTS OF PRECOATING SURFACE TREATMENTS ON FATIGUE OF TI-6A1-4V
    EBERHARDT, AW
    KIN, BS
    RIGNEY, D
    KUTNER, GL
    HARTE, CR
    JOURNAL OF APPLIED BIOMATERIALS, 1995, 6 (03) : 171 - 174
  • [22] SURFACE EFFECTS DURING FRETTING FATIGUE OF TI-6A1-4V
    MALKIN, S
    COURTNEY, TH
    MAJORS, DP
    WEAR, 1972, 22 (02) : 235 - &
  • [23] Composition and structure of Ti-6A1-4V alloy plasma-based ion implanted with nitrogen
    Ji, HB
    Xia, LF
    Ma, XX
    Sun, Y
    Sun, MR
    Zhang, ZX
    Zhang, HF
    RARE METALS, 2000, 19 (03) : 197 - 203
  • [24] Surface characteristics of Ti-6A1-4V alloy by EDM with Cu-SiC composite electrode
    Li, L.
    Feng, L.
    Bai, X.
    Li, Z. Y.
    APPLIED SURFACE SCIENCE, 2016, 388 : 546 - 550
  • [25] THE EFFECT OF ION PLATING ON THE FRICTION AND WEAR OF TI-6A1-4V ALLOY
    EYLON, D
    BETTS, RK
    FUJISHIRO, S
    THIN SOLID FILMS, 1980, 73 (02) : 323 - 329
  • [26] Hydrogen-induced hot workability in Ti-6A1-4V alloy
    宗影影
    单德彬
    吕炎
    郭斌
    TransactionsofNonferrousMetalsSocietyofChina, 2006, (S3) : 2072 - 2076
  • [27] OXIDE ADHERENCE AND PORCELAIN BONDING TO TITANIUM AND TI-6A1-4V ALLOY
    ADACHI, M
    MACKERT, JR
    PARRY, EE
    FAIRHURST, CW
    JOURNAL OF DENTAL RESEARCH, 1990, 69 (06) : 1230 - 1235
  • [28] IMPROVEMENT IN FATIGUE LIFETIME OF TI-6A1-4V ALLOY BY BORON IMPLANTATION
    ZHANG, DW
    ZHANG, XP
    YU, WC
    WANG, ZG
    SURFACE & COATINGS TECHNOLOGY, 1993, 58 (02): : 119 - 123
  • [29] INITIATION OF STRESS-CORROSION CRACKING IN TI-6A1-4V ALLOY
    LINK, F
    MUNZ, D
    CORROSION SCIENCE, 1973, 13 (10) : 809 - &
  • [30] Experimental study on surface integrity of cryogenically machined Ti-6A1-4V alloy for biomedical devices
    Hard, M.
    Klocke, F.
    Doebbeler, B.
    Binder, M.
    Jawahir, I. S.
    4TH CIRP CONFERENCE ON SURFACE INTEGRITY (CSI 2018), 2018, 71 : 181 - 186