INFLUENCE OF LOCALIZED PLASTICITY ON IASCC SENSITIVITY OF AUSTENITIC STAINLESS STEELS UNDER PWR PRIMARY WATER.

被引:0
|
作者
Cisse, Sarata [1 ]
Tanguy, Benoit [1 ]
Laffont, Lydia [2 ]
Lafont, Marie-Christine [2 ]
Guerre, Catherine [3 ]
Andrieu, Eric [2 ]
机构
[1] CEA Saclay, Nucl Mat Dept, F-91191 Gif Sur Yvette, France
[2] Inst CARNOT, CIRMAT ENSIACET, F-31030 Toulouse, France
[3] CEA, DEN DPC, SCCME, Lab Etud Corros, F-91191 Gif Sur Yvette, France
关键词
irradiation assisted stress corrosion cracking (IASCC); plastic deformation localization; precipitation strengthened stainless steel A286; DEFORMATION; 304-STAINLESS-STEEL; MICROSTRUCTURE; INITIATION; MECHANISM;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The sensibility of precipitation-strengthened A286 austenitic stainless steel to Stress Corrosion Cracking (SCC) is studied by means of Slow Strain Rate Tests (SSRT). First, alloy cold working by Low Cycle Fatigue (LCF) is investigated. Fatigue tests under plastic strain control are performed at different strain levels (Delta epsilon(p)/2=0.2%, 0.5% and 0.8%) in order to establish correlation between stress softening and deformation microstructure resulting from LCF tests. Deformed microstructures have been identified through TEM investigations. Three states of cyclic behaviour for precipitation-strengthened A286 have been identified: hardening, cyclic softening and finally saturation of softening. It is shown that the A286 alloy cyclic softening is due to microstructural features such as defects - free deformation bands resulting from dislocations motion along family plans < 111>, that swept defects or gamma' precipitates and lead to deformation localization. In order to quantify effects of plastic localized deformation on intergranular stress corrosion cracking (IGSCC) of the A286 alloy in PWR primary water, slow strain rate tests are conducted. For each cycling conditions, two specimens at a similar stress level are tested: the first containing free precipitate deformation bands, the other not significant of a localized deformation state. SSRT tests are still in progress.
引用
收藏
页码:1417 / 1427
页数:11
相关论文
共 50 条
  • [41] Influence of silicon, carbon and phosphorus on intergranular corrosion of high purity austenitic stainless steels under transpassive conditions
    Stolarz, J
    JOURNAL DE PHYSIQUE IV, 1995, 5 (C7): : 423 - 428
  • [42] Influence of load ratio, rise time and waveform on the corrosion fatigue crack growth of austenitic stainless steel in a PWR primary coolant environment
    Platts, Norman
    Tice, David
    Rigby, Keith
    Stairmand, John
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE 2007, VOL 1: CODES AND STANDARDS, 2007, 1 : 287 - 302
  • [43] Hydrogen absorption associated with the corrosion mechanism of 316L stainless steels in primary medium of Pressurized Water Reactor (PWR)
    Dumerval, Marie
    Perrin, Stephane
    Marchetti, Loic
    Tabarant, Michel
    Jomard, Francois
    Wouters, Yves
    CORROSION SCIENCE, 2014, 85 : 251 - 257
  • [44] Effect of surface preparation on the corrosion of austenitic stainless steel 304L in high temperature steam and simulated PWR primary water
    Cisse, Sarata
    Laffont, Lydia
    Tanguy, Benoit
    Lafont, Marie-Christine
    Andrieu, Eric
    CORROSION SCIENCE, 2012, 56 : 209 - 216
  • [45] Stress Corrosion Cracking in Austenitic Stainless Steels in Reactor Primary Water-High Purity Oxidizing and in Supercritical Conditions
    Das, Annesha
    Roychowdhury, Supratik
    Kain, Vivekanand
    MATERIALS PERFORMANCE AND CHARACTERIZATION, 2022, 11 (02) : 139 - 156
  • [46] INFLUENCE OF INSENSITIVE STRAIN REGION FOR STRAIN RATE ON FATIGUE LIFE OF STAINLESS STEEL IN PWR PRIMARY WATER ENVIRONMENT
    Kamaya, Masayuki
    PROCEEDINGS OF ASME 2023 PRESSURE VESSELS & PIPING CONFERENCE, PVP2023, VOL 1, 2023,
  • [47] Corrosion fatigue initiation and short crack growth behaviour of austenitic stainless steels under light water reactor conditions
    Seifert, H. P.
    Ritter, S.
    Leber, H. J.
    CORROSION SCIENCE, 2012, 59 : 20 - 34
  • [48] Proton irradiation assisted localized corrosion and stress corrosion cracking in 304 nuclear grade stainless steel in simulated primary PWR water
    Ping Deng
    Qunjia Peng
    En-Hou Han
    Wei Ke
    Chen Sun
    JournalofMaterialsScience&Technology, 2021, 65 (06) : 61 - 71
  • [49] Proton irradiation assisted localized corrosion and stress corrosion cracking in 304 nuclear grade stainless steel in simulated primary PWR water
    Deng, Ping
    Peng, Qunjia
    Han, En-Hou
    Ke, Wei
    Sun, Chen
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 65 : 61 - 71
  • [50] Behavior of different austenitic stainless steels, conventional, reduced activation (RA) and ODS chromium-rich ferritic-martensitic steels under neutron irradiation at 325°C in PWR environment
    Brachet, JC
    Averty, X
    Lamagnère, P
    Alamo, A
    Rozenblum, F
    Raquet, O
    Bertin, JL
    EFFECTS OF RADIATION ON MATERIALS: 20TH INTERNATIONAL SYMPOSIUM, 2001, 1045 : 500 - 520