Thermal expansion anisotropy in a Ti-6Al-4V/SiC composite

被引:18
|
作者
Choo, H
Rangaswamy, P
Bourke, MAM
Larsen, JM
机构
[1] Los Alamos Natl Lab, LANSCE12, Los Alamos, NM 87545 USA
[2] USAF, Res Lab, Wright Patterson AFB, OH 45433 USA
关键词
titanium; composite; neutron scattering; thermal expansion; thermal load partitioning; Schapery model;
D O I
10.1016/S0921-5093(01)01463-0
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
We studied the thermal expansion behavior of a Ti-6Al-4V/35 vol.% continuous SiC fiber composite using in situ high temperature neutron diffraction (ND). The lattice expansion of constituent phases within the composite was monitored from axial (parallel to the unidirectionally aligned fibers) and transverse (perpendicular to the fibers) directions during heating from room temperature (RT) to 1170 K. The phase-specific thermal expansion of the Ti-6Al-4V matrix and SiC fibers in the composite is discussed in the context of thermal load partitioning between the matrix and fibers. In the axial direction, the matrix and the fiber share the thermal load and co-expand up to about 800-900 K, above which the thermal load transfer becomes ineffective. In the transverse direction, the matrix and fibers expand independently over the whole temperature range, Using the Schapery model (J. Comp. Mater. 2 (1968) 380) and the rule-of-mixtures (ROM), the macroscopic thermal expansion of the composite is predicted and compared with the experimental results. (C) 2002 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:236 / 241
页数:6
相关论文
共 50 条
  • [31] Effect of anisotropy on mechanical properties of Ti-6Al-4V in superplastic region
    Wahed, M. A.
    Gupta, A. K.
    Singh, S. K.
    Kotkunde, N.
    INTERNATIONAL CONFERENCE ON RECENT ADVANCES IN MATERIALS & MANUFACTURING TECHNOLOGIES, 2018, 346
  • [32] Transformation superplasticity of Ti-6Al-4V and Ti-6Al-4V/TiC composites at high stresses
    Schuh, C
    Dunand, DC
    SUPERPLASTICITY IN ADVANCED MATERIALS, ICSAM-2000, 2001, 357-3 : 177 - 182
  • [33] ELEVATED-TEMPERATURE PLASTIC ANISOTROPY OF TI-6AL-4V PLATE
    RENNHACK, EH
    CROOKS, DD
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1979, 10 (04): : 457 - 462
  • [34] Anisotropy in Chip Formation in Orthogonal Cutting of Rolled Ti-6Al-4V
    Tamura, Shoichi
    Matsumura, Takashi
    JOURNAL OF MANUFACTURING SCIENCE AND ENGINEERING-TRANSACTIONS OF THE ASME, 2025, 147 (01):
  • [35] Mechanical properties anisotropy of Ti-6Al-4V alloy fabricated by ,β forging
    Weng, Han-bo
    Huang, Sen-sen
    Yang, Jie
    Qi, Min
    Ma, Ying-jie
    Wang, Yu-xiang
    Xu, Dao-kui
    Qiu, Jian-ke
    Lei, Jia-feng
    Gong, Bin
    Yang, Rui
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2023, 33 (11) : 3348 - 3363
  • [36] Efficient modelling of the elastoplastic anisotropy of additively manufactured Ti-6Al-4V
    Agius, Dylan
    Wallbrink, Chris
    Kourousis, Kyriakos, I
    ADDITIVE MANUFACTURING, 2021, 38
  • [37] An acoustic emission study of anisotropy in additively manufactured Ti-6Al-4V
    Seyed A. Niknam
    Dongsheng Li
    Gopal Das
    The International Journal of Advanced Manufacturing Technology, 2019, 100 : 1731 - 1740
  • [38] An acoustic emission study of anisotropy in additively manufactured Ti-6Al-4V
    Niknam, Seyed A.
    Li, Dongsheng
    Das, Gopal
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2019, 100 (5-8): : 1731 - 1740
  • [39] ANISOTROPY CONTROL THROUGH THE USE OF HYDROGEN IN TI-6AL-4V ALLOY
    BIRLA, NC
    BASU, RK
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 1984, 37 (05): : 631 - 635
  • [40] Hydroxyapatite and bioactive glass composite coating on Ti-6Al-4V
    Du, Ruilin
    Zeng, Shaoxian
    Hu, Yuhuai
    Xie, Xinghui
    BIOCERAMICS, VOL 19, PTS 1 AND 2, 2007, 330-332 : 589 - +