Study of Micro-arc Oxidation Process in Magnesium Surface

被引:0
|
作者
Chen, Ze-min [1 ]
Lu, Pin [2 ]
Dong, Qiu-hong [1 ]
机构
[1] Langfang Normal Coll, Sch Chem & Mat Sci, Langfang 065000, Peoples R China
[2] Hebei Univ, Coll Chem & Environm Sci, Baoding 071002, Peoples R China
关键词
Magnesium; Micro-arc oxidation; Potentiodynamic polarization;
D O I
10.4028/www.scientific.net/AMM.190-191.595
中图分类号
TP [自动化技术、计算机技术];
学科分类号
0812 ;
摘要
This study selected sodium silicate, sodium fluoride, glycerol hydroxyl acid, potassium hydroxide and phosphine oxide (LAP) as the stabilizer electrolyte, and then on micro-arc oxidation of magnesium with constant current density. The microstructure, corrosion resistance, chemical composition, structure and characterization of micro-arc oxidation film were determined by SEM and anodic oxidation methods. Experimental results indicated that the test pieces of magnesium would formed an silver-gray uniform densification oxide film on the surface by micro-arc oxidation treatment, and the corrosion resistance of magnesium film-formed had increased by potentiodynamic polarization curve testing.
引用
收藏
页码:595 / +
页数:2
相关论文
共 50 条
  • [21] Research on formation and growth process of ceramic coatings on magnesium alloy by micro-arc oxidation
    Ge, Yan-Feng
    Jiang, Bai-Ling
    Wang, Cong-Jie
    Long, Yi
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2014, 35 (12): : 190 - 194
  • [22] Magnesium with micro-arc oxidation coating and polymeric membrane: an in vitro study on microenvironment
    Honglong Li
    Haobo Pan
    Chengyun Ning
    Guoxin Tan
    Jingwen Liao
    Guoxin Ni
    Journal of Materials Science: Materials in Medicine, 2015, 26
  • [23] Magnesium with micro-arc oxidation coating and polymeric membrane: an in vitro study on microenvironment
    Li, Honglong
    Pan, Haobo
    Ning, Chengyun
    Tan, Guoxin
    Liao, Jingwen
    Ni, Guoxin
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN MEDICINE, 2015, 26 (03)
  • [24] Degradation of Micro-arc Oxidation Coatings on the Surface of Magnesium Alloy under NaCl Droplet
    Wan, Yanhua
    Liu, Yuanyuan
    MATERIALS ENGINEERING FOR ADVANCED TECHNOLOGIES, PTS 1 AND 2, 2011, 480-481 : 437 - 442
  • [25] A novel superhydrophobic micro-arc oxidation coating on magnesium alloy
    Zhang, Bingzi
    NATIONAL SCIENCE REVIEW, 2017, 4 (06) : 793 - 793
  • [26] Research Progress on Micro-arc Oxidation of Medical Magnesium Alloy
    Feng Y.-R.
    Zhou L.
    Jia H.-Y.
    Zhang X.
    Zhao L.-B.
    Fang D.-Q.
    Surface Technology, 2023, 52 (07): : 11 - 24
  • [27] Phase composition of micro-arc oxidation coating on magnesium alloys
    Li, Song
    Liu, Yao-Hui
    Zhang, Ji-Cheng
    Song, Li-Min
    Hangkong Cailiao Xuebao/Journal of Aeronautical Materials, 2008, 28 (06): : 10 - 15
  • [28] Discharge mechanism of ultrasound micro-arc oxidation on magnesium alloy
    李慕勤
    曲立杰
    马春力
    马臣
    王晶彦
    李海涛
    China Welding, 2015, 24 (02) : 30 - 34
  • [29] Research status of magnesium alloys by micro-arc oxidation: a review
    Dou, Jinhe
    Chen, Yang
    Yu, Huijun
    Chen, Chuanzhong
    SURFACE ENGINEERING, 2017, 33 (10) : 731 - 738
  • [30] Discharge mechanism of ultrasound micro-arc oxidation on magnesium alloy
    State Key Laboratory of Advanced Welding and Joining, Harbin Institute of Technology, Harbin, China
    不详
    China Weld Eng Ed, 2 (30-34):