Catalytic degradation of high-density polyethylene in a reactive extruder

被引:8
|
作者
Wallis, Michael D. [1 ]
Sarathy, Sandeep [1 ]
Bhatia, Suresh K. [1 ]
Massarotto, P. [1 ]
Kosior, Edward [2 ]
Mercier, Alain [3 ]
机构
[1] Univ Queensland, Div Chem Engn, Brisbane, QLD 4072, Australia
[2] Nextek Proprietary Ltd, Bronte, NSW 2024, Australia
[3] Granit Syst SA, CH-1003 Lausanne, Switzerland
关键词
D O I
10.1021/ie0714450
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The catalytic degradation of high-density polyethylene was conducted in a reactive extruder at reaction temperatures of 425, 450, and 475 degrees C using silica-alumina as the cracking catalyst. A continuous kinetic model was proposed and compared to the carbon number distribution of the reaction products. The model prediction of the product selectivity described the experimental data well for a reaction temperature of 425 degrees C; however, it was. too simplistic to predict the decrease in C-4 and increase in C-3 occurring at higher reaction temperatures. The liquid product obtained from the reactive extruder was comparable to gasoline; however, it did show a significantly higher C-5 fraction.
引用
收藏
页码:5175 / 5181
页数:7
相关论文
共 50 条
  • [1] Thermal degradation of high density polyethylene in a reactive extruder
    Wallis, Michael D.
    Bhatia, Suresh K.
    POLYMER DEGRADATION AND STABILITY, 2007, 92 (09) : 1721 - 1729
  • [2] A STUDY OF DEGRADATION OF HIGH-DENSITY POLYETHYLENE IN A COROTATING INTERMESHING TWIN SCREW EXTRUDER
    DONTULA, N
    CAMPBELL, GA
    CONNELLY, R
    POLYMER ENGINEERING AND SCIENCE, 1993, 33 (05): : 271 - 278
  • [3] Catalytic degradation of high-density polyethylene over different zeolitic structures
    Manos, G
    Garforth, A
    Dwyer, J
    INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2000, 39 (05) : 1198 - 1202
  • [4] Thermal and thermo-catalytic degradation of high-density polyethylene waste
    Miskolczi, N
    Bartha, L
    Deák, G
    Jóver, B
    Kalló, D
    JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 2004, 72 (02) : 235 - 242
  • [5] THE GRAFTING OF MALEIC-ANHYDRIDE ON HIGH-DENSITY POLYETHYLENE IN AN EXTRUDER
    GANZEVELD, KJ
    JANSSEN, LPBM
    POLYMER ENGINEERING AND SCIENCE, 1992, 32 (07): : 467 - 474
  • [6] Investigation of catalytic degradation of high-density polyethylene by hydrocarbon group type analysis
    Seo, YH
    Lee, KH
    Shin, DH
    JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 2003, 70 (02) : 383 - 398
  • [7] Development of HZSM-12 zeolite for catalytic degradation of high-density polyethylene
    Silva, Antonio O. S.
    Souza, Marcelo J. B.
    Pedrosa, Anne M. G.
    Coriolano, Ana C. F.
    Fernandes, Valter J., Jr.
    Araujo, Antonio S.
    MICROPOROUS AND MESOPOROUS MATERIALS, 2017, 244 : 1 - 6
  • [8] THERMAL-DEGRADATION OF HIGH-DENSITY POLYETHYLENE
    MURATA, K
    MAKINO, T
    NIPPON KAGAKU KAISHI, 1973, (12) : 2414 - 2420
  • [9] Catalytic Degradation of High-Density Polyethylene over a Clay Catalyst Compared with Other Catalysts
    Liu, Mi
    Zhuo, Jian K.
    Xiong, Si J.
    Yao, Qiang
    ENERGY & FUELS, 2014, 28 (09) : 6038 - 6045
  • [10] SYNTHESIS OF BRANCHED POLYETHYLENE BY CATALYTIC DEGRADATION ISOMERIZATION OF HIGH-DENSITY POLYETHYLENE IN THE PRESENCE OF SILICA-ALUMINA CATALYST
    NANBU, H
    ISHIHARA, Y
    HONMA, H
    TAKESUE, T
    IKEMURA, T
    NIPPON KAGAKU KAISHI, 1987, (04) : 765 - 770