Microstructure and properties of the Si3N4/Si3N4 brazing joint

被引:0
|
作者
Zhang, J [1 ]
Naka, N [1 ]
Zhou, Y [1 ]
Lei, TQ [1 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150001, Peoples R China
关键词
Si3N4; ceramic; braze welding; interface; microstructure;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Si3N4 ceramic was brazed using a filler alloy Of (CUZn)(85)Til(5) alloy, and a Si3N4/Si3N4 joint with a high bonding strength was obtain under a suitable brazing condition. The brazing joint was composed of Cu2TiZn and Cu solution containing Titanium Silicide and Titanium Nitride. With increasing brazing temperature from 1123K to 1323K, the thickness of the reaction layer increased and the amount and size of the reactant increased. The addition of the Zn made the melting point of the filler alloy and the brazing temperature decreased, which improved the flowability and wettablility of the filler alloy. The evaporation of Zn was enhanced with increasing welding temperature. The shear strength of the Si3N4/Si3N4 joint increased with increasing welding temperature. The average shear strength of the joint reached 265 MPa when the welding temperature is 1223K.
引用
收藏
页码:222 / 225
页数:4
相关论文
共 50 条
  • [31] Superplastic forming of Si3N4 and Si3N4/SiC nanocomposites
    Rouxel, T
    Besson, JL
    Mayne, M
    Bahloul, D
    Goursat, P
    SUPERPLASTICITY IN ADVANCED MATERIALS - ICSAM-97, 1997, 243-2 : 233 - 237
  • [32] Effect of brazing temperature on microstructure and mechanical properties of Si3N4/Si3N4 joints brazed with Ag–Cu–Ti + Mo composite filler
    Y. M. He
    J. Zhang
    X. Wang
    Y. Sun
    Journal of Materials Science, 2011, 46 : 2796 - 2804
  • [33] Joining of Si3N4 to Si3N4 using rapidly-solidified CuNiTiB brazing filler foils
    Jilin Univ of Technology, Changchun, China
    J Mater Process Technol, 1-3 (137-142):
  • [34] Joining of Si3N4 to Si3N4 using rapidly-solidified CuNiTiB brazing filler foils
    Xiong, HP
    Wan, CG
    Zhou, ZF
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 1998, 75 (1-3) : 137 - 142
  • [35] Joining of Si3N4/Si3N4 with CuNiTiB paste brazing filler metals and interfacial reactions of the joints
    Wang, CG
    Xiong, HP
    Zhou, ZF
    JOURNAL OF MATERIALS SCIENCE, 1999, 34 (12) : 3013 - 3019
  • [36] Joining of Si3N4/Si3N4 with CuNiTiB paste brazing filler metals and interfacial reactions of the joints
    Chuangeng Wan
    Huaping Xiong
    Zhenfeng Zhou
    Journal of Materials Science, 1999, 34 : 3013 - 3019
  • [37] Titanium metallization of Si3N4 by molten salt reaction and its application in Si3N4/Si3N4 joining
    Chen, J
    Pan, W
    Zheng, SY
    Huang, Y
    PROCEEDINGS OF THE FIRST CHINA INTERNATIONAL CONFERENCE ON HIGH-PERFORMANCE CERAMICS, 2001, : 578 - 580
  • [38] INTERFACIAL REACTIONS IN THE AL/SI3N4/SI AND AU/SI3N4/SI SYSTEMS
    EDELMAN, F
    GUTMANAS, E
    BRENER, R
    INTERFACES BETWEEN POLYMERS, METALS, AND CERAMICS, 1989, 153 : 77 - 82
  • [39] Active metal brazing of Si3N4 to metals
    Heim, M
    Tessarotto, LAB
    Greenhut, VA
    22ND ANNUAL CONFERENCE ON COMPOSITES, ADVANCED CERAMICS, MATERIALS, AND STRUCTURES: B, 1998, 19 (04): : 347 - 354
  • [40] PROPERTIES OF SINTERED SI3N4
    TERWILLI.GR
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1974, 57 (01) : 48 - 49