An investigation of Mode I and Mode II fracture toughness enhancement using aligned carbon nanotubes forests at the crack interface

被引:72
|
作者
Falzon, Brian G. [1 ]
Hawkins, Stephen C. [2 ]
Huynh, Chi P. [2 ]
Radjef, Racim [3 ]
Brown, Callum [3 ]
机构
[1] Queens Univ Belfast, Sch Mech & Aerosp Engn, Belfast BT9 5AH, Antrim, North Ireland
[2] CSIRO Mat Sci & Engn, Clayton, Vic 3168, Australia
[3] Monash Univ, Dept Mech & Aerosp Engn, Clayton, Vic 3800, Australia
关键词
Carbon nanotubes; Composite materials; Structural failure; Mode I testing; Mode II testing; Fracture toughness; STIFFENER RUNOUT SPECIMENS; MECHANICAL-PROPERTIES; UNIAXIAL COMPRESSION; COMPOSITE PANEL; IMPACT DAMAGE; EPOXY MATRIX; PART I; BEHAVIOR; NANOCOMPOSITES; PERFORMANCE;
D O I
10.1016/j.compstruct.2013.05.051
中图分类号
O3 [力学];
学科分类号
08 ; 0801 ;
摘要
A novel approach for introducing aligned multi-walled carbon nanotubes (MWCNTs) in a carbon-fibre composite pre-impregnated (prepreg) laminate, to improve the through-thickness fracture toughness, is presented. Carbon nanotube (CNT) 'forests' were grown on a silicon substrate with a thermal oxide layer, using a chemical vapour deposition (CVD) process. The forests were then transferred to a pre-cured laminate interface, using a combination of pressure and heat, while maintaining through-thickness CNT alignment. Standard Mode I and four-point bend end-notched flexure Mode II tests were undertaken on a set of specimens and compared with pristine specimens. Mode I fracture toughness for T700/M21 laminates was improved by an average of 31% while for T700/SE84LV specimens, an improvement of 61% was observed. Only T700/M21 specimens were tested in Mode II which yielded an average fracture toughness improvement of 161%. Scanning Electron Microscopy (SEM) showed good wetting of the CNT forest as well as evidence of penetration of the forest into the adjacent plies. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:65 / 73
页数:9
相关论文
共 50 条
  • [31] Determination of mode I and mode II fracture toughness of walnut and cherry in TR and RT crack propagation system by the Arcan test
    Murata, Koji
    Bachtiar, Erik Valentine
    Niemz, Peter
    HOLZFORSCHUNG, 2017, 71 (12) : 985 - 990
  • [32] Mixed Mode I/II fracture toughness of bonded joints
    Pirondi, A
    Nicoletto, G
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2002, 22 (02) : 109 - 117
  • [33] Fracture toughness for mixed mode I/II of epoxy resin
    Araki, W
    Nemoto, K
    Adachi, T
    Yamaji, A
    ACTA MATERIALIA, 2005, 53 (03) : 869 - 875
  • [34] On the combined mode I mode II fracture toughness of a fiber reinforced polymer composite
    Manoharan, M
    Xiao, H
    INTERNATIONAL JOURNAL OF FRACTURE, 1997, 88 (01) : L3 - L7
  • [35] Fracture toughness of aged dental composites in combined mode I and mode II loading
    Scherrer, SS
    Botsis, J
    Studer, M
    Pini, M
    Wiskott, HWA
    Belser, UC
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 2000, 53 (04): : 362 - 370
  • [36] Fracture toughness in SPCC/CFRP hybrid laminates: Mode I and mode II perspectives
    Nugraha, Ariyana Dwiputra
    Hakim, Muhammad Luthfi
    Pramana, Ari
    Triawan, Farid
    Handayani, Murni
    Rahmayanti, Yosephin Dewiani
    Muflikhun, Muhammad Akhsin
    RESULTS IN ENGINEERING, 2024, 24
  • [37] Interlaminar fracture toughness of CFRP in mode I and mode II determined by Raman spectroscopy
    Miyagawa, H
    Sato, C
    Ikegami, K
    COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2001, 32 (3-4) : 477 - 486
  • [38] Mode II interlaminar fracture toughness of carbon nanotubes/epoxy film-interleaved carbon fiber composites
    Shin, Yong Chul
    Lee, Woo Il
    Kim, Han Sang
    COMPOSITE STRUCTURES, 2020, 236 (236)
  • [39] Application of the effective crack method to mode I and mode II interlaminar fracture of carbon/epoxy unidirectional laminates
    de Morais, A. B.
    Pereira, A. B.
    COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2007, 38 (03) : 785 - 794
  • [40] Investigation of mixed mode I/II interlaminar fracture toughness of laminated composites by using a CTS type specimen
    Rikards, R
    Buchholz, FG
    Wang, H
    Bledzki, AK
    Korjakin, A
    Richard, HA
    ENGINEERING FRACTURE MECHANICS, 1998, 61 (3-4) : 325 - 342