Advanced inspection technique for deep-submicron and high-aspect-ratio contact holes

被引:8
|
作者
Matsui, M
Nozoe, M
Arauchi, K
Takafuji, A
Nishiyama, H
Goto, Y
机构
[1] Hitachi Ltd, Cent Res Lab, Tokyo 1858601, Japan
[2] Hitachi ULSI Syst, Tokyo 1988512, Japan
关键词
electron beams; contact holes; incomplete contact failure; high aspect ratio; inspection; charge-up voltage;
D O I
10.1117/1.1585062
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
We developed a technique using electron beams for inspecting contact holes immediately after dry etching and detecting incomplete contact failures. Wafers with deep-submicron contact holes that had high aspect ratios of 10 could be detected during practical inspection time by controlling the charging effect on the wafer surfaces. Measurements of the energy distribution in the secondary electrons exhausted from the bottom of the holes indicated that they were accelerated by the charge-up voltage on the wafer surfaces. Our analysis showed that high-density electron beams must be used to charge the surfaces when the aspect ratio is high. The minimum thickness of the residual SiO2 that could be detected at the bottom of the contact holes was 2 nm using an aspect ratio of 8. Applying this mechanism to optimize the dry etching process in semiconductor manufacturing showed that we could achieve reliable process control. (C) 2003 Society of Photo-Optical Instrumentation Engineers.
引用
收藏
页码:227 / 232
页数:6
相关论文
共 50 条
  • [41] High-aspect-ratio bulk micromachining of titanium
    Aimi, MF
    Rao, MP
    Macdonald, NC
    Zuruzi, AS
    Bothman, DP
    NATURE MATERIALS, 2004, 3 (02) : 103 - 105
  • [42] SMT REQUIREMENTS FOR HIGH-ASPECT-RATIO PTHS
    LANGAN, JP
    PLATING AND SURFACE FINISHING, 1992, 79 (01): : 42 - 43
  • [43] High-aspect-ratio bulk micromachining of titanium
    Marco F. Aimi
    Masa P. Rao
    Noel C. MacDonald
    Abu Samah Zuruzi
    David P. Bothman
    Nature Materials, 2004, 3 : 103 - 105
  • [44] LIMITATIONS OF ELECTROPLATING ON HIGH-ASPECT-RATIO PTHS
    LANGAN, JP
    PLATING AND SURFACE FINISHING, 1992, 79 (02): : 40 - 40
  • [45] High-aspect-ratio microstructures for magnetoelectronic applications
    Wang, T
    McCandless, AB
    Ford, S
    Kelly, KW
    Lienau, R
    Hensley, D
    Desta, Y
    Ling, ZG
    MICROMACHINING AND MICROFABRICATION PROCESS TECHNOLOGY VIII, 2003, 4979 : 464 - 471
  • [46] High-aspect-ratio nanoimprint process chains
    Cadarso, Victor J.
    Chidambaram, Nachiappan
    Jacot-Descombes, Loic
    Schift, Helmut
    MICROSYSTEMS & NANOENGINEERING, 2017, 3
  • [47] Controlled Collapse of High-Aspect-Ratio Nanostructures
    Duan, Huigao
    Yang, Joel K. W.
    Berggren, Karl K.
    SMALL, 2011, 7 (18) : 2661 - 2668
  • [48] The production of high-aspect-ratio microstructures (HARMS)
    Keatch, R
    Lawrenson, B
    Finlay, M
    Lewis, B
    Horsfield, C
    FUSION TECHNOLOGY, 2000, 38 (01): : 139 - 142
  • [49] High-aspect-ratio photolithography for MEMS applications
    Miyajima, H
    Mehregany, M
    JOURNAL OF MICROELECTROMECHANICAL SYSTEMS, 1995, 4 (04) : 220 - 229
  • [50] High-aspect-ratio silicon dioxide pillars
    Trifonov, T
    Rodríguez, A
    Servera, F
    Marsal, LF
    Pallarès, J
    Alcubilla, R
    PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 2005, 202 (08): : 1634 - 1638