The effect of thermocycling on the fracture toughness and hardness of core buildup materials

被引:20
|
作者
Tirado, JIM
Nagy, WW [1 ]
Dhuru, VB
Ziebert, AJ
机构
[1] Marquette Univ, Sch Dent, Div Dent Biomat, Milwaukee, WI 53233 USA
[2] Marquette Univ, Sch Dent, Div Prosthodont, Milwaukee, WI 53233 USA
来源
JOURNAL OF PROSTHETIC DENTISTRY | 2001年 / 86卷 / 05期
关键词
D O I
10.1067/mpr.2001.120110
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Statement of problem. Thermocycling has been shown to cause surface degradation of many dental materials, but its effect Oil the fracture toughness mid hardness of direct core buildup materials is unknown. Purpose. This study was designed to determine the effect of thermocycling on the fracture toughness and hardness of 5 core buildup materials. Material and methods. Fifteen specimens were prepared from each of the following materials: Fluorocore, VariGlass VLC, Valiant PhD, Vitremer, and Chelon-Silver. American Standard for Testing Materials guidelines for single-edge notch, bar-shaped specimens were used. Ten specimens of each material were thermocycled for 2000 cycles, the other 5 specimens were not thermocycled. All specimens were Subjected to 3-point bending in a universal testing machine. The toad it fracture was recorded, and the fracture toughness (K-IC) was calculated. Barcol hardness values were also determined. Data were analyzed with 1-way analysis of variance and compared with the Tukey multiple range test (P < .05). Pearson's correlation coefficient,vas also calculated to measure the association between fracture toughness mid hardness. Results. Fluorocore had the highest thermocycled mean K-IC and Valiant PhD the highest non-thermocycled K-IC. Chelon-Silver demonstrated the lowest mean K-IC both before and after thermocycling. One-way analysis of variance demonstrated significant differences between conditions, and the Tukey test showed significant differences (P < .05) between materials for both conditions. Most specimens also showed significant hardness differences between conditions. Pearson's correlation coefficient indicated only a mild-to-moderate correlation between hardness and fracture toughness. Conclusion. Within the limitations of this study, the thermocycling process negatively affected the fracture toughness and hardness of the core buildup materials tested.
引用
收藏
页码:474 / 480
页数:7
相关论文
共 50 条
  • [21] A model of hardness and fracture toughness of solids
    Mazhnik, Efim
    Oganov, Artem R.
    JOURNAL OF APPLIED PHYSICS, 2019, 126 (12)
  • [22] Examining the changes of hardness and fracture toughness of different materials joined by laser beam
    Karaaslan, A
    Yumurtaci, S
    ISMTII'2001: PROCEEDINGS OF THE FIFTH INTERNATIONAL SYMPOSIUM ON MEASUREMENT TECHNOLOGY AND INTELLIGENT INSTRUMENTS, 2001, : 473 - 477
  • [23] HARDNESS AND FRACTURE-TOUGHNESS OF SEMICONDUCTING MATERIALS STUDIED BY INDENTATION AND EROSION TECHNIQUES
    ERICSON, F
    JOHANSSON, S
    SCHWEITZ, JA
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1988, 105 : 131 - 141
  • [24] Comparative Evaluation of Fracture Resistance of Composite Core Buildup Materials: An In Vitro Study
    Pande, Deepmala
    Benjamin, Niharika
    Rani, Vishakha
    Hina, Malik
    Haldar, Shreya
    Nirmal, Harni
    Gole, Shivani
    Ali, Md Sadique
    CUREUS JOURNAL OF MEDICAL SCIENCE, 2024, 16 (06)
  • [27] The effect of coarse aggregate hardness on the fracture toughness and compressive strength of concrete
    Siregar, Atur P. N.
    Pasaribu, Emma L.
    Suarnita, I. Wayan
    INTERNATIONAL CONFERENCE ON SUSTAINABLE CIVIL ENGINEERING STRUCTURES AND CONSTRUCTION MATERIALS (SCESCM 2018), 2019, 258
  • [28] INDENTATION FRACTURE-TOUGHNESS OF 3 NEW CERAMIC CORE MATERIALS
    CHU, TM
    WAGNER, WC
    RAZZOOG, ME
    JOURNAL OF DENTAL RESEARCH, 1995, 74 : 471 - 471
  • [29] Fracture toughness of various core build-up materials.
    Mardirossian, G
    Bonilla, E
    Caputo, AA
    JOURNAL OF DENTAL RESEARCH, 1998, 77 : 674 - 674
  • [30] The fracture toughness of four core build-up materials.
    Ziebert, AJ
    Dhuru, VB
    Schultz, WT
    Thiel, JA
    JOURNAL OF DENTAL RESEARCH, 1997, 76 : 498 - 498