Effect of laser power on orientation and microstructure of TiO2 films prepared by laser chemical vapor deposition method

被引:14
|
作者
Guo, Dongyun [1 ,2 ]
Ito, Akihiko [2 ]
Goto, Takashi [2 ]
Tu, Rong [2 ]
Wang, Chuanbin [1 ]
Shen, Qiang [1 ]
Zhang, Lianmeng [1 ]
机构
[1] Wuhan Univ Technol, Sch Mat Sci & Engn, State Key Lab Adv Technol Mat Synth & Proc, Wuhan 430070, Hubei, Peoples R China
[2] Tohoku Univ, Inst Mat Res, Sendai, Miyagi 9808577, Japan
关键词
TiO2; film; Laser chemical vapor deposition; Laser power; Orientation; Microstructure; DIELECTRIC-PROPERTIES; CONSTANT; ANATASE; GROWTH; CVD;
D O I
10.1016/j.matlet.2012.11.121
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The TiO2 films were prepared on.Pt/Ti/SiO2/Si substrate by a laser chemical vapor deposition method. With increasing laser power (P-L) from 48 to 98 W, the deposition temperature (T-dep) monotonously increased from 849 to 929 K. At T-dep=849 K (P-L=48 W), the rutile TiO2 film was prepared with strong (110) and (200) peaks. With increasing T-dep from 849 to 883 K (P-L=71 W), the intensity of (110) peak increased. The (110)-oriented TiO2 films were obtained for T-dep beyond 903 K (P-L= 81 W). All TiO2 films showed faceted grains with the columnar cross-section. With increasing T-dep, the grain size increased and the column became wider. The high deposition rate '(R-dep) ranged from 13.04 to 24.84 mu m h(-1). (C) 2012 Elsevier B.V. All rights reserved.
引用
收藏
页码:179 / 182
页数:4
相关论文
共 50 条
  • [21] PHOTOCHEMICAL PROPERTIES OF ULTRATHIN TIO2 FILMS PREPARED BY CHEMICAL VAPOR-DEPOSITION
    SATO, S
    SOBCZYNSKI, A
    WHITE, JM
    BARD, AJ
    CAMPION, A
    FOX, MA
    MALLOUK, TE
    WEBBER, SE
    JOURNAL OF PHOTOCHEMISTRY AND PHOTOBIOLOGY A-CHEMISTRY, 1989, 50 (02) : 283 - 290
  • [22] Properties of TiO2 thin films on GaAs prepared by metalorganic chemical vapor deposition
    Lee, M.-K. (mklee@mail.ee.nsysu.edu.tw), 1600, Japan Society of Applied Physics (42):
  • [23] Nanoparticle TiO2 Films Prepared by Pulsed Laser Deposition: Laser Desorption and Cationization of Model Adsorbates
    Gamez, F.
    Plaza-Reyes, A.
    Hurtado, P.
    Guillen, F.
    Anta, J. A.
    Martinez-Haya, B.
    Perez, S.
    Sanz, M.
    Castillejo, M.
    Izquierdo, J. G.
    Banares, L.
    JOURNAL OF PHYSICAL CHEMISTRY C, 2010, 114 (41): : 17409 - 17415
  • [24] Texture and orientation characteristics of α-Al2O3 films prepared by laser chemical vapor deposition using Nd:YAG laser
    Ito, Akihiko
    Kadokura, Hokuto
    Kimura, Teiichi
    Goto, Takashi
    JOURNAL OF ALLOYS AND COMPOUNDS, 2010, 489 (02) : 469 - 474
  • [25] Growth and microstructure of Ba β-alumina films by laser chemical vapor deposition
    Ito, Akihiko
    You, Yu
    Katsui, Hirokazu
    Goto, Takashi
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2013, 33 (13-14) : 2655 - 2661
  • [26] A study of top layer of TiO2 membrane prepared by chemical vapor deposition method
    Peng, DK
    Yang, PH
    Liu, ZT
    Meng, GY
    CHEMICAL JOURNAL OF CHINESE UNIVERSITIES-CHINESE, 1997, 18 (04): : 499 - 503
  • [27] Comparison of Pt/TiO2 nanocomposite films prepared by sputtering and pulsed laser deposition
    Sasaki, T
    Koshizaki, N
    Beck, KM
    APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING, 1999, 69 (Suppl 1): : S771 - S774
  • [28] XPS study of cobalt doped TiO2 films prepared by pulsed laser deposition
    Gong, Bin
    Luo, Xi
    Bao, Nina
    Ding, Jun
    Li, Sean
    Yi, Jiabao
    SURFACE AND INTERFACE ANALYSIS, 2014, 46 (10-11) : 1043 - 1046
  • [29] Properties of TiO2 thin films on InP substrate prepared by metalorganic chemical vapor deposition
    Lee, Ming-Kwei
    Hung, Yi-Min
    Huang, Jung-Jie
    Japanese Journal of Applied Physics, Part 1: Regular Papers and Short Notes and Review Papers, 2001, 40 (11): : 6543 - 6546
  • [30] Photoelectrochemical study of thin anatase TiO2 films prepared by metallorganic chemical vapor deposition
    Boschloo, GK
    Goossens, A
    Schoonman, J
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1997, 144 (04) : 1311 - 1317