Few-layered graphene reinforced Al-10 wt% Si-2 wt% Cu matrix composites

被引:14
|
作者
Senyurt, Berk [1 ,2 ]
Kucukelyas, Burak [1 ,2 ]
Bellek, Mustafa [2 ,3 ]
Kavak, Sina [2 ,4 ]
Borand, Gokce [1 ]
Uzunsoy, Deniz [1 ]
Agaogullari, Duygu [2 ,4 ]
Akcamli, Nazli [1 ]
机构
[1] Bursa Tech Univ, Fac Engn & Nat Sci, Dept Met & Mat Engn, TR-16310 Bursa, Turkey
[2] Istanbul Tech Univ, Fac Chem & Met Engn, Dept Met & Mat Engn, Particulate Mat Labs PML,Graphene & 2D Mat Lab, TR-34469 Istanbul, Turkey
[3] Aselsan Inc, Aselsan Res Ctr, TR-34906 Istanbul, Turkey
[4] Istanbul Tech Univ, Prof Dr Adnan Tekin Mat Sci & Prod Technol Appl R, TR-34469 Istanbul, Turkey
关键词
Few-layered graphene; Al-Si-Cu matrix Composites; Mechanical alloying; Mechanical properties; Wear and corrosion resistance; MECHANICAL-PROPERTIES; ARC-DISCHARGE; STRUCTURAL-CHARACTERIZATION; AL-CU; METAL; CORROSION; BEHAVIOR; GNPS; WEAR; MICROSTRUCTURE;
D O I
10.1016/j.jmrt.2022.09.049
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Few-layered graphene (FLG) reinforced Al-10 wt% Si-2 wt% Cu (Al10Si2Cu) matrix com-posites were fabricated via a powder metallurgical route. FLG powders were produced in an originally designed DC arc reactor via arc discharge method. Al, Si, Cu and FLG powders were subjected to high-energy ball milling at different durations to produce ternary Al alloy with homogeneously dispersed FLG, and bulk composites were fabricated via subsequent uni-axial compaction and pressureless sintering. The effects of varying FLG amounts and milling duration on the properties of the powder and bulk samples were investigated. The characterization of as-blended and mechanically alloyed (MAed) powders and their sin-tered forms were performed in terms of microstructural, thermal, mechanical, wear and corrosion properties. According to the results, the hardness values of the 4 h MAed Al10Si2Cu-xFLG composites were determined as 102, 154, 191 and 241 HV for x 1/4 0, 1, 2 and 5 wt%, respectively. Despite the greater hardness value of the Al10Si2Cu-5FLG-4h com-posite, its compressive strength was low due to its brittle structure. The highest compressive strength was shown by the Al10Si2Cu-1FLG as 463 MPa by an approximate increase of 53% compared to that of the Al10Si2Cu matrix. Moreover, the tribology tests showed that FLG addition (up to 2 wt%) improved the wear rate of the Al10Si2Cu matrix. However, a deteriorative effect of FLG on the corrosion resistance of the composites was determined.(c) 2022 The Author(s). Published by Elsevier B.V. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).
引用
收藏
页码:486 / 501
页数:16
相关论文
共 50 条
  • [31] Characterization Investigations of 2 wt% LaB6 Particulate-Reinforced Al-7 wt% Si Matrix Composites Fabricated by Powder Metallurgy Methods
    Sıddıka Mertdinç
    Duygu Ağaoğulları
    Emre Tekoğlu
    M. Lütfi Öveçoğlu
    Metals and Materials International, 2020, 26 : 827 - 843
  • [32] MICROSTRUCTURE AND MECHANICAL-PROPERTIES OF RHEOCAST AL-10 WT-PERCENT CU ALLOY
    PRASAD, PR
    RAY, S
    GAINDHAR, JL
    KAPOOR, ML
    ZEITSCHRIFT FUR METALLKUNDE, 1982, 73 (07): : 420 - 425
  • [33] On the microstructural refinement in commercial purity Al and Al-10 wt% Cu alloy under ultrasonication during solidification
    Kotadia, H. R.
    Qian, M.
    Eskin, D. G.
    Das, A.
    MATERIALS & DESIGN, 2017, 132 : 266 - 274
  • [34] Influence of the milling process on TiB2 particle reinforced Al-7 wt.% Si matrix composites
    Mertdinc, Siddika
    Tekoglu, Emre
    Agaogullari, Duygu
    Ovecoglu, M. Lutfi
    MATERIALS TESTING, 2018, 60 (7-8) : 719 - 726
  • [35] The corrosion behavior of graphene reinforced titanium matrix composites in 3.5 wt% NaCl solution
    Khezerlou, Hadi
    Mutuk, Tugba
    Gurbuza, Mevlut
    Hosseini, Mir Ghasem
    DIAMOND AND RELATED MATERIALS, 2024, 148
  • [36] B4C particulate-reinforced Al-8.5 wt% Si-3.5 wt% Cu matrix composites: Powder metallurgical fabrication, age hardening, and characterization
    Akcamli, Nazli
    Senyurt, Berk
    CERAMICS INTERNATIONAL, 2021, 47 (05) : 6813 - 6826
  • [37] Densification kinetics, phase assemblage and hardness of spark plasma sintered Cu–10 wt% TiB2 and Cu–10 wt% TiB2–10 wt% Pb composites
    Amit S. Sharma
    Nisha Mishra
    Krishanu Biswas
    Bikramjit Basu
    Journal of Materials Research, 2013, 28 : 1517 - 1528
  • [38] Investigation of Mechanical and Tribological Properties of Al–7 Wt.% Si alloy Metal Matrix Composites Reinforced with SiC
    Rahul Singh
    Abhishek Kr Singh
    Pankaj Chaurashiya
    Amrendra Rai
    Vinay Kumar Singh
    Silicon, 2023, 15 : 4365 - 4374
  • [39] Powder Metallurgical Processing of Al-5 wt% Cu Matrix Composites Reinforced with MoSi2 and WSi2 Particulates
    Mertdinc-Ulkuseven, Siddika
    Ovali-Dondas, Didem
    Suzer, Ilayda
    Altintas, Mert
    Karaca, Murat Can
    Ozal, Bahadir
    Agaogullari, Duygu
    Ovecoglu, Mustafa Lutfi
    ADVANCED ENGINEERING MATERIALS, 2025, 27 (06)
  • [40] On the characterization of microstructure and fracture in a high-pressure die-casting Al-10 wt%Si alloy
    Jiao, Xiangyi
    Liu, Chaofeng
    Wang, Jun
    Guo, Zhipeng
    Wang, Junyou
    Wang, Zhuoming
    Gao, Junming
    Xiong, Shoumei
    PROGRESS IN NATURAL SCIENCE-MATERIALS INTERNATIONAL, 2020, 30 (02) : 221 - 228