Use of acoustic emission and ultrasonic techniques for monitoring crack initiation/growth during ratcheting studies on 304LN stainless steel straight pipe

被引:33
|
作者
Mukhopadhyay, C. K. [1 ]
Jayakumar, T. [1 ]
Haneef, T. K. [1 ]
Kumar, S. Suresh [2 ]
Rao, B. P. C. [1 ]
Goyal, Sumit [3 ]
Gupta, Suneel K. [3 ]
Bhasin, Vivek [3 ]
Vishnuvardhan, S. [4 ]
Raghava, G. [4 ]
Gandhi, P. [4 ]
机构
[1] Indira Gandhi Ctr Atom Res, Non Destruct Evaluat Div, Kalpakkam 603102, Tamil Nadu, India
[2] BHAVINI, Kalpakkam 603102, Tamil Nadu, India
[3] Bhabha Atom Res Ctr, Reactor Safety Div, Bombay 400085, Maharashtra, India
[4] CSIR, Struct Engn Res Ctr, Madras 600113, Tamil Nadu, India
关键词
Acoustic emission; Ultrasonic; Ratcheting; 304LN stainless steel; Through-thickness crack; AISI TYPE 304-STAINLESS-STEEL; SA333; GR.6; STEEL; TENSILE DEFORMATION; NOTCHED SPECIMENS; FAILURE; FATIGUE; STRESS; ALLOY;
D O I
10.1016/j.ijpvp.2014.01.005
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This paper describes the use of acoustic emission (AE) and ultrasonic techniques for monitoring crack initiation/growth during ratcheting studies on a straight pipe made of 304LN austenitic stainless steel under reversed four point bending. Generation of higher AE activity and AE events with higher peak amplitudes accompanied by AE cluster formation in a localized region between 826 and 845 cycles revealed the initiation of crack during the ratcheting test. Ultrasonic examination by using multiple skip technique conducted periodically at regular intervals of 25 cycles confirmed the formation of the crack only after 1000 cycles. Final rupture of the pipe occurred by through-thickness cracks after 1203 and 1225 cycles at two locations. In the range of cycles where the cracks grew, AE increased with the accumulated cycles, indicating good correlation between crack growth and AE. Acoustic emission was correlated with ballooning. While the ballooning rate decreases with cycles, count rate for different sensors increase. This has been attributed to the superposition of the generation of AE due to crack growth which increases continuously to that generated by circumferential change in strain. The superior sensitivity and reliability of acoustic emission for early detection of fatigue cracks during ratcheting test in pipe specimen is demonstrated. (C) 2014 Elsevier Ltd. All rights reserved.
引用
收藏
页码:27 / 36
页数:10
相关论文
共 25 条
  • [21] Quantitatively related acoustic emission signal with stress corrosion crack growth rate of sensitized 304 stainless steel in high-temperature water
    Zhang, Zhen
    Zhang, Ziyu
    Tan, Jibo
    Wu, Xinqiang
    CORROSION SCIENCE, 2019, 157 : 79 - 86
  • [22] Correlations of electrochemical noise, acoustic emission and complementary monitoring techniques during intergranular stress-corrosion cracking of austenitic stainless steel
    Kovac, Jaka
    Alaux, Carole
    Marrow, T. James
    Govekar, Edvard
    Legat, Andraz
    CORROSION SCIENCE, 2010, 52 (06) : 2015 - 2025
  • [23] ACOUSTIC-EMISSION BEHAVIOR DURING STAGE-II FATIGUE-CRACK GROWTH IN AN AISI TYPE-316 AUSTENITIC STAINLESS-STEEL
    MOORTHY, V
    JAYAKUMAR, T
    RAJ, B
    BULLETIN OF MATERIALS SCIENCE, 1994, 17 (06) : 699 - 715
  • [24] Acoustic emission for identification of stage IIa to IIb transition during stage II fatigue crack growth in parent and weld metal in AISI 316 austenitic stainless steel
    Moorthy, V
    Jayakumar, T
    Raj, B
    MATERIALS SCIENCE AND TECHNOLOGY, 1996, 12 (01) : 56 - 58
  • [25] Influence of microstructure on acoustic emission behavior during stage 2 fatigue crack growth in solution annealed, thermally aged and weld specimens of AISI type 316 stainless steel
    Moorthy, V
    Jayakumar, T
    Raj, B
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1996, 212 (02): : 273 - 280