Sintered Sm2Co17-Based Magnets With Small Additions of Indium

被引:6
|
作者
Gabay, Alexander M. [1 ]
Marinescu, Melania [2 ]
Liu, JinFang [2 ]
Hadjipanayis, George C. [1 ]
机构
[1] Univ Delaware, Dept Phys & Astron, Newark, DE 19716 USA
[2] Elect Energy Corp, Landisville, PA 17538 USA
关键词
Coercive force; indium; permanent magnets; samarium alloys;
D O I
10.1109/TMAG.2008.2001540
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
In an attempt to develop anisotropic high-temperature permanent magnets consisting Of Sm-2 (Co,Fe)(17) grains separated by thin layers of a nonmagnetic phase, small amounts of Ag, C, Ga, In, and Sri were added to the Sm2Co17-based alloys and sintered magnets. Grain-boundary phase(s) with the melting temperature of 985-1070 degrees C was obtained by adding 0.5-1.5 at. % In to Sm-Co, Sm-Co-Fe, and Sm-Co-Mn alloys with the Sin content slightly enriched compared to the 2 : 17 stoichiometry. Iron, manganese and, apparently, oxygen tend to decrease the melting temperature of the grain-boundary phase(s). Due to this low-melting-temperature phase, sintering of the milled Sm2Co17-based alloys becomes possible at temperatures as low as 1025-1075 degrees C. This phase is also believed to be responsible for the coercivity of 6-8 kOe observed in the Sm-Co-Fe-Mn-In alloys. The coercivity was found to be critically sensitive to the postsintering heat treatment: it dramatically deteriorates when the magnets are annealed below the melting temperature of the grain boundary phase(s).
引用
收藏
页码:4218 / 4221
页数:4
相关论文
共 50 条
  • [41] Magnetic hardening in nanograin Sm-Co 2:17 magnets
    Corte-Real, M
    Chen, ZM
    Okumura, H
    Hadjipanayis, G
    IEEE TRANSACTIONS ON MAGNETICS, 2000, 36 (05) : 3306 - 3308
  • [42] Coercivity temperature dependence of Sm2Co17-type sintered magnets with different cell and cell boundary microchemistry
    Yu, Nengjun
    Zhu, Minggang
    Song, Liwei
    Fang, Yikun
    Song, KuiKui
    Wang, Qiang
    Li, Wei
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2018, 452 : 272 - 277
  • [43] Influence mechanism of Fe content on the magnetic properties of Sm2Co17-type sintered magnets: Microstructure and Microchemistry
    Yu, Nengjun
    Gao, Wuyi
    Pan, Minxiang
    Yang, Hangfu
    Wu, Qiong
    Zhang, Pengyue
    Ge, Hongliang
    JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 818
  • [44] Effects of magnetic field heat treatment on magnetic properties and microstructure of Sm2Co17-type sintered magnets
    Liu, Lian
    Li, Yingchang
    Yu, Nengjun
    Ren, Zesong
    Song, Chi
    Pan, Minxiang
    Yang, Hangfu
    Wu, Qiong
    Ge, Hongliang
    Zhu, Minggang
    Li, Wei
    JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 1005
  • [45] Microstructures and magnetic properties of spark plasma sintered Fe-Cr-Co type and Sm2Co17 type magnets
    Matsumoto, H.
    Ikuta, N.
    Fujiwara, T.
    Konno, K.
    Nomoto, T.
    Matsuura, M.
    Taketomi, H.
    Yoshikawa, H.
    Takahashi, S.
    Kaga, H.
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2004, 272 : E1873 - E1875
  • [46] Analysis of the temperature dependence of the coercive field of Sm2Co17 based magnets
    Kronmüller, H
    Goll, D
    SCRIPTA MATERIALIA, 2003, 48 (07) : 833 - 838
  • [47] Micromagnetism and microstructure of the cell walls in Sm2Co17 based permanent magnets
    Goll, D
    Kronmüller, H
    Hadjipanayis, GC
    RARE EARTH MAGNETS AND THEIR APPLICATIONS, 2002, : 696 - 703
  • [48] Nanocomposite Sm2Co17/Co permanent magnets by mechanical alloying
    Chen, SK
    Tsai, JL
    Chin, TS
    JOURNAL OF APPLIED PHYSICS, 1996, 79 (08) : 5964 - 5966
  • [49] Synthesis and properties of a magnetically hard Sm5(Fe,Co,Tl)17 phase in sintered magnets
    Huang, M.Q.
    Simizu, S.
    Miller, K.
    Wallace, W.E.
    1600, (73):
  • [50] SYNTHESIS AND PROPERTIES OF A MAGNETICALLY HARD SM5(FE,CO,TI)17 PHASE IN SINTERED MAGNETS
    HUANG, MQ
    SIMIZU, S
    MILLER, K
    WALLACE, WE
    JOURNAL OF APPLIED PHYSICS, 1993, 73 (10) : 5902 - 5904