Dual-electrolyte lithium-air batteries: influence of catalyst, temperature, and solid-electrolyte conductivity on the efficiency and power density

被引:52
|
作者
Li, Longjun [1 ]
Manthiram, Arumugam
机构
[1] Univ Texas Austin, Electrochem Energy Lab, Austin, TX 78712 USA
关键词
OXYGEN REDUCTION; CARBON CORROSION; ELECTROCATALYSTS; CHEMISTRY; ETHER; ACID;
D O I
10.1039/c3ta01241g
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Two major issues limiting the conversion efficiency and power density of dual-electrolyte Li-air cells are the lack of efficient oxygen evolution catalysts and high internal resistance associated with the solid electrolyte. In this context, the charge voltage is lowered by 0.11 V at a charge current density of 2 mA cm(-2) by employing nanocrystalline IrO2 synthesized by a modified Adams fusion method. Similarly, the overall internal resistance of the cell is reduced substantially by increasing the operating temperature of the cell from 20 to 40 degrees C, resulting in a nearly three-fold increase in the maximum power density. Overall, the conversion efficiency at 2 mA cm(-2) is improved from 61% to 74% at 40 degrees C with the nanocrystalline IrO2. The internal resistance is further reduced by employing a more conductive solid electrolyte at 40 degrees C, resulting in a maximum power density and conversion efficiency at 2 mA cm(-2) of, respectively, 40 mW cm(-2) and 80%.
引用
收藏
页码:5121 / 5127
页数:7
相关论文
共 50 条
  • [21] A NEW GELLING AGENT AND ITS APPLICATION AS A SOLID-ELECTROLYTE FOR LITHIUM BATTERIES
    UE, M
    KAITOH, M
    YASUKAWA, E
    MORI, S
    ELECTROCHIMICA ACTA, 1993, 38 (09) : 1301 - 1302
  • [22] SOLID-ELECTROLYTE SEPARATORS BASED ON BINARY NITRIDES FOR HIGH-TEMPERATURE LITHIUM STORAGE BATTERIES
    BATALOV, NN
    ZHELTONOZHKO, OV
    ZAREMBO, SN
    AKHMETZYANOV, TM
    VOLKOVA, OV
    ZELYUTIN, GV
    OBROSOV, VP
    TAMM, VK
    RUSSIAN JOURNAL OF ELECTROCHEMISTRY, 1995, 31 (04) : 356 - 364
  • [23] Effect of solid-electrolyte pellet density on failure of solid-state batteries
    Diallo, Mouhamad S.
    Shi, Tan
    Zhang, Yaqian
    Peng, Xinxing
    Shozib, Imtiaz
    Wang, Yan
    Miara, Lincoln J.
    Scott, Mary C.
    Tu, Qingsong Howard
    Ceder, Gerbrand
    NATURE COMMUNICATIONS, 2024, 15 (01)
  • [24] Effect of solid-electrolyte pellet density on failure of solid-state batteries
    Mouhamad S. Diallo
    Tan Shi
    Yaqian Zhang
    Xinxing Peng
    Imtiaz Shozib
    Yan Wang
    Lincoln J. Miara
    Mary C. Scott
    Qingsong Howard Tu
    Gerbrand Ceder
    Nature Communications, 15
  • [25] Electron Transport and Electrolyte Reduction in the Solid-Electrolyte Interphase of Rechargeable Lithium Ion Batteries with Silicon Anodes
    Benitez, Laura
    Seminario, Jorge M.
    JOURNAL OF PHYSICAL CHEMISTRY C, 2016, 120 (32): : 17978 - 17988
  • [26] Fabrication of composite solid electrolyte based on MOF with functional ionic liquid for integrated lithium-air batteries
    Lou, Ping
    Li, Long
    Wu, Yiyun
    Yue, Lingping
    Wang, Yao
    Tang, Shun
    Zhang, Weixin
    Cao, Yuancheng
    IONICS, 2023, 29 (05) : 1803 - 1812
  • [27] Integrated Impedance-NMR identification of electrolyte stability in Lithium-Air batteries
    Dornbusch, Donald A.
    Viggiano, Rocco P.
    Lvovich, Vadim F.
    ELECTROCHIMICA ACTA, 2020, 349
  • [28] Gel electrolyte via in situ polymerization to promote durable lithium-air batteries
    Cao, Renfei
    Chen, Kai
    Cui, Yangfeng
    Liu, Jianwei
    Liu, Wanqiang
    Huang, Gang
    Zhang, Xinbo
    CHINESE CHEMICAL LETTERS, 2023, 34 (12)
  • [29] Gel electrolyte via in situ polymerization to promote durable lithium-air batteries
    Renfei Cao
    Kai Chen
    Yangfeng Cui
    Jianwei Liu
    Wanqiang Liu
    Gang Huang
    Xinbo Zhang
    Chinese Chemical Letters, 2023, 34 (12) : 392 - 396
  • [30] Improving the cycling performance of lithium-air batteries using a nitrite salt electrolyte
    Azuma, Shota
    Sano, Mitsuki
    Moro, Itsuki
    Ozawa, Fumisato
    Saito, Morihiro
    Nomura, Akihiro
    ELECTROCHIMICA ACTA, 2024, 489