Failure investigation on deformed superheater tubes

被引:42
|
作者
Othman, H. [2 ]
Purbolaksono, J. [1 ]
Ahmad, B. [2 ]
机构
[1] Univ Tenaga Nas, Kajang 43009, Malaysia
[2] TNB Res, Kajang 43000, Malaysia
关键词
Failure analysis; Finite element method; Superheater tube; Deformation;
D O I
10.1016/j.engfailanal.2008.05.023
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Investigation is conducted following the discovery of significant deformations and the presence of cracks in the vicinity of welded joints at the superheater tubes of a heat recovery steam generator (HRSG) in a Malaysian Electricity Company's power plant. This study performs the finite element (FE) analyses in order to identify the possible root cause failure of the deformed superheater tubes using software package of MSC PATRAN/NASTRAN. The locations of maximum stress induced by the deformed tube are determined. The correlation between the maximum stress and allowable restriction condition is presented, and it shows good correlations with the findings obtained from the visual inspection on site. (c) 2008 Elsevier Ltd. All rights reserved.
引用
收藏
页码:329 / 339
页数:11
相关论文
共 50 条
  • [21] Failure Analysis of Utility Boiler Superheater Tubes of A213 T12
    Ali Karimi
    Journal of Failure Analysis and Prevention, 2023, 23 : 30 - 36
  • [22] IMPROVING QUALITY OF STEAM SUPERHEATER TUBES
    SHVEDCHE.AA
    VILYAMS, OS
    KIRVALID.NS
    DUPLII, GD
    KOROBOCH.IY
    KHAUSTOV, GI
    KURILENK.VK
    STAL IN ENGLISH-USSR, 1968, (07): : 590 - &
  • [23] Failure Analysis of Utility Boiler Superheater Tubes of A213 T12
    Karimi, Ali
    JOURNAL OF FAILURE ANALYSIS AND PREVENTION, 2023, 23 (01) : 30 - 36
  • [24] Microscopical investigation of steamside oxide on X20CrMoV121 superheater tubes
    Montgomery, Melanie
    Hansson, Anette N.
    Jensen, Soren A.
    Vilhelmsen, Tommy
    MATERIALS AT HIGH TEMPERATURES, 2011, 28 (04) : 355 - 360
  • [25] Microscopical investigation of steamside oxide on X20CrMoV121 superheater tubes
    Montgomery, M.
    Hansson, A. N.
    Vilhelmsen, T.
    Jensen, S. A.
    MATERIALS AT HIGH TEMPERATURES, 2012, 29 (03) : 199 - 204
  • [26] Investigation of Premature Failure of a Coal-Fired Boiler Superheater Tube
    Biraj Kumar Sahoo
    Snehashish Tripathy
    M. Ghosh
    Swapan Kumar Das
    Goutam Das
    Journal of Failure Analysis and Prevention, 2019, 19 : 792 - 801
  • [27] An investigation of failure analysis of a superheater boiler tube working for 40 months
    Ahmadian, Peyman
    CANADIAN METALLURGICAL QUARTERLY, 2024, 63 (04) : 1347 - 1355
  • [28] BONUS SUPERHEATER FAILURE
    KING, EM
    LONG, EL
    NUCLEAR SAFETY, 1965, 7 (01): : 113 - &
  • [29] Investigation of Premature Failure of a Coal-Fired Boiler Superheater Tube
    Sahoo, Biraj Kumar
    Tripathy, Snehashish
    Ghosh, M.
    Das, Swapan Kumar
    Das, Goutam
    JOURNAL OF FAILURE ANALYSIS AND PREVENTION, 2019, 19 (03) : 792 - 801
  • [30] Failure Prediction of Superheater Tubes in Rotary Tube Bending Process Using GTN Damage Model
    Safdarian, R.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2019, 72 (02) : 475 - 486