DEFORMATION AND FRACTURE ANALYSIS OF COATING-SUBSTRATE SYSTEMS

被引:3
|
作者
Kot, M. [1 ]
机构
[1] AGH Univ Sci & Technol, Fac Mech Engn & Robot, PL-30059 Krakow, Poland
关键词
coatings; deformation; stress; fracture; TRIBOLOGICAL PROPERTIES; MULTILAYER COATINGS; THIN-FILMS; DIAMOND; TOUGHNESS; INDENTATION; STRESS; TIN; NANOINDENTATION; MICROSTRUCTURE;
D O I
10.1515/amm-2015-0378
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The paper presents the deformation and fracture analysis of coating-substrate systems dining spherical indentation. CrN and TiN ceramic coatings with a thickness of 1-5 mu m were tested using 10 to 200 pm tip radius spherical indenters. The typical results of indentation tests i.e. force-penetration depth curves were transformed into stress-strain curves using an algorithm developed by the author. The test results are compared with the results of numerical analysis conducted using FEM modelling Such a complex analysis allows users to determine the level of tensile stress leading to the formation of cracks observed using SEM and TEM microscopy, and to define the failure maps for the coating substrate-systems.
引用
收藏
页码:2307 / 2317
页数:11
相关论文
共 50 条
  • [41] Influence of viscoelastic property on laser-generated surface acoustic waves in coating-substrate systems
    Sun, Hong-xiang
    Zhang, Shu-yi
    Xu, Bai-qiang
    JOURNAL OF APPLIED PHYSICS, 2011, 109 (07)
  • [42] Crack problem for a functionally graded orthotropic coating-substrate structure
    Guo, Li-Cheng
    Wu, L. Z.
    Yu, H. J.
    PROGRESSES IN FRACTURE AND STRENGTH OF MATERIALS AND STRUCTURES, 1-4, 2007, 353-358 : 263 - 265
  • [43] The fracture analysis of a graded coating/substrate system of finite thickness with arbitrary spatial variations of coating properties: Plane deformation
    Wang, YS
    Huang, GY
    Gross, D
    ENGINEERING FRACTURE MECHANICS, 2005, 72 (12) : 1942 - 1953
  • [44] Investigation of the Influence of Parameters of Thin Coating on Mechanical Behavior of the System "Coating-Substrate"
    Eremina, Galina M.
    Smolin, Alexey Yu.
    PROCEEDINGS OF THE ADVANCED MATERIALS WITH HIERARCHICAL STRUCTURE FOR NEW TECHNOLOGIES AND RELIABLE STRUCTURES, 2018, 2051
  • [45] Spherical adhesion contact problem for FGM coating-substrate system
    Yang, Fan
    Liu, Tie-Jun
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2021, 35 (12) : 1237 - 1262
  • [46] Investigation of the electron beam thermal affecting on the coating-substrate composition
    Klimenov, V.A.
    Kovalevskaya, Zh.G.
    Eroshenko, A.Yu.
    Gubar'kov, D.V.
    Svarochnoe Proizvodstvo, 2002, (06): : 20 - 23
  • [47] Solving modern problems of a coating-substrate system in a viscoelastic approximation
    N. O. Gonchukova
    Protection of Metals and Physical Chemistry of Surfaces, 2009, 45 : 333 - 341
  • [48] Deformation and fracture of TiN coating on a Si(111) substrate during nanoindentation
    An, T.
    Wang, L. L.
    Tian, H. W.
    Wen, M.
    Zheng, W. T.
    APPLIED SURFACE SCIENCE, 2011, 257 (17) : 7475 - 7480
  • [49] Solving modern problems of a coating-substrate system in a viscoelastic approximation
    Gonchukova, N. O.
    PROTECTION OF METALS AND PHYSICAL CHEMISTRY OF SURFACES, 2009, 45 (03) : 333 - 341
  • [50] THERMODYNAMIC GUIDANCE FOR IMPLANTATION TREATMENTS TO IMPROVE COATING-SUBSTRATE ADHESION
    SINGER, IL
    FAYEULLE, S
    EHNI, PD
    VARDIMAN, RG
    APPLIED PHYSICS LETTERS, 1994, 65 (25) : 3191 - 3193