Sulfide Stress Cracking (SSC) of Low Alloy Linepipe Steels in Low H2S Content Sour Environment

被引:0
|
作者
Shimamura, Junji [1 ]
Morikawa, Tatsuya [2 ]
Yamasaki, Shigeto [2 ]
Tanaka, Masaki [2 ]
机构
[1] JFE Steel Corp, Steel Res Lab, Fukuyama, Hiroshima, Japan
[2] Kyushu Univ, Fac Engn, Dept Mat, Fukuoka, Japan
关键词
linepipe; low alloy steel; sulfide stress cracking; thermo-mechanical control process; bainite; hardness; crack initiation; hydrogen embrittlement; corrosion; CORROSION CRACKING; HYDROGEN EMBRITTLEMENT; MICROSTRUCTURE; STRENGTH; BEHAVIOR; FAILURE; CARBON;
D O I
10.2355/tetsutohagane.TETSU-2022-013
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Resistance to Sulfide Stress Cracking (SSC) caused by local hard zones of pipe inner surface has been required in low alloy linepipe steel. In this study, using two samples with different surface hardness, the detailed SSC initiation behavior was clarified by four-point bend (4PB) SSC tests in which immersion time and applied stress were changed in a sour environment containing 0.15 bar hydrogen sulfide (H2S) gas. SSC cracks occurred when the applied stress was higher than 90% actual yield strength (AYS) in higher surface hardness samples over 270 HV0.1. From the fracture surface observation of SSC crack sample, it was found that the mechanism gradually shifted from active path corrosion (APC) to hydrogen embrittlement (HE), and that the influence of APC mechanism remained partially in the process of SSC initiation at the tip of corrosion pit or groove. The polarization measurement in the 4PB SSC test showed that the anodic and cathodic reactions (especially cathodic reactions) were activated when the applied stress was 90% AYS or higher. The FEM coupled analysis simulating the stress and strain concentration at the bottom tip of the corrosion groove and the hydrogen diffusion and accumulation was carried out. The principal stress in the tensile direction showed the maximum value at 0.04-0.06 mm away from the tip of the corrosion groove, and the hydrogen accumulation became the maximum. It was analytically found that the SSC crack initiated and propagated with HE mechanism dominated type when the threshold value of about 0.82 ppm is exceeded.
引用
收藏
页码:642 / 655
页数:14
相关论文
共 50 条
  • [31] MECHANISM OF STRESS-CORROSION CRACKING OF STEELS IN H2S
    CHU, WY
    LI, SQ
    HAIAO, CM
    TIEN, JZ
    CORROSION, 1980, 36 (09) : 475 - 482
  • [32] The influence of H2S on hydrogen absorption and sulfide stress cracking resistance of high strength low alloy carbon steel C110
    Liu, Lianlian
    Case, Raymundo
    JOURNAL OF NATURAL GAS SCIENCE AND ENGINEERING, 2022, 99
  • [33] Stress corrosion cracking, of typical steels for pressure vessels in wet H2S service environment
    Chen, XD
    Jiang, JL
    Yang, TC
    Hu, JH
    Ai, ZB
    Cheng, SX
    ENVIRONMENT EFFECTS ON FRACTURE AND DAMAGE, 2004, : 79 - 85
  • [34] STRESS RELIEF CRACKING IN LOW ALLOY FERRITIC STEELS
    PRICE, AT
    SIVERNS, MJ
    METAL CONSTRUCTION AND BRITISH WELDING JOURNAL, 1970, 2 (06): : 239 - &
  • [35] The susceptibility to sulphide stress cracking of low alloy steels
    Gojic, M
    Kosec, L
    Vehovar, L
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 1998, 49 (01): : 27 - 33
  • [36] Comparison on the cracking susceptibility of different low alloy steel weldments exposed to the environment containing wet H2S
    Tang, Jian-Qun
    Gong, Jian-Ming
    Zhang, Xian-Chen
    Tu, Shan-ng Tu
    ENGINEERING FAILURE ANALYSIS, 2006, 13 (07) : 1057 - 1064
  • [37] Effects of H2S partial pressure and pH of test solution on the hydrogen induced cracking of linepipe steels
    Kim, WK
    Koh, SU
    Kim, KY
    Yang, BY
    Kang, KB
    PROCEEDINGS OF THE FIFTEENTH (2005) INTERNATIONAL OFFSHORE AND POLAR ENGINEERING CONFERENCE, VOL 4, 2005, : 143 - 147
  • [38] Some features of sulfide cracking of low-alloy and low-carbon steels
    Melekhov, RK
    Smiyan, OD
    Karvatskyi, LM
    Kapinos, LV
    Lytvyntseva, OM
    MATERIALS SCIENCE, 1995, 31 (02) : 226 - 231
  • [39] Some Features of Sulfide Cracking of Low-Alloy and Low-Carbon Steels
    Melekhov, R. K.
    Smiyan, O. D.
    Karvats'kyi, L. M.
    Kapinos, L. V.
    Materials Science, 31 (02):
  • [40] Linepipe steels for use in wet environments containing H2S
    Iino, M.
    Key Engineering Materials, 1982, 1 : 1 - 14