CO oxidation over Au/TiO2 catalyst: Pretreatment effects, catalyst deactivation, and carbonates production

被引:61
|
作者
Saavedra, Johnny [1 ]
Powell, Camilah [1 ]
Panthi, Basu [1 ]
Pursell, Christopher J. [1 ]
Chandler, Bert D. [1 ]
机构
[1] Trinity Univ, Dept Chem, San Antonio, TX 78212 USA
基金
美国国家科学基金会;
关键词
CO oxidation; Michaelis-Menten kinetics; Pretreatment; Carbonates; Au/TiO2; IR spectroscopy; Heat of adsorption; Deactivation; CO adsorption; Temkin adsorption; SUPPORTED GOLD CATALYSTS; AU NANOPARTICLES; MONOXIDE OXIDATION; OXYGEN ACTIVATION; HYDROXYL-GROUPS; ACTIVE-SITE; TEMPERATURE; H-2; ADSORPTION; STABILITY;
D O I
10.1016/j.jcat.2013.06.021
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
A commercially available Au/TiO2 catalyst was subjected to a variety of thermal treatments in order to understand how variations in catalyst pretreatment procedures might affect CO oxidation catalysis. Catalytic activity was found to be inversely correlated to the temperature of the pretreatment. Infrared spectroscopy of adsorbed CO experiments, followed by a Temkin analysis of the data, indicated that the thermal treatments caused essentially no changes to the electronics of the Au particles; this, and a series of catalysis control experiments, and previous transmission electron microscopy (TEM) studies ruled out particle growth as a contributing factor to the activity loss. Fourier transform infrared (FTIR) spectroscopy showed that pretreating the catalyst results in water desorption from the surface, but the observable water loss was similar for all the treatments and could not be correlated with catalytic activity. A Michaelis-Menten kinetic treatment indicated that the main reason for deactivation is a loss in the number of active sites with little changes in their intrinsic activity. In situ FTIR experiments during CO oxidation showed extensive buildup of carbonate-like surface species when the pretreated catalysts were contacted with the feed gas. A semi-quantitative infrared spectroscopy method was developed for comparing the amount of carbonates present on each catalyst; results from these experiments showed a strong correlation between the steady-state catalytic activity and amount of surface carbonates generated during the initial moments of catalysis. Further, this experimental protocol was used to show that the carbonates reside on the titania support rather than on the Au, as there was no evidence that they poison Au-CO binding sites. The role of the carbonates in the reaction scheme, their potential role in catalyst deactivation, and the role of surface hydroxyls and water are discussed. (C) 2013 Elsevier Inc. All rights reserved.
引用
收藏
页码:37 / 47
页数:11
相关论文
共 50 条
  • [41] Methanol production from CO2 reduction over Ni/TiO2 catalyst
    Athikaphan, Pakpoom
    Neramittagapong, Sutasinee
    Assawasaengrat, Pornsawan
    Neramittagapong, Arthit
    ENERGY REPORTS, 2020, 6 : 1162 - 1166
  • [42] The Impact of Water on CO Oxidation with Au/TiO2 Catalysts: Poison or Promotor? A Study with an Au–TiO2/MCM-48 Model Catalyst
    Andrea De Toni
    Hermann Gies
    Wolfgang Grünert
    Catalysis Letters, 2011, 141 : 1282 - 1287
  • [43] Effect of Pretreatment Time in Dry Reforming over Ni/TiO2 Catalyst
    Kim, Sung Su
    Choi, Hyun Jin
    Hong, Sung Chang
    JOURNAL OF CHEMICAL ENGINEERING OF JAPAN, 2012, 45 (01) : 41 - 45
  • [44] Investigation on selective oxidation of CO in hydrogen - rich gas for nano Au/ZnO/TiO2 catalyst
    Wang, Chao
    Xu, Xin
    Luo, Guo-Hua
    Shiyou Huagong Gaodeng Xuexiao Xuebao/Journal of Petrochemical Universities, 2007, 20 (01): : 63 - 66
  • [45] Cumene photo-oxidation over powder TiO2 catalyst
    Wittenberg, R
    Pradera, MA
    Navio, JA
    LANGMUIR, 1997, 13 (08) : 2373 - 2379
  • [46] Au/TiO2 catalyst prepared by impregnation method for low temperature oxidation of H2 and CO
    Arunajatesan, V
    Viandt, M
    McIntosh, S
    Cruz, M
    Renneke, R
    Chen, BS
    GOLD BULLETIN, 2005, 38 (03): : 133 - 133
  • [47] Catalytic wet oxidation of phenol over a Pt/TiO2 catalyst
    Maugans, CB
    Akgerman, A
    WATER RESEARCH, 1997, 31 (12) : 3116 - 3124
  • [48] Mercury oxidation by hydrochloric acid over a VOx/TiO2 catalyst
    Kamata, Hiroyuki
    Ueno, Shun-ichiro
    Naito, Toshiyuki
    Yamaguchi, Akimasa
    Ito, Shigeo
    CATALYSIS COMMUNICATIONS, 2008, 9 (14) : 2441 - 2444
  • [49] Inhibition at Perimeter Sites of Au/TiO2 Oxidation Catalyst by Reactant Oxygen
    Green, Isabel Xiaoye
    Tang, Wenjie
    McEntee, Monica
    Neurock, Matthew
    Yates, John T., Jr.
    JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 2012, 134 (30) : 12717 - 12723
  • [50] Zn Modification of Pd/TiO2/Ti Catalyst for CO Oxidation
    Samadi, Payam
    Binczarski, Michal J.
    Maniukiewicz, Waldemar
    Pawlaczyk, Aleksandra
    Rogowski, Jacek
    Szubiakiewicz, Elzbieta
    Szynkowska-Jozwik, Malgorzata I.
    Witonska, Izabela A.
    MATERIALS, 2023, 16 (03)