Microstructure and hardness evolution of nanochannel W films irradiated by helium at high temperature

被引:42
|
作者
Qin, Wenjing [1 ,2 ]
Wang, Yongqiang [3 ]
Tang, Ming [3 ]
Ren, Feng [1 ,2 ]
Fu, Qiang [1 ,2 ]
Cai, Guangxu [1 ,2 ]
Dong, Lan [1 ,2 ]
Hu, Lulu [1 ,2 ]
Wei, Guo [1 ,2 ]
Jiang, Changzhong [1 ,2 ]
机构
[1] Wuhan Univ, Sch Phys & Technol, Ctr Ion Beam Applicat, Ctr Electron Microscopy, Wuhan 430072, Hubei, Peoples R China
[2] Wuhan Univ, Hubei Nucl Solid Phys Key Lab, Wuhan 430072, Hubei, Peoples R China
[3] Los Alamos Natl Lab, Mat Sci & Technol Div, Los Alamos, NM 87545 USA
关键词
Nanochannel structure; He concentration; Swelling; Hardening; GAS-BUBBLE SUPERLATTICE; TUNGSTEN THIN-FILMS; MOLECULAR-DYNAMICS; PURE TUNGSTEN; NEUTRON-IRRADIATION; IMPLANTED TUNGSTEN; STAINLESS-STEEL; ION-IRRADIATION; HE BUBBLES; INDENTATION;
D O I
10.1016/j.jnucmat.2018.02.013
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Plasma facing materials (PFMs) face one of the most serious challenges in fusion reactors, including unprecedented harsh environment such as 14.1 MeV neutron and transmutation gas irradiation at high temperature. Tungsten (W) is considered to be one of the most promising PFM, however, virtually insolubility of helium (He) in W causes new material issues such as He bubbles and W "fuzz" microstructure. In our previous studies, we presented a new strategy using nanochannel structure designed in the W film to increase the releasing of He atoms and thus to minimize the He nucleation and "fuzz" formation behavior. In this work, we report the further study on the diffusion of He atoms in the nanochannel W films irradiated at a high temperature of 600 degrees C. More specifically, the temperature influences on the formation and growth of He bubbles, the lattice swelling, and the mechanical properties of the nanochannel W films were investigated. Compared with the bulk W, the nanochannel W films possessed smaller bubble size and lower bubble areal density, indicating that noticeable amounts of He atoms have been released out along the nanochannels during the high temperature irradiations. Thus, with lower He concentration in the nanochannel W films, the formation of the bubble superlattice is delayed, which suppresses the lattice swelling and reduces hardening. These aspects indicate the nanochannel W films have better radiation resistance even at high temperature irradiations. (c) 2018 Elsevier B.V. All rights reserved.
引用
收藏
页码:132 / 140
页数:9
相关论文
共 50 条
  • [41] Microstructure Evolution and Hardness of Hypereutectic High Chromium Cast Iron after Tempering
    Liu Yawei
    Liu Wei
    Yang Penghui
    Fu Hanguang
    Yin Wenhang
    Jin Tounan
    Chen Zhengyang
    Journal of Materials Engineering and Performance, 2024, 33 : 2724 - 2735
  • [42] Evolution of microstructure and photoluminescence of ZnO thin films irradiated with 3 MeV alpha particles
    Plugaru, R.
    Gruia, I
    Gavrila, R.
    Romanitan, C.
    Mihalache, I
    Istrate, A.
    Plugaru, N.
    SURFACES AND INTERFACES, 2020, 20
  • [43] Trends in vacancy distribution and hardness of high temperature neutron irradiated single crystal tungsten
    Bonny, G.
    Konstantinovic, M. J.
    Bakaeva, A.
    Yin, C.
    Castin, N.
    Mergia, K.
    Chatzikos, V
    Dellis, S.
    Khvan, T.
    Bakaev, A.
    Dubinko, A.
    Terentyev, D.
    ACTA MATERIALIA, 2020, 198 : 1 - 9
  • [44] MICROSTRUCTURE OF HIGH-TEMPERATURE NEUTRON-IRRADIATED TANTALUM AND MOLYBDENUM
    KULCINSKI, GL
    MASTEL, B
    JOURNAL OF APPLIED PHYSICS, 1970, 41 (11) : 4752 - +
  • [45] Helium effects on mechanical properties and microstructure of high fluence ion-irradiated RAFM steel
    Ogiwara, H.
    Kohyama, A.
    Tanigawa, H.
    Sakasegawa, H.
    JOURNAL OF NUCLEAR MATERIALS, 2007, 367 : 428 - 433
  • [46] EVOLUTION OF DEFECTS AND DEFECT CLUSTERS IN β-SiC IRRADIATED AT HIGH TEMPERATURE
    Xi, Jianqi
    Zhang, Peng
    He, Chaohui
    Zheng, Mingjie
    Zang, Hang
    Guo, Daxi
    Ma, Li
    FUSION SCIENCE AND TECHNOLOGY, 2014, 66 (01) : 235 - 244
  • [48] Effect of High-Temperature Annealing on the Microstructure and Hardness of White Pig Iron
    V. K. Afanas'ev
    G. V. Shcherbedinskii
    A. V. Kol'ba
    A. V. Sochnev
    Metal Science and Heat Treatment, 2003, 45 : 95 - 97
  • [49] The effect of high-temperature annealing on the microstructure and hardness of white pig iron
    Afanas'ev, V.K.
    Shcherbedinskij, G.V.
    Kol'ba, A.V.
    Sochnev, A.V.
    Metallovedenie i Termicheskaya Obrabotka Metallov, 2003, (03): : 17 - 19
  • [50] Effect of high-temperature annealing on the microstructure and hardness of white pig iron
    Afanas'ev, VK
    Shcherbedinskii, GV
    Kol'ba, AV
    Sochnev, AV
    METAL SCIENCE AND HEAT TREATMENT, 2003, 45 (3-4) : 95 - 97