Effect of hexagonal-BN additions on the sliding-wear resistance of fine-grained α-SiC densified with Y3Al5O12 liquid phase by spark-plasma sintering

被引:32
|
作者
Motealleh, Azadeh [1 ]
Ortiz, Angel L. [1 ]
Borrero-Lopez, Oscar [1 ]
Guiberteau, Fernando [1 ]
机构
[1] Univ Extremadura, Dept Ingn Mecan Energet & Mat, Badajoz 06006, Spain
关键词
SiC; Sliding wear; Spark-plasma sintering; Liquid-phase sintering; INTERGRANULAR PHASE; CERAMICS;
D O I
10.1016/j.jeurceramsoc.2013.09.016
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effect of flaky hexagonal (h) BN additions (1, 5, and 10 vol.%) on the lubricated sliding-wear behavior of fine-grained, liquid-phase-sintered SiC ceramics fabricated by spark-plasma sintering was investigated. It was found that resistance to the initial mild, deformation-controlled wear decreases with increasing h-BN content in the composite, which progressively exhibits a greater wear rate and a sooner transition to severe wear. This is because the softer h-BN particles reduce the hardness and do not act as internal lubricant, while promoting poorer grain cohesion due to their morphologically-favored segregation at grain boundaries. By contrast, their addition is increasingly beneficial in terms of resistance to the subsequent severe, fracture-controlled wear upon prolonged sliding contact, with a lower wear rate. This is because the flaky h-BN particles increase the fracture toughness, and also act efficiently as external lubricant when pulled-out from the microstructure. Finally, implications for the design of advanced triboceramics are discussed. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:565 / 574
页数:10
相关论文
共 22 条
  • [21] Aqueous colloidal processing of nano-SiC and its nano-Y3Al5O12 liquid-phase sintering additives with carbon nanotubes
    Candelario, Victor M.
    Moreno, Rodrigo
    Shen, Zhijian
    Ortiz, Angel L.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2015, 35 (13) : 3363 - 3368
  • [22] The Effect of Sintering Temperature on Phase-Related Peculiarities of the Microstructure, Flexural Strength, and Fracture Toughness of Fine-Grained ZrO2-Y2O3-Al2O3-CoO-CeO2-Fe2O3 Ceramics
    Kulyk, Volodymyr
    Vasyliv, Bogdan
    Duriagina, Zoia
    Lyutyy, Pavlo
    Vavrukh, Valentyna
    Kostryzhev, Andrii
    CRYSTALS, 2024, 14 (02)