Hydrogen transport in solution-treated and pre-strained austenitic stainless steels and its role in hydrogen-enhanced fatigue crack growth

被引:122
|
作者
Mine, Y. [1 ,2 ]
Narazaki, C. [3 ]
Murakami, K. [3 ]
Matsuoka, S. [1 ,2 ]
Murakami, Y. [1 ,2 ]
机构
[1] Kyushu Univ, Dept Mech Engn Sci, Nishi Ku, Fukuoka 8190395, Japan
[2] Natl Inst Adv Ind Sci & Technol, Res Ctr Hydrogen Ind Use & Storage HYDROGENIUS, Nishi Ku, Fukuoka 8190395, Japan
[3] Kyushu Univ, Grad Sch Engn, Fukuoka 8190395, Japan
关键词
Hydrogen; Solubility; Diffusivity; Fatigue crack growth; Strain-induced martensitic transformation; Austenitic stainless steel; BEHAVIOR; EMBRITTLEMENT; PERMEATION; MECHANISM;
D O I
10.1016/j.ijhydene.2008.11.018
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Hydrogen solubility and diffusion in Type 304, 316L and 310S austenitic stainless steels exposed to high-pressure hydrogen gas has been investigated. The effects of absorbed hydrogen and strain-induced martensite on fatigue crack growth behaviour of the former two steels have also been measured. in the pressure range 10-84 MPa, the hydrogen permeation of the stainless steels could be successfully quantified using Sieverts' law modified by using hydrogen fugacity and Fick's law. For the austenitic stainless steels, hydrogen diffusivity was enhanced with an increase in strain-induced martensite. The introduction of dislocation and other lattice defects by pre-straining increased the hydrogen concentration of the austenite, without affecting diffusivity. It has been shown that the coupled effect of strain-induced martensite and exposure to hydrogen increased the growth rate of fatigue cracks. (c) 2008 International Association for Hydrogen Energy. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:1097 / 1107
页数:11
相关论文
共 50 条
  • [21] EFFECT OF TEST FREQUENCY ON HYDROGEN-ENHANCED FATIGUE CRACK GROWTH IN TYPE 304 STAINLESS STEEL AND DUCTILE CAST IRON
    Matsunaga, Hisao
    Nakashima, Takuya
    Yamada, Kosei
    Matsuo, Takashi
    Yamabe, Junichiro
    Matsuoka, Saburo
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE, 2016, VOL 6B, 2017,
  • [22] Peculiar temperature dependence of hydrogen-enhanced fatigue crack growth of low-carbon steel in gaseous hydrogen
    Matsuoka, Saburo
    Takakuwa, Osamu
    Okazaki, Saburo
    Yoshikawa, Michio
    Yamabe, Junichiro
    Matsunaga, Hisao
    SCRIPTA MATERIALIA, 2018, 154 : 101 - 105
  • [23] EFFECT OF INTERNAL HYDROGEN ON CRACK-GROWTH BEHAVIOR OF AUSTENITIC STAINLESS-STEELS
    MIYOSHI, Y
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 72 (05): : S507 - S507
  • [24] HYDROGEN INDUCED SLOW CRACK-GROWTH IN STABLE AUSTENITIC STAINLESS-STEELS
    CHU, WY
    YAO, J
    HSIAO, CM
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1984, 15 (04): : 729 - 733
  • [25] Criteria for determining hydrogen compatibility and the mechanisms for hydrogen-assisted, surface crack growth in austenitic stainless steels
    Matsuoka, Saburo
    Yamabe, Junichiro
    Matsunaga, Hisao
    ENGINEERING FRACTURE MECHANICS, 2016, 153 : 103 - 127
  • [26] Creep-Fatigue Crack Growth Testing and Analysis of Pre-strained 316H Stainless Steel
    Mehmanparast, Ali
    Davies, Catrin M.
    Nikbin, Kamran
    21ST EUROPEAN CONFERENCE ON FRACTURE, (ECF21), 2016, 2 : 785 - 792
  • [27] Distinct Evidence of Hydrogen-Enhanced Defect Formation on Pre-Strained Nickel Alloy 625 during In Situ Electrochemical Nanoindentation Test
    Soundararajan, Chandrahaasan K.
    Lu, Xu
    Wang, Dong
    Vinogradov, Alexei
    METALS, 2024, 14 (02)
  • [28] INTERNAL HYDROGEN-INDUCED SUBCRITICAL CRACK-GROWTH IN AUSTENITIC STAINLESS-STEELS
    HUANG, JH
    ALTSTETTER, CJ
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1991, 22 (11): : 2605 - 2618
  • [29] Micro-Mechanical Characterisation of Hydrogen Embrittlement and Fatigue Crack Growth Behaviours in Metastable Austenitic Stainless Steels with Microstructure Refinement
    Mine, Yoji
    JOURNAL OF THE JAPAN INSTITUTE OF METALS AND MATERIALS, 2025, 89 (01) : 42 - 56
  • [30] Warm deformation enhances strength and inhibits hydrogen induced fatigue crack growth in metastable 304 and 316 austenitic stainless steels
    Wu, Zhitao
    Zhang, Kaiyu
    Zhou, Chengshuang
    Zhou, Zhengrong
    Zhang, Wenli
    Bao, Fan
    Zheng, Jinyang
    Zhang, Lin
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 818