EFFECT OF UNDERMATCHED WELD ON DEFORMATION AND BRITTLE FRACTURE BEHAVIORS IN HIGH-TENSILE STRENGTH STEEL PLATE WELDED JOINT

被引:0
|
作者
Mochizuki, Masahito [1 ]
Kawabata, Tomoya [1 ]
机构
[1] Osaka Univ, Suita, Osaka 5650871, Japan
关键词
D O I
暂无
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
High tensile strength steel such as 950 MPa class is used in hydropower plant components due to its lower cost and higher reliability. This steel is already used for penstocks in the Kanna-gawa and Omaru-gawa hydropower plants in Japan. Proper welding is one of the most critical factors to ensure integrity of the plant components against brittle fracture from weld defects. For example, preheat- and interpass-temperature controls are essential to avoid weld defects and to ensure strength, since the weld process induces residual stress and possible weld deformations such as angular distortion or unevenness. Undermatching (lower strength in weld metal than in the base plate) makes high strength steel plate become easier to use for welding because restrictions in the welding process can be reduced by using softer welding consumables. Tensile strength in welded joints increases near the base plate when the undermatched zone is not much wider than the thickness. When the appropriate welding conditions for assuring strength and preventing brittle fracture are clarified, it becomes clear to be possible to use undermatched joints for penstock. In this paper, numerical simulation of stress-strain behavior during the weld process is performed by considering the microstructural effect due to phase transformation. Phase transformation data is obtained from measured dilatometric curves in continuous cooling transformation (CCT) diagrams. Phase transformation data involves many parameters, including not only the maximum temperature, cooling rate and heat input, but also the superposition of multi heat cycles. Then, the characteristics of deformation and strength in a welded joint of 950 MPa class steel plate for penstock with undermatched region, which is equivalent to using weld material with lower strength level, are discussed to expand the allowable welding conditions in penstock fabrication. Finally, brittle fracture behaviors are discussed by using standard crack-tip opening displacement (CTOD) tests and wide plate tests with through-thickness notch by the welded joint.
引用
收藏
页码:145 / 154
页数:10
相关论文
共 50 条
  • [21] Investigation in Structure of Fusion Zone of Welded Joint of High-Strength Steel with Austenite Weld
    Dzyubyk, Andrij
    Lisovska, Lidiya
    Voitovich, Andriy
    Khomych, Ivan
    Soloviov, Oleh
    Dzyubyk, Liudmyla
    NEW TECHNOLOGIES, DEVELOPMENT AND APPLICATION VII, VOL 1, NT 2024, 2024, 1069 : 346 - 355
  • [22] Cyclic tensile test on plate-to-box column welded joints with high strength steel
    Liang, Gang
    Lu, Zhihan
    Liu, Yunhe
    Guo, Hongchao
    JOURNAL OF CONSTRUCTIONAL STEEL RESEARCH, 2025, 227
  • [23] FRACTURE-BEHAVIOR OF A LARGE-SCALE, TORCH-CUT HIGH-TENSILE STRENGTH STEEL RACK
    HONDA, H
    NAGAO, Y
    ENGINEERING FRACTURE MECHANICS, 1986, 24 (01) : 11 - 24
  • [24] Quasi-brittle Deformation and Fracture Behaviors of NM450TP High-Strength Wear-Resistant Steel Plates during Twice Tensile Test
    Li, Guan-nan
    Wen, Tong
    Zheng, Yu
    Zhou, Yin
    He, Dong-po
    Liu, Feng
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2023, 32 (19) : 8870 - 8879
  • [25] Quasi-brittle Deformation and Fracture Behaviors of NM450TP High-Strength Wear-Resistant Steel Plates during Twice Tensile Test
    Guan-nan Li
    Tong Wen
    Yu Zheng
    Yin Zhou
    Dong-po He
    Feng Liu
    Journal of Materials Engineering and Performance, 2023, 32 : 8870 - 8879
  • [26] EFFECT OF WELD HAZ MIS-MATCHING ON JOINT PERFORMANCES IN HIGH CHROMIUM STEEL WELDED JOINT
    Mochizuki, Masahito
    PROCEEDINGS OF THE 20TH INTERNATIONAL CONFERENCE ON NUCLEAR ENGINEERING AND THE ASME 2012 POWER CONFERENCE - 2012, VOL 1, 2012, : 457 - 466
  • [27] Effect of pre-fatigue on impact tensile properties of laser welded butt joint of high strength steel plates
    Suzuki Motor Co., Takatsuka-cho, Hamamatsu, 432-8611
    不详
    不详
    Zairyo, 2006, 9 (824-830):
  • [28] Improvement of weld details to avoid brittle fracture initiating at the toes of weld access hole of the beam end — prediction of ultimate strength of welded joint with conventional detail
    Koji Azuma
    Tsutomu Iwashita
    Toshiomi Itatani
    Welding in the World, 2022, 66 : 1929 - 1939
  • [29] Improvement of weld details to avoid brittle fracture initiating at the toes of weld access hole of the beam end - prediction of ultimate strength of welded joint with conventional detail
    Azuma, Koji
    Iwashita, Tsutomu
    Itatani, Toshiomi
    WELDING IN THE WORLD, 2022, 66 (09) : 1929 - 1939
  • [30] EFFECT OF SOME FACTORS ON TOUGHNESS IN WELD BOND FOR HIGH TENSILE STRENGTH STEEL.
    Kikuta, Yoneo
    Araki, Takao