Oxidation and Crack Healing Behavior of a Fine-Grained Cr2AlC Ceramic

被引:101
|
作者
Li, Shibo [1 ,2 ]
Xiao, Liou [1 ]
Song, Guiming [2 ]
Wu, Xiaomin [3 ]
Sloof, Wim G. [2 ]
van der Zwaag, Sybrand [3 ]
机构
[1] Beijing Jiaotong Univ, Sch Mech & Elect Control Engn, Ctr Mat Sci & Engn, Beijing 100044, Peoples R China
[2] Delft Univ Technol, Dept Mat Sci & Engn, NL-2628 CD Delft, Netherlands
[3] Delft Univ Technol, Fac Aerosp Engn, NL-2629 HS Delft, Netherlands
基金
中国国家自然科学基金;
关键词
HIGH-TEMPERATURE OXIDATION; STABILITY; ALUMINUM; TI3ALC2; TI2ALC;
D O I
10.1111/jace.12170
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
This work reports the oxidation and crack healing behavior of a fine-grained (similar to 2m) Cr2AlC MAX phase ceramic. The oxidation behavior was investigated in the temperature range 900 degrees C1200 degrees C for times up to 100h. The material showed a good oxidation resistance, owing to the formation of a dense and thin -Al2O3 layer. The microstructure, composition and thickness of the oxide scale were characterized. Its oxidative crack healing behavior as a function of temperature, healing time, and initial crack size was studied systematically. The material showed excellent healing behavior. The main crack healing mechanism is the filling of the crack by oxides well adhering to the crack faces. The crack geometry before and after healing was characterized by X-ray tomography. Three-point bend tests showed the dependence of strength recovery at 1100 degrees C as a function of initial crack length and healing time.
引用
收藏
页码:892 / 899
页数:8
相关论文
共 50 条
  • [21] Compressive deformation behavior of ternary compound Cr2AlC
    Wubian Tian
    ZhengMing Sun
    Hitoshi Hashimoto
    Yulei Du
    Journal of Materials Science, 2009, 44 : 102 - 107
  • [22] High-temperature oxidation and hot corrosion of Cr2AlC
    Lin, Z. J.
    Li, M. S.
    Wang, J. Y.
    Zhou, Y. C.
    ACTA MATERIALIA, 2007, 55 (18) : 6182 - 6191
  • [23] Oxidation of Cr2AlC Between 900 and 1200°C in Air
    Lee, D. B.
    Park, S. W.
    OXIDATION OF METALS, 2007, 68 (5-6): : 211 - 222
  • [24] Oxidation of Cr2AlC Between 900 and 1200 °C in Air
    D. B. Lee
    S. W. Park
    Oxidation of Metals, 2007, 68 : 211 - 222
  • [25] Synthesis and mechanical properties of high-purity Cr2AlC ceramic
    Ying, Guobing
    He, Xiaodong
    Li, Mingwei
    Han, Wenbo
    He, Fei
    Du, Shanyi
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (06): : 2635 - 2640
  • [26] A Critical Review of the Oxidation of Ti2AlC, Ti3AlC2 and Cr2AlC in Air
    Tallman, Darin J.
    Anasori, Babak
    Barsoum, Michel W.
    MATERIALS RESEARCH LETTERS, 2013, 1 (03): : 115 - 125
  • [27] Reducing the erosive wear rate of Cr2AlC MAX phase ceramic by oxidative healing of local impact damage
    Shen, Lu
    Eichner, Daniel
    van der Zwaag, Sybrand
    Leyens, Christoph
    Sloof, Willem G.
    WEAR, 2016, 358-359 : 1 - 6
  • [28] Multiple crack healing of a Ti2AlC ceramic
    Li, Shibo
    Song, Guiming
    Kwakernaak, Kees
    van der Zwaag, Sybrand
    Sloof, Wim G.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2012, 32 (08) : 1813 - 1820
  • [29] Oxidation behavior of Cr2AlC ceramics at 1,100 and 1,250 °C
    Tian, Wubian
    Wang, Peiling
    Kan, Yanmei
    Zhang, Guojun
    JOURNAL OF MATERIALS SCIENCE, 2008, 43 (08) : 2785 - 2791
  • [30] Oxidation behavior of Cr2AlC ceramics at 1,100 and 1,250 °C
    Wubian Tian
    Peiling Wang
    Yanmei Kan
    Guojun Zhang
    Journal of Materials Science, 2008, 43 : 2785 - 2791