Effect of boron concentration and grain size on weld heat affected zone microfissuring in Inconel 718 base superalloys

被引:38
|
作者
Guo, H [1 ]
Chaturvedi, MC
Richards, NL
机构
[1] Univ Manitoba, Dept Mech & Ind Engn, Winnipeg, MB R3T 5V6, Canada
[2] Bristol Aerosp Ltd, Winnipeg, MB R3C 2S4, Canada
关键词
D O I
10.1179/136217199101537761
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Microfissuring in the heal affected zone (HAZ) around electron beam (EB) welds was studied in two Inconel 718 based superalloys containing the minimum possible concentrations of C S and P, and 11 and 43 wt-ppm concentrations of B. The microfissuring susceptibility was evaluated by measuring the microcracks formed in the HAZs of EB welds and by examining the hot ductility behaviour of the material. Bead on plate type EB welding, and on cooling hot ductility tests in a Gleeble 1500 thermomechanical simulator were performed on the two alloys with different grain sizes. The results of the hot ductility tests and crack measurements on EB welded samples correlated very well with each other. Using both techniques it was observed that the HAZ microfissuring of Inconel 718 increased with an increase in B concentration and an increase in grain size. The effect of B was attributed to its segregation to the grain boundaries, which resulted in a reduction in the melting point of the grain boundary material. This rendered them susceptible to liquation in the HAZ, and formation of microfissures due to the introduction of stresses during the cooling portion of the welding thermal cycle.
引用
收藏
页码:257 / 264
页数:8
相关论文
共 50 条
  • [21] Improved Resistance to Laser Weld Heat-Affected Zone Microfissuring in a Newly Developed Superalloy HAYNES 282
    Osoba, L. O.
    Ding, R. G.
    Ojo, O. A.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2012, 43A (11): : 4281 - 4295
  • [22] Improved Resistance to Laser Weld Heat-Affected Zone Microfissuring in a Newly Developed Superalloy HAYNES 282
    L. O. Osoba
    R. G. Ding
    O. A. Ojo
    Metallurgical and Materials Transactions A, 2012, 43 : 4281 - 4295
  • [23] WELDED HEAT-AFFECTED ZONE IN NICKEL BASE ALLOY 718
    LUCAS, MJ
    JACKSON, CE
    WELDING JOURNAL, 1970, 49 (02) : S46 - &
  • [24] THE EFFECT OF INITIAL MICROSTRUCTURE ON HEAT-AFFECTED ZONE MICROFISSURING IN INCOLOY-903
    LIU, YG
    NAKKALIL, R
    RICHARDS, NL
    CHATURVEDI, MC
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1995, 202 (1-2): : 179 - 187
  • [25] Characterization of heat affected zone liquation cracking in laser additive manufacturing of Inconel 718
    Chen, Yuan
    Zhang, Ke
    Huang, Jian
    Hosseini, Seyed Reza Elmi
    Li, Zhuguo
    MATERIALS & DESIGN, 2016, 90 : 586 - 594
  • [26] Effect of weld cooling rate on Laves phase formation in Inconel 718 fusion zone
    Manikandan, S. G. K.
    Sivakumar, D.
    Rao, K. Prasad
    Kamaraj, M.
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2014, 214 (02) : 358 - 364
  • [27] MORPHOLOGY OF WELD HEAT-AFFECTED ZONE LIQUATION IN CAST ALLOY-718
    BAESLACK, WA
    NELSON, DE
    METALLOGRAPHY, 1986, 19 (03): : 371 - 379
  • [28] A MODEL FOR HEAT-AFFECTED ZONE CRACKING IN NICKEL-BASE SUPERALLOYS
    OWCZARSKI, WA
    DUVALL, DS
    SULLIVAN, CP
    WELDING JOURNAL, 1966, 45 (04) : S145 - +
  • [29] On the grain boundary strengthening effect of boron in γ/γ′ Cobalt-base superalloys
    Kolb, M.
    Freund, L. P.
    Fischer, F.
    Povstugar, I.
    Makineni, S. K.
    Gault, B.
    Raabe, D.
    Mueller, J.
    Spiecker, E.
    Neumeier, S.
    Goeken, M.
    ACTA MATERIALIA, 2018, 145 : 247 - 254
  • [30] Effect of Precipitate Phases and Grain Size on Mechanical Properties of Inconel 718 Superalloy After Various Heat Treatments
    Zhang, Min
    Ma, Chuanchuan
    Xue, Chun
    Zhong, Wenchang
    Gao, Bo
    Shuai, Meirong
    Tuo, Leifeng
    Chu, Zhibing
    RARE METAL MATERIALS AND ENGINEERING, 2024, 53 (08) : 2131 - 2136