Effect of Ni addition on pressureless sintering of tungsten diboride

被引:14
|
作者
Cao, Xiaozhou [1 ,2 ]
Wang, Chao [1 ]
Shi, Lihan [3 ]
Yang, He [1 ,2 ]
Xue, Xianxin [1 ,2 ]
Li, Haitao [4 ]
机构
[1] Northeastern Univ, Sch Met & Mat, Shenyang 110819, Peoples R China
[2] Key Lab Recycling Sci Met Resource, Shenyang 110819, Liaoning Provin, Peoples R China
[3] Shanghai Leading Met Technol Co Ltd, Shanghai, Peoples R China
[4] Shenyang Aircraft Design & Res Inst, Shenyang 110015, Peoples R China
基金
中国国家自然科学基金;
关键词
WB2; Nickel addition; Microstructure; Mechanical property; Pressureless sintering; TIB2-WB2; SOLID-SOLUTIONS; ACTIVATED COMBUSTION SYNTHESIS; PHASE-DECOMPOSITION; SIMULTANEOUS DENSIFICATION; MECHANICAL-PROPERTIES; POROSITY; MICROSTRUCTURE; TEMPERATURE; CERAMICS; TIME;
D O I
10.1016/j.ijrmhm.2013.07.013
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
WB2 ceramic was prepared by a two-step-sintering method. First, phase-pure WB2 powder was successfully synthesised by solid-state reaction using tungsten and boron powder with a molar ratio of 1:2.5. The mixed powders were treated by pressureless high-temperature synthesis (1500 degrees C, 1 h, in vacuum). Second, WB2 powder with Ni was used as a sintering aid (1500 degrees C, 1 h, in vacuum), and the influence of the content of sintering aids on the density, porosity, phase and microstructure was studied. The relationship between Vickers micro-hardness, flexural strength and microstructure was also investigated. The result showed that the properties of the WB2 ceramic can be optimised by adjusting the content of sintering aids. The best performance of the WB2 ceramic is obtained using a sintering aid content of 5 wt.%; the relative density, porosity, Vickers micro-hardness and flexural strength of the sintered sample can reach 91.80%, 3.30%, 2623 MPa and 170 MPa, respectively. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:597 / 602
页数:6
相关论文
共 50 条
  • [21] Effect of the addition of silicon nitride on sintering behaviour and microstructure of zirconium diboride
    Monteverde, F
    Bellosi, A
    SCRIPTA MATERIALIA, 2002, 46 (03) : 223 - 228
  • [22] Low temperature synthesis and pressureless sintering of nanocrystalline zirconium diboride powders
    Gocmez, Hasan
    Tuncer, Mustafa
    Yeniceri, Yavuz Selim
    CERAMICS INTERNATIONAL, 2014, 40 (08) : 12117 - 12122
  • [23] Pressureless sintering of zirconium diboride using boron carbide and carbon additions
    Zhu, Sumin
    Fahrenholtz, William G.
    Hilmas, Gregory E.
    Zhang, Shi C.
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2007, 90 (11) : 3660 - 3663
  • [24] Effect of Al addition on pressureless sintering of B4C
    Mashhadi, Mehri
    Taheri-Nassaj, Ehsan
    Sglavo, Vincenzo M.
    Sarpoolaky, Hossein
    Ehsani, Naser
    CERAMICS INTERNATIONAL, 2009, 35 (02) : 831 - 837
  • [25] Pressureless sintering and properties of titanium diboride ceramics containing chromium and iron
    Kang, SH
    Kim, DJ
    Kang, ES
    Baek, SS
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2001, 84 (04) : 893 - 895
  • [26] Pressureless sintering of titanium diboride with nickel, nickel boride, and iron additives
    Einarsrud, MA
    Hagen, E
    Pettersen, G
    Grande, T
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1997, 80 (12) : 3013 - 3020
  • [27] Effect of Ni additives on pressureless sintering of SHS ZrB2
    Khanra, AK
    Godkhindi, MM
    ADVANCES IN APPLIED CERAMICS, 2005, 104 (06) : 273 - 276
  • [28] Binderless tungsten carbide carbon control with pressureless sintering
    Fox, R. T.
    Nilsson, R.
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2018, 76 : 82 - 89
  • [29] Effect of boron addition on sintering of tungsten based alloys
    M. Debata
    A. Upadhyaya
    Journal of Materials Science, 2004, 39 : 2539 - 2541
  • [30] Effect of boron addition on sintering of tungsten based alloys
    Debata, M
    Upadhyaya, A
    JOURNAL OF MATERIALS SCIENCE, 2004, 39 (07) : 2539 - 2541