Strain Hardening of ZK60 Magnesium Alloys

被引:0
|
作者
Cho, Jae-Hyung [1 ]
Kang, Suk-Bong [1 ]
Han, Sang-Ho [1 ]
机构
[1] Korea Inst Mat Sci, Chang Won 641831, Gyeongnam, South Korea
来源
关键词
ZK60; magnesium alloys; compression; texture and microstructure; EBSD; MG-ZN; UNIAXIAL COMPRESSION; TEXTURE DEVELOPMENT; ZIRCONIUM ALLOYS; DEFORMATION; MICROSTRUCTURE; POLYCRYSTALS; DIFFRACTION; SIMULATION; SLIP;
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
ZK60(Mg-Zn-Zr) alloys possessed precipitate hardening behavior during aging, and the frequency and size of rod and disc shaped precipitates changed with aging. Strain hardening and texturing of ZK60 alloys were investigated during uniaxial warm compression. Uniaxial warm compression tests were carried out at various deformation rates and temperatures. Heat treatments of solid solution (T4) and aging (T6) affected flow stress behaviors. Aging heat treatment samples (T6) had higher yield stresses and lower strain hardening rates than solution heat-treated samples (T4). Both hardening by deformation and softening by dynamic recrystallization (DRX) at elevated temperatures were observed. Most of precipitates formed during aging contained Zn and Zr elements. Linear strain hardening behavior was examined using a visco-plastic self consistent (VPSC) model.
引用
收藏
页码:361 / 364
页数:4
相关论文
共 50 条
  • [31] Dynamic Compression Behavior of ZK60 Magnesium Alloy under Different Strain Rate
    Zhu Shuiwen
    Zhang wei
    Chen Guoping
    Peng wei
    PROCEEDINGS OF THE 5TH INTERNATIONAL CONFERENCE ON CIVIL ENGINEERING AND TRANSPORTATION 2015, 2016, 30 : 1643 - 1646
  • [32] Evolution of precipitates in ZK60 magnesium alloy during high strain rate deformation
    Yang, Yang
    Wang, Zhen
    Jiang, Lihong
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 705 : 566 - 571
  • [33] The Effect of Ultragrain Refinement on the Strength and Strain Rate Sensitivity of a ZK60 Magnesium Alloy
    Carvalho, Amanda P.
    Figueiredo, Roberto B.
    ADVANCED ENGINEERING MATERIALS, 2022, 24 (03)
  • [34] Corrosion Protection of ZK60 Wrought Magnesium Alloys by Micro-Arc Oxidation
    Xue, Yuna
    Pang, Xin
    Karparvarfard, Seyyed Mohamad Hasan
    Jahed, Hamid
    Luo, Sheji
    Shen, Yi
    METALS, 2022, 12 (03)
  • [35] Microstructure Characterization of ZK60 Magnesium Alloys Using TEM and HR-EBSD
    Cho, Jae-Hyung
    Kim, Soo-Hyun
    Han, Sang-Ho
    Kang, Suk-Bong
    MICROSCOPY AND MICROANALYSIS, 2013, 19 : 8 - 12
  • [36] Three-dimensional processing maps and flow instability of magnesium alloys ZK60
    National Die and Mold CAD Engineering Research Center, Shanghai Jiaotong University, Shanghai 200030, China
    Zhongguo Youse Jinshu Xuebao, 2008, 6 (1020-1026):
  • [37] Multiaxial fatigue of extruded ZK60 magnesium alloy
    Albinmousa, Jafar
    Adinoyi, Muhammed J.
    Merah, Nesar
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2019, 42 (10) : 2276 - 2289
  • [38] Dislocation configurations in an extruded ZK60 magnesium alloy
    Li, B.
    Ma, E.
    Ramesh, K. T.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2008, 39A (11): : 2607 - 2614
  • [39] Extraordinary superplastic ductility of magnesium alloy ZK60
    Lapovok, R
    Cottam, R
    Thomson, P
    Estrin, Y
    JOURNAL OF MATERIALS RESEARCH, 2005, 20 (06) : 1375 - 1378
  • [40] Superplasticity and diffusion bonding of magnesium alloy ZK60
    Yu, YD
    Jiang, HY
    Li, Q
    Zai, CQ
    Ding, WJ
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2005, 15 (06) : 1253 - 1257