Effect of different disinfectant methods on the initial microtensile bond strength of a self-etch adhesive to dentin

被引:23
|
作者
Dalkilic, Evrim Eliguzeloglu [1 ]
Arisu, Hacer Deniz [2 ]
Kivanc, Bagdagul Helvacioglu [3 ]
Uctasli, Mine Betul [2 ]
Omurlu, Huma [2 ]
机构
[1] Yuzuncu Yil Univ, Dept Restorat Dent, Fac Dent, TR-65080 Van, Turkey
[2] Gazi Univ, Dept Restorat Dent, Fac Dent, TR-06500 Ankara, Turkey
[3] Gazi Univ, Dept Endodont, Fac Dent, TR-06500 Ankara, Turkey
关键词
Ozone; Nd:YAG laser; Microtensile; Bond strength; Chlorhexidine; NDYAG LASER IRRADIATION; CARIOUS DENTIN; YAG LASER; IN-VITRO; OZONE; ENAMEL; CARIES; RESTORATIONS; SYSTEMS; CHLORHEXIDINE;
D O I
10.1007/s10103-011-0987-x
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
The aim of this in vitro study was to evaluate the effect of different disinfection methods on the initial microtensile bond strength of a two-step, self-etch adhesive to dentin. Twenty mandibular molars were sectioned parallel to the occlusal plane to expose the mid-coronal dentin. All of the teeth were divided into four groups (n = 5 per group): (1) in group OZ, the dentin surfaces were exposed to ozone gas from the Ozonytron X delivery system (OzonyTron X-Bioozonix, Munich, Germany), (2) in group ND, the dentin surfaces were irradiated with an Nd:YAG laser (Pulsmaster 600 IQ, American Dental Technologies, U.S.), (3) in group CHX, the dentin surfaces were treated with a 2% chlorhexidine solution, and (4) in the control group, no treatment was applied. In all of the groups, the teeth were restored with Clearfil SE Bond (Kuraray, Tokyo, Japan) and Clearfil Majesty Posterior (Kuraray, Tokyo, Japan), according to the manufacturer's instructions. The teeth were sectioned perpendicular to the bonded surface (surface area of approximately 1 mm(2)). Thus, six to seven specimens were obtained from each tooth, and a total of 34 specimens were analyzed in each group. The specimens were attached to the microtensile test machine (Micro Tensile Tester, T-61010 K, Bisco, U.S.). The data was analyzed using the one-way analysis of variance (ANOVA) and Tukey test (p < 0.05). Fracture modes of each specimen were determined using a stereomicroscope (SZ-PT Olympus, Tokyo, Japan) and a scanning electron microscope (SEM). The lowest bond strength occurred in the OZ group. Significant differences were determined only between group OZ and the other groups (group ND, group CHX, and control group) (p < 0.05). In conclusion, although ozone decreased the microtensile bond strength of the self-etch adhesive system to dentin, the Nd:YAG laser and 2% chlorhexidine did not change the microtensile bond strength so in context of the present study it would appear that the Nd:YAG laser and 2% chlorhexidine may be used as pre-restorative sterilization procedures on the dentin prior to the application of a two-step, self-etch adhesive.
引用
收藏
页码:819 / 825
页数:7
相关论文
共 50 条
  • [1] Effect of different disinfectant methods on the initial microtensile bond strength of a self-etch adhesive to dentin
    Evrim Eliguzeloglu Dalkilic
    Hacer Deniz Arisu
    Bagdagul Helvacioglu Kivanc
    Mine Betul Uctasli
    Huma Omurlu
    Lasers in Medical Science, 2012, 27 : 819 - 825
  • [2] Effect of Desensitizing Agents on the Microtensile Bond Strength of a Two-step Self-etch Adhesive to Dentin
    Arisu, H. D.
    Dalkihc, E.
    Uctasli, M. B.
    OPERATIVE DENTISTRY, 2011, 36 (02) : 153 - 161
  • [3] Microtensile Bond Strength of Self-Etch Adhesives on Dentin Treated with Chlorhexidine
    Furtado, Carolina O. D. A.
    Baroudi, Kusai
    Amaral, Marina
    Amorim, Thiago N.
    Devito, Karina L.
    de Goes, Mario F.
    Salvio, Luciana A.
    EUROPEAN JOURNAL OF PROSTHODONTICS AND RESTORATIVE DENTISTRY, 2024, 32 (01): : 133 - 141
  • [4] Microtensile bond strength of different self-etch adhesives to sound human dentin.
    Fuentes, M. V.
    Monticelli, F.
    Goracci, C.
    Toledano, M.
    Ferrari, M.
    JOURNAL OF DENTAL RESEARCH, 2003, 82 : B56 - B56
  • [5] Microtensile bond strength of etch and rinse versus self-etch adhesive systems
    Hamouda, Ibrahim M.
    Samra, Nagia R.
    Badawi, Manal F.
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2011, 4 (03) : 461 - 466
  • [6] Microtensile bond strength of a filled vs unfilled adhesive to dentin using self-etch and total-etch technique
    Say, EC
    Nakajima, M
    Senawongse, P
    Soyman, M
    Özer, F
    Ogata, M
    Tagami, J
    JOURNAL OF DENTISTRY, 2006, 34 (04) : 283 - 291
  • [7] Influence of pretreatments on microtensile bond strength to eroded dentin using a universal adhesive in self-etch mode
    Hartz, Julia J.
    Keller, Sarina P.
    Taubock, Tobias T.
    Attin, Thomas
    Wegehaupt, Florian J.
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2022, 114
  • [8] Effect of Mode of Application on the Microtensile Bond Strength of a Self-etch and Etch-and-Rinse Adhesive System
    Reis, A.
    Zander-Grande, C.
    Kossatz, S.
    Stanislawczuk, R.
    Manso, A.
    Carvalho, R. M.
    Loguercio, A. D.
    OPERATIVE DENTISTRY, 2010, 35 (04) : 428 - 435
  • [9] Effect of hydrostatic pulpal water pressure on microtensile bond strength of self-etch adhesives to dentin
    Abdalla, Ali I.
    Elsayed, Hussein Y.
    Garcia-Godoy, Franklin
    AMERICAN JOURNAL OF DENTISTRY, 2008, 21 (04): : 233 - 238
  • [10] Microtensile bond strength of self-etch adhesives in different surface conditionings
    Sohrabi, A.
    Amini, M.
    Afzali, B. M.
    Ghasemi, A.
    Sohrabi, A.
    Pakdel, S. M. Vahid
    EUROPEAN JOURNAL OF PAEDIATRIC DENTISTRY, 2012, 13 (04) : 317 - 320