In-situ observation on twin boundary evolution and crack initiation behavior during tensile test on 316L austenitic stainless steel

被引:33
|
作者
Wang, Wei [1 ]
Liu, Tingguang [1 ]
Cao, Xinyuan [1 ]
Lu, Yonghao [1 ]
Shoji, Tetsuo [2 ]
机构
[1] Univ Sci & Technol Beijing, Natl Ctr Mat Serv Safety, Beijing 100083, Peoples R China
[2] Tohoku Univ, Fracture & Reliabil Res Inst, Aoba Ku, 6-6-01 Aramaki Aoba, Sendai, Miyagi 9808579, Japan
关键词
Twin boundary; Electron back-scatter diffraction; Slip system; In-situ tensile test; Schmid factor; CRYSTALLOGRAPHIC ORIENTATION; FATIGUE CRACKING; SLIP SYSTEMS; EBSD; DEFORMATION; TEXTURE; METALS; ENERGY; NICKEL; STRAIN;
D O I
10.1016/j.matchar.2017.08.020
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This paper reports an in-situ observation on the twin boundary evolution and crack initiation behavior during the tensile test in 316L stainless steel by means of the electron backscattered diffraction (EBSD) method. The results indicated that the percentage of the twin boundaries gradually reduced with increasing elongation and the crack initiated at the twin boundary after a definite elongation. The difference in Schmid factor value between two grains besides twin boundaries continuously increased with increase of elongation, which led to movement of the dislocations within grains to twin boundaries. High density of the dislocations led to a larger local misorientation value difference between two sides of the twin boundaries, which indicated that those twin boundaries accumulated more strains during the tensile. As a result, the twin lost their coincidence site lattice with austenite grains, and twin boundaries transformed to random high angle ones, and the finally led to initiation of the crack at the high angle boundary where the twin boundary transformed.
引用
收藏
页码:169 / 174
页数:6
相关论文
共 50 条
  • [31] In-situ observation of asymmetrical deformation around inclusion in a heterogeneous additively manufactured 316L stainless steel
    Decheng Kong
    Chaofang Dong
    Xiaoqing Ni
    Zhang Liang
    Xiaogang Li
    Journal of Materials Science & Technology, 2021, 89 (30) : 133 - 140
  • [32] In-situ observation of asymmetrical deformation around inclusion in a heterogeneous additively manufactured 316L stainless steel
    Kong, Decheng
    Dong, Chaofang
    Ni, Xiaoqing
    Liang, Zhang
    Li, Xiaogang
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 89 : 133 - 140
  • [33] An In-Situ Electrochemical Nanoindentation (ECNI) Study on the Effect of Hydrogen on the Mechanical Properties of 316L Austenitic Stainless Steel
    Basa, Adina
    Wang, Dong
    Espallargas, Nuria
    Wan, Di
    MATERIALS, 2021, 14 (21)
  • [34] Effect of Nitrogen on the Fatigue Crack Growth Behavior of 316L Austenitic Stainless Steels
    Babu, M. Nani
    Sasikala, G.
    Sadananda, K.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2019, 50A (07): : 3091 - 3105
  • [35] In-situ observation of crack initiation and propagation in Ti/Al composite laminates during tensile test
    Qin, Liang
    Wang, Jin
    Wu, Qian
    Guo, Xunzhong
    Tao, Jie
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 712 : 69 - 75
  • [36] Effect of Nitrogen on the Fatigue Crack Growth Behavior of 316L Austenitic Stainless Steels
    M. Nani Babu
    G. Sasikala
    K. Sadananda
    Metallurgical and Materials Transactions A, 2019, 50 : 3091 - 3105
  • [37] Grain Boundary Engineering for Control of Fatigue Fracture in 316L Austenitic Stainless Steel
    Kobayashi, Shigeaki
    Ogou, Satoshi
    Tsurekawa, Sadahiro
    MATERIALS TRANSACTIONS, 2019, 60 (05) : 623 - 630
  • [38] A 'sigma d' approach for the assessment of creep crack initiation in 316L stainless steel CT test specimens
    Hooton, DG
    Green, D
    ECF 11 - MECHANISMS AND MECHANICS OF DAMAGE AND FAILURE, VOLS I-III, 1996, : 837 - 842
  • [40] Effect of Severe Cold or Warm Deformation on Microstructure Evolution and Tensile Behavior of a 316L Stainless Steel
    Odnobokova, Marina
    Belyakov, Andrey
    Kaibyshev, Rustam
    ADVANCED ENGINEERING MATERIALS, 2015, 17 (12) : 1812 - 1820