Austenitization and formation of ausferrite structure in austempered ductile iron with dual matrix

被引:3
|
作者
Hoang Anh Tuan [1 ]
Nguyen Hong Hai [2 ]
Nguyen Huu Dung [2 ]
Tran The Nam [3 ]
Nguyen Duong Nam [4 ]
机构
[1] Inst Technol, Dept Def, Hanoi, Vietnam
[2] HUST, Sch Mat Sci & Engn, Hanoi, Vietnam
[3] VietNam Maritime Univ, Dept Sci & Technol, Haiphong, Vietnam
[4] VietNam Maritime Univ, Sch Mech Engn, Haiphong, Vietnam
关键词
dual matrix ADI; carbon concentration; ausferrite; austempering; HEAT-TREATMENT; TRANSFORMATION; MICROSTRUCTURE; PERFORMANCE; SIMULATION; KINETICS;
D O I
10.1088/2053-1591/ac6730
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effect of austenitizing conditions on the microstructure and mechanical properties of an austempered ductile iron (ADI) with a dual matrix was investigated. Carbon diffusion plays a critical role in the phase transformation of austenitization. In initially pearlitic structures, the carbon diffusion distances involved during austenitization are smaller compared to those in ferritic structures. The study was carried out to examine the influence of temperature and times of the austenitization process on the maximum carbon content in austenite and then its effect on the processing window of ADI with the dual matrix. An alloyed ductile iron (3,6%C; 2,44%Si; 0,36%Mn; 0,9%Ni; 0,61%Cu; 0,11%Cr; 0,036%Mg; 0,015%S va 0,006%P) was fully austenitic at various temperatures 870 degrees C-930 degrees C. The minimum hardness reaches the value of 270 HB. An increase in austenitization temperature increases the carbon content dissolved in the austenite, which in turn, decreases the free energy controlling the transformation of austenite to bainite ferrite and high carbon austenite. Raising the austenitization temperature makes the process window shift toward the extending time. The carbon atoms must diffuse out of the ferrite needle with a diffusion distance equal to the ferrite layer thickness. At 360 degrees C austempered temperature, diffusion coefficient D = 4.60.10(-17)(m(2)/s). With a ferrite needle thickness of 1 mu m = 10(-6) m, the diffusion time would be t = 5330 (s).
引用
收藏
页数:10
相关论文
共 50 条
  • [31] Carbidic austempered ductile iron
    Wervey B.
    International Journal of Metalcasting, 2015, 9 (01) : 73 - 75
  • [32] The microstructure of austempered ductile iron
    Honarbakhsh-Raouf, A
    Edmonds, DV
    ELECTRON MICROSCOPY 1998, VOL 2: MATERIALS SCIENCE 1, 1998, : 173 - 174
  • [33] Highsilicone Austempered Ductile Iron
    Kochanski, A.
    Krzynska, A.
    Radziszewski, T.
    ARCHIVES OF FOUNDRY ENGINEERING, 2014, 14 (01) : 55 - 58
  • [34] AUSTEMPERED DUCTILE IRON PROCESS
    JANOWAK, J
    HEAT TREATMENT OF METALS, 1985, 12 (01): : 2 - 4
  • [35] Machinability of austempered ductile iron
    Moncada, OJ
    Spicacci, RH
    Sikora, JA
    TRANSACTIONS OF THE AMERICAN FOUNDRYMEN'S SOCIETY, VOL 106, 1998, 106 : 39 - 45
  • [36] Machining austempered ductile iron
    Brandenberg, K
    MANUFACTURING ENGINEERING, 2002, 128 (05): : 125 - +
  • [37] Ausforming austempered ductile iron
    Burke, CM
    Moore, DJ
    Rundman, KB
    TRANSACTIONS OF THE AMERICAN FOUNDRYMEN'S SOCIETY, VOL 106, 1998, 106 : 91 - 97
  • [38] AUSTEMPERED DUCTILE IRON.
    Shepperson, S.
    Allen, C.
    1600, (26):
  • [39] Formation of strain-induced martensite in austempered ductile iron
    Srinivasmurthy Daber
    P. Prasad Rao
    Journal of Materials Science, 2008, 43 : 357 - 367
  • [40] Fatigue of austempered ductile iron
    Greno, GL
    Pardo, EL
    Boeri, RE
    TRANSACTIONS OF THE AMERICAN FOUNDRYMEN'S SOCIETY, VOL 106, 1998, 106 : 31 - 37