Brazing ZrO2 ceramic to Ti-6Al-4V alloy using NiCrSiB amorphous filler foil: Interfacial microstructure and joint properties

被引:68
|
作者
Cao, J. [1 ,2 ]
Song, X. G. [1 ,2 ]
Li, C. [2 ]
Zhao, L. Y. [2 ]
Feng, J. C. [1 ,2 ]
机构
[1] Harbin Inst Technol Weihai, Shandong Prov Key Lab Special Welding Technol, Weihai 264209, Peoples R China
[2] Harbin Inst Technol, State Key Lab Adv Welding & Joining, Harbin 150001, Peoples R China
基金
中国国家自然科学基金;
关键词
Brazing; ZrO2; ceramic; TC4 titanium alloy; Interfacial microstructure; Mechanical properties; OXIDE FUEL-CELL; STAINLESS-STEEL; BRAZED JOINT; ZIRCONIA; TI; AG; CU; METAL; YTTRIA; ELECTROLYTE;
D O I
10.1016/j.matchar.2013.04.009
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Reliable brazing of ZrO2 ceramic and Ti-6Al-4V alloy was achieved using NiCrSiB amorphous filler foil. The interfacial microstructure of ZrO2/Ti-6Al-4V joints was characterized by scanning electron microscope, energy dispersive spectrometer and micro-focused X-ray diffractometer. The effects of brazing temperature on the interfacial microstructure and joining properties of brazed joints were investigated in detail. Active Ti of Ti-6Al-4V alloy dissolved into molten filler metal and reacted with ZrO2 ceramic to form a continuous TiO reaction layer, which played an important role in brazing. Various reaction phases including Ti2Ni, Ti5Si3 and beta-Ti were formed in brazed joints. With an increasing of brazing temperature, the TiO layer thickened gradually while the Ti2Ni amount reduced. Shear test indicated that brazed joints tend to fracture at the interface between ZrO2 ceramic and brazing seam or Ti2Ni intermetallic layer. The maximum average shear strength reached 284.6 MPa when brazed at 1025 degrees C for 10 min. (C) 2013 Elsevier Inc. All rights reserved.
引用
收藏
页码:85 / 91
页数:7
相关论文
共 50 条
  • [31] Wear studies of spark plasma sintered ZrO2 reinforced Ti-6Al-4V alloy
    Semetse, Lerato
    Obadele, Babatunde Abiodun
    Raganya, Lerato
    Olubambi, Peter Apata
    MATERIALS TODAY-PROCEEDINGS, 2020, 28 : 468 - 474
  • [33] Joining of Zirconia and Ti-6Al-4V Using a Ti-based Amorphous Filler
    Liu, Yuhua
    Hu, Jiandong
    Zhang, Yaping
    Guo, Zuoxing
    Yang, Yue
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2011, 27 (07) : 653 - 658
  • [34] Study on vacuum brazing of titanium alloy Ti-6Al-4V
    Wu, Minfang
    Jiang, Chengyu
    Yu, Zhishui
    Liang, Chao
    2002, Editorial Office of Chinese Journal of Mechanical Engineering (38):
  • [35] Study of brazing Ti-6Al-4V and TZM alloy using pure silver
    Chan, HY
    Shiue, RK
    JOURNAL OF MATERIALS SCIENCE LETTERS, 2003, 22 (23) : 1659 - 1663
  • [36] Microstructure and properties of Al2O3/CuSnTi+B/Ti-6Al-4V alloy joint
    He, P. (hithepeng@hit.edu.cn), 1600, Chinese Ceramic Society (40):
  • [37] Brazing ZrO2 ceramic and TC4 alloy by novel WB reinforced Ag-Cu composite filler: Microstructure and properties
    Dai, Xiangyu
    Cao, Jian
    Wang, Zichen
    Wang, Xiaoyang
    Chen, Lei
    Huang, Yongxian
    Feng, Jicai
    CERAMICS INTERNATIONAL, 2017, 43 (17) : 15296 - 15305
  • [38] Microstructure of Reactive Composite Brazing Joints of Cf/SiC Composite to Ti-6Al-4V Alloy with Cu-Ti-C Filler Material
    Ban Yonghua
    Huang Jihua
    Zhang Hua
    Zhao Xingke
    Zhang Zhiyuan
    RARE METAL MATERIALS AND ENGINEERING, 2009, 38 (04) : 713 - 716
  • [39] Vacuum brazing of medical TA9 alloy to ZrO2 bioceramics using a biocompatible filler: Interfacial microstructure, mechanical properties and biocompatibility
    Chen, Xiukai
    Cao, Yunfei
    Chen, Chen
    Wan, Zhiwen
    Tian, Jun
    Bian, Hong
    Song, Xiaoguo
    Fu, Wei
    CERAMICS INTERNATIONAL, 2024, 50 (07) : 12621 - 12631
  • [40] Effect of microstructure on mechanical properties and topography of a Ti-6Al-4V alloy
    Azkarate, I.
    Gil-Negrete, A.
    Irisarri, A.M.
    Revista de Metalurgia (Madrid), 1988, 24 (06): : 372 - 378