Composite Ta-Cu powders prepared by high energy milling

被引:19
|
作者
Costa, F. A. [1 ]
Silva, A. G. P. [2 ]
Silva, J. F., Jr. [1 ]
Gomes, U. U. [3 ]
机构
[1] Univ Fed Rio Grande do Norte, Programa Posgrad Ciencia & Engn Mat, BR-59072970 Natal, RN, Brazil
[2] UENF, Lab Mat Avancados, BR-28015620 Campos Dos Goytacazes, RJ, Brazil
[3] Univ Fed Rio Grande do Norte, Dept Fis Teor & Expt, BR-59072970 Natal, RN, Brazil
关键词
Ta-Cu alloy; amorphization; high energy milling; composite particles;
D O I
10.1016/j.ijrmhm.2007.12.002
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A mixture of Ta and 20 wt%Cu elemental powders were milled in a high energy mill under two conditions of milling intensity. Composite particles in both conditions were formed. The original Ta particles were firstly fragmented and then pierced in the deformed Cu particles. Cu hardens due to cold work and breaks. The final powder is finer than the initial powders. The final composite particles are homogeneous and consist of amorphous, separated Cu and Ta phases. The more intense milling condition produced composite particles with shorter milling time and amorphization of both phases after 50 h of milling. The less intense milling condition amorphized only the Cu phase. The composite particles can produce denser structures than mixed powders, if heated above the Cu melting point. (C) 2008 Elsevier Ltd. All rights reserved.
引用
收藏
页码:499 / 503
页数:5
相关论文
共 50 条
  • [41] Cu-Cr nanocrystalline powder prepared by high-energy ball milling
    Shi, Kun-Yu
    Shen, Tao
    Chen, Chun-Hao
    Xue, Li-Hong
    Yan, You-Wei
    Fenmo Yejin Cailiao Kexue yu Gongcheng/Materials Science and Engineering of Powder Metallurgy, 2013, 18 (04): : 532 - 538
  • [42] Mechanical Milling of Prealloyed Cu-Cr Powders Prepared by Gas Atomization
    Yeo, Hwan Kyun
    Ahn, Sang Ho
    Han, Kwan Hee
    ADVANCED MATERIALS AND PROCESSING, 2007, 26-28 : 469 - +
  • [43] Zirconium-boron reactive composite powders prepared by arrested reactive milling
    Hastings, Daniel
    Schoenitz, Mirko
    Dreizin, Edward L.
    JOURNAL OF ENERGETIC MATERIALS, 2020, 38 (02) : 142 - 161
  • [44] Effect of Milling Time on properties of Ti-48at%Al Composite Powder prepared by High Energy Milling
    YiFeng
    Cai Xiaolan
    ZhouLei
    Yu mingjun
    Li zheng
    Jiang qingwei
    MICRO-NANO TECHNOLOGY XV, 2014, 609-610 : 185 - +
  • [45] Sintering Behavior of Nanocrystalline Al6063 Powders Prepared by High-Energy Mechanical Milling
    Asgharzadeh, H.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2016, 69 (07) : 1359 - 1368
  • [46] Sintering Behavior of Nanocrystalline Al6063 Powders Prepared by High-Energy Mechanical Milling
    H. Asgharzadeh
    Transactions of the Indian Institute of Metals, 2016, 69 : 1359 - 1368
  • [47] The structure of nanocrystalline Fe, W and NiAl powders prepared by high-energy ball-milling
    Wagner, CNJ
    Yang, E
    Boldrick, MS
    NANOSTRUCTURED MATERIALS, 1996, 7 (1-2): : 1 - 11
  • [48] Amorphization behavior of mechanical alloyed Co-Ta alloy powders prepared by ball milling
    Lee, PY
    Yang, JL
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1996, 208 (01): : 76 - 79
  • [49] AMORPHOUS TA-RICH TA-CU FILMS AS DIFFUSION-BARRIERS BETWEEN AU AND GAAS
    OH, JE
    WOOLLAM, JA
    POUCH, JJ
    ALTEROVITZ, SA
    INGRAM, DC
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY B, 1988, 6 (03): : 825 - 830
  • [50] High energy planetary ball milling of SiC powders
    Pan, Y. B.
    Huang, Z. R.
    Jiang, D. L.
    Mazerolles, L.
    Michel, D.
    Pastol, J. -L.
    Wang, G.
    COMPOSITE MATERIALS V, 2007, 351 : 7 - +