Microstructure and tensile properties of low cost titanium alloys at different cooling rate

被引:11
|
作者
Wang Guo [1 ]
Hui Songxiao [1 ]
Ye Wenjun [1 ]
Mi Xujun [1 ]
Wang Yongling [1 ]
Zhang Wenjing [1 ]
机构
[1] Gen Res Inst Nonferrous Met, State Key Lab Fabricat & Proc Nonferrous Met, Beijing 100088, Peoples R China
关键词
titanium alloys; microstructure; martensite; tensile properties; fracture morphology; MECHANICAL-PROPERTIES; GRAIN-SIZE; TEMPERATURE;
D O I
10.1007/s12598-012-0552-1
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Titanium and titanium alloys have several advantages, but the cost of titanium alloys is very expensive compared with the traditional metal materials. This article introduces two new low-cost titanium alloys Ti-2.1Cr-1.3Fe (TCF alloy) and Ti-3A1-2.1Cr-1.3Fe (TACF alloy). In this study, we used Cr-Fe master alloy as one of the raw materials to develop the two new alloys. We introduce the microstructure and tensile properties of the two new alloys from beta solution treated with different cooling methods. Optical microscopy (OM), X-ray diffractometry (XRD), and transmission electron microscopy (TEM) were employed to analyze the phase constitution, and scanning electron microscopy (SEM) was used to observe the fracture surfaces. The results indicate that the microstructures consist of beta grain boundary and alpha' martensite after water quenching (WQ), beta matrix and a phase after air cooling (AC) and furnace cooling (FC), respectively. Also, the microstructure is the typical basketweave structures after FC. Of course, athermal to is also observed by TEM after WQ. The strength increases with decreasing cooling rates and the plasticity is reversed. Because of the athermal to, the strength and ductility are highest and lowest when the cooling method is WQ. The strength of TACF alloy is higher than the TCF alloy, but the plasticity is lower. The fracture surfaces are almost entirely covered with dimples under the cooling methods of AC and FC. Also, we observe an intergranular fracture area that is generated by athermal to, although some dimples are observed after WQ.
引用
收藏
页码:531 / 536
页数:6
相关论文
共 50 条
  • [31] Microstructure and Mechanical Properties of As-Cast γ-TiAl Alloys with Different Cooling Rates
    K. Yang
    Z. J. Yang
    P. Deng
    Z. Y. Chen
    Z. W. Huang
    H. L. Sun
    Journal of Materials Engineering and Performance, 2019, 28 : 2271 - 2280
  • [32] Microstructure and Mechanical Properties of As-Cast -TiAl Alloys with Different Cooling Rates
    Yang, K.
    Yang, Z. J.
    Deng, P.
    Chen, Z. Y.
    Huang, Z. W.
    Sun, H. L.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (04) : 2271 - 2280
  • [33] Effect of cooling rate on microstructure and mechanical properties of TC16 titanium alloy
    Zhang Z.-Q.
    Dong L.-M.
    Hu M.
    Lei X.-F.
    Yang Y.
    Yang R.
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2019, 29 (07): : 1391 - 1398
  • [34] EFFECT OF COOLING RATE ON THE STRUCTURE OF TITANIUM-ALLOYS
    KOVNERISTYI, YK
    BOLOTINA, NP
    NARTOVA, TT
    METAL SCIENCE AND HEAT TREATMENT, 1981, 23 (3-4) : 284 - 285
  • [35] EFFECT OF COOLING RATE ON HARDNESS OF COMMERCIAL TITANIUM ALLOYS
    MARTENS, H
    TRANSACTIONS OF THE AMERICAN INSTITUTE OF MINING AND METALLURGICAL ENGINEERS, 1956, 206 (02): : 288 - 288
  • [36] The influences of anneal temperature and cooling rate on microstructure and tensile properties of laser deposited Ti-4Al-1.5Mn titanium alloy
    Tian, X. J.
    Zhang, S. Q.
    Wang, H. M.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 608 : 95 - 101
  • [37] Effect of cooling rate on microstructure and tensile properties of powder metallurgy Ni-based superalloy
    Ding, Han-hui
    He, Guo-ai
    Wang, Xin
    Liu, Feng
    Huang, Lan
    Jiang, Liang
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2018, 28 (03) : 451 - 460
  • [38] The Effect of Cooling Rate on the Microstructure and Physical Properties of Hypereutectic Al-Ce Alloys
    Behera, Swaroop Kumar
    Van Hoogstraten, Jenna
    Rane, Kaustubh Kishore
    Weiss, David
    Rohatgi, Pradeep
    INTERNATIONAL JOURNAL OF METALCASTING, 2024, 18 (01) : 6 - 13
  • [39] Effects of Cooling Rate and Component on the Microstructure and Mechanical Properties of Mg–Zn–Y Alloys
    Shuang Shao
    Yong Liu
    Chun-Shui Xu
    Ying-Xuan Xu
    Bin Wu
    Xiao-Shu Zeng
    Xian-Feng Lu
    Xiang-Jie Yang
    Acta Metallurgica Sinica(English Letters), 2015, 28 (01) : 7 - 14
  • [40] EFFECT OF COOLING RATE ON CORROSION PROPERTIES AND MICROSTRUCTURE OF HIGH STRENGTH ALUMINIUM ALLOYS.
    't Hart, W.G.J.
    Kolkman, H.J.
    Schra, L.
    Nationaal Lucht-en Ruimtevaartlaboratorium, Verslagen en Verhandelingen, 1982,